{"id":2924,"date":"2026-01-26T06:15:48","date_gmt":"2026-01-26T06:15:48","guid":{"rendered":"https:\/\/nylonplastic.com\/?post_type=product&#038;p=2924"},"modified":"2026-01-26T06:38:27","modified_gmt":"2026-01-26T06:38:27","slug":"pbt-gf30","status":"publish","type":"product","link":"https:\/\/nylonplastic.com\/de\/product\/pbt-gf30\/","title":{"rendered":"PBT GF30 mit Glasfaserverst\u00e4rkung 30% - Nylon-Kunststoff"},"content":{"rendered":"<h2><a href=\"https:\/\/www.wanhan-plastic.com\/\"><img fetchpriority=\"high\" decoding=\"async\" class=\"alignnone wp-image-2406 size-full\" src=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_01-e1763968617686.jpg\" alt=\"\u4e07\u7ff0\u8be6\u60c5 01\" width=\"800\" height=\"937\"  title=\"PBT GF30 mit Glasfaserverst\u00e4rkung 30% - Nylon-Kunststoff\" srcset=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_01-e1763968617686.jpg 800w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_01-e1763968617686-256x300.jpg 256w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_01-e1763968617686-768x900.jpg 768w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_01-e1763968617686-600x703.jpg 600w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/a><\/h2>\n<h4><\/h4>\n<h3><strong>PBT GF30 Technische Daten (gesch\u00e4tzte typische Werte)<\/strong><\/h3>\n<div class=\"ds-scroll-area _1210dd7 c03cafe9\">\n<table>\n<thead>\n<tr>\n<th>Eigentum<\/th>\n<th>Wert<\/th>\n<th>Test Standard<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>Glasfasergehalt<\/strong><\/td>\n<td>30%<\/td>\n<td>ISO 1172<\/td>\n<\/tr>\n<tr>\n<td><strong>Zugfestigkeit<\/strong><\/td>\n<td>120 - 140 MPa<\/td>\n<td>ISO 527<\/td>\n<\/tr>\n<tr>\n<td><strong>Biegemodus<\/strong><\/td>\n<td>9.000 - 11.000 MPa<\/td>\n<td>ISO 178<\/td>\n<\/tr>\n<tr>\n<td><strong>Kerbschlagz\u00e4higkeit<\/strong><\/td>\n<td>7 - 9 kJ\/m\u00b2<\/td>\n<td>ISO 180<\/td>\n<\/tr>\n<tr>\n<td><strong>HDT @1,8 MPa<\/strong><\/td>\n<td>210 - 220 \u00b0C<\/td>\n<td>ISO 75<\/td>\n<\/tr>\n<tr>\n<td><strong>Vergleichender Tracking-Index (CTI)<\/strong><\/td>\n<td>550 V<\/td>\n<td>IEC 60112<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<h3><strong>PBT GF Serie Leistungsvergleichstabelle (gesch\u00e4tzte typische Werte)<\/strong><\/h3>\n<div class=\"ds-scroll-area _1210dd7 c03cafe9\">\n<table>\n<thead>\n<tr>\n<th>Eigentum<\/th>\n<th>PBT GF10<\/th>\n<th>PBT GF15<\/th>\n<th>PBