CNC Machining Materials: Metals & Plastics Properties | nylonplastic.com

nylonplastic.com

Materialien für die CNC-Bearbeitung

Comprehensive guide to metals and plastics for precision CNC machining. Explore material properties, applications, and selection criteria.

Request Material Consultation

Materialien für die CNC-Bearbeitung

Selecting the right material is critical for successful CNC machining projects. Our comprehensive material database helps you choose the optimal metals and plastics based on your application requirements, budget, and performance needs.

Metals & Alloys for CNC Machining

Aluminum Alloys

Lightweight, excellent machinability, good strength-to-weight ratio, and corrosion resistance. Ideal for aerospace, automotive, and consumer electronics.

  • 6061: Most common, good strength
  • 7075: High strength, aerospace grade
  • 2024: High toughness, aircraft structures
  • 5052: Excellent corrosion resistance

Rostfreier Stahl

Excellent corrosion resistance, high strength, and good aesthetic appeal. Suitable for medical, marine, and food processing applications.

  • 304: General purpose, corrosion resistant
  • 316: Superior corrosion resistance
  • 303: Improved machinability
  • 17-4 PH: Precipitation hardening

Werkzeugstahl

High hardness, wear resistance, and ability to hold cutting edges. Perfect for molds, dies, and cutting tools.

  • D2: High carbon, high chromium
  • A2: Air hardening, good toughness
  • O1: Oil hardening, excellent machinability
  • M2: High-speed steel, retains hardness

Titanium Alloys

Exceptional strength-to-weight ratio, biocompatibility, and corrosion resistance. Preferred for aerospace, medical, and high-performance applications.

  • Grade 2: Commercial purity
  • Grade 5 (6AL-4V): Most common alloy
  • Grade 23: Medical grade, enhanced biocompatibility

Copper & Brass

Excellent electrical and thermal conductivity, good corrosion resistance, and antimicrobial properties. Ideal for electrical components and plumbing.

  • C110: Electrolytic tough pitch copper
  • C360: Free-cutting brass
  • C464: Naval brass, corrosion resistant

Magnesium Alloys

Extremely lightweight, good strength-to-weight ratio, and excellent machinability. Used in automotive and aerospace where weight reduction is critical.

  • AZ31B: General purpose
  • AZ91D: Die casting alloy
  • ZK60A: High strength

Engineering Plastics for CNC Machining

Nylon (PA)

Good mechanical properties, wear resistance, and toughness. Excellent for gears, bearings, and structural components.

  • PA 6: General purpose
  • PA 66: Higher temperature resistance
  • Glass-filled: Enhanced stiffness

Acetal (POM)

High stiffness, low friction, and excellent dimensional stability. Ideal for precision parts and moving components.

  • POM-C: Copolymer, better chemical resistance
  • POM-H: Homopolymer, higher mechanical strength

Polycarbonat (PC)

High impact strength, transparency, and good dimensional stability. Perfect for protective covers and transparent components.

  • Excellent impact resistance
  • Good optical clarity
  • UV resistant grades available

PEEK

High-performance thermoplastic with exceptional thermal, chemical, and mechanical properties. Used in demanding applications.

  • Continuous use to 250°C
  • Excellent chemical resistance
  • High strength and stiffness

ABS

Good impact strength, rigidity, and surface quality. Easy to machine and post-process. Common for prototypes and consumer products.

  • Good impact resistance
  • Easy to paint and glue
  • Cost-effective

PTFE (Teflon)

Exceptional chemical resistance, lowest coefficient of friction, and excellent high-temperature performance.

  • Excellent chemical resistance
  • Very low friction
  • Useful from -200°C to 260°C

Material Properties & Data

Compare key properties of common CNC machining materials to make informed decisions for your projects. All data represents typical values for standard grades.

Metals Mechanical Properties Comparison

Material Zugfestigkeit (MPa) Yield Strength (MPa) Elongation (%) Hardness Dichte (g/cm³)
Aluminum 6061 310 276 12-17 95 HB 2.70
Rostfreier Stahl 304 515 205 40 70 HRB 8.00
Steel 4140 655 415 25.7 197 HB 7.85
Titanium Grade 5 895 828 10 36 HRC 4.43
Brass C360 531 393 18 78 HRB 8.50
Copper C110 340 330 12 42 HRB 8.94

Plastics Mechanical Properties Comparison

Material Zugfestigkeit (MPa) Biegemodul (GPa) Impact Strength (J/m) HDT @ 1.8MPa (°C) Dichte (g/cm³)
Nylon 6 81 2.9 53 65 1.13
Acetal (POM) 69 2.8 76 110 1.41
Polycarbonat 72 2.4 640 130 1.20
ABS 40 2.1 200 85 1.05
PEEK 100 3.8 85 160 1.32
PTFE 27 0.5 160 50 2.16

Note on Material Selection: Properties can vary significantly based on specific grade, heat treatment, and manufacturing process. Contact our material experts for guidance on selecting the optimal material for your specific application requirements and operating conditions.

Industrieanwendungen

Different materials excel in specific applications based on their unique properties and performance characteristics. Below are common industry applications for various CNC machining materials.

Luft- und Raumfahrt

High strength-to-weight ratio materials for aircraft components, satellites, and spacecraft. Critical applications require materials with excellent fatigue resistance and reliability.

Recommended Materials: Aluminum 7075, Titanium Grade 5, PEEK, Inconel

Medical & Healthcare

Biocompatible materials for surgical instruments, implants, and medical device components. Requires sterilization capability and tissue compatibility.

Recommended Materials: Titanium Grade 23, Stainless Steel 316L, PEEK, Medical-grade Nylon

Automobilindustrie

Durable materials for engine components, transmission parts, and interior features. Balance of performance, weight, and cost considerations.

Recommended Materials: Aluminum 6061, Steel 4140, Brass, Acetal, Nylon

Elektronik

Materials for enclosures, heat sinks, connectors, and insulating components. Requires specific electrical, thermal, and dimensional stability properties.

Recommended Materials: Aluminum 6061, Copper, Brass, Polycarbonate, ABS

Industrielle Maschinen

Wear-resistant materials for gears, bearings, bushings, and mechanical components. Demanding applications requiring durability and precision.

Recommended Materials: Steel 4140, Tool Steel, Bronze, Acetal, Nylon

Konsumgüter

Aesthetic materials for consumer electronics, household items, and recreational equipment. Balance of appearance, feel, and performance.

Recommended Materials: Aluminum, Brass, Polycarbonate, ABS, Acetal

Leitfaden zur Materialauswahl

Follow this decision framework to choose the optimal material for your CNC machining project based on application requirements and performance needs.

1

Application Requirements

What are the primary functional requirements?

  • Structural Components: Consider strength, stiffness, and weight
  • Moving Parts: Evaluate wear resistance and friction properties
  • High Temperature: Assess thermal stability and heat resistance
  • Corrosive Environments: Review chemical compatibility
  • Electrical Applications: Consider conductivity and insulation needs
2

Performance Priorities

What are your key performance criteria?

  • Strength vs. Weight: Aluminum, Titanium for best ratio
  • Wear Resistance: Tool steels, hardened materials
  • Corrosion Resistance: Stainless steel, titanium, plastics
  • Temperature Resistance: High-temp alloys, PEEK, PTFE
  • Machinability: Aluminum, brass, acetal for easy machining
3

Economic Considerations

What are your budget and volume constraints?

  • Prototyping: ABS, aluminum 6061 for cost-effectiveness
  • Low Volume Production: Standard metals and plastics
  • High Volume Production: Consider machining time and material cost
  • Lifecycle Cost: Evaluate durability and maintenance requirements
  • Secondary Operations: Factor in finishing and post-processing

Need Help Selecting the Right Material?

Our material experts are here to help you choose the optimal CNC machining material for your specific application requirements and performance needs. Contact us today for technical consultation and competitive pricing.

Contact Us Today
+86 18719180813

© nylonplastic.com - Professional Supplier of CNC Machining Materials & Engineering Plastics

We do not sell, trade, or rent your personal data. You can contact us at any time to request, update, or delete your information.

For questions or concerns, reach out to:[email protected]

Nach oben blättern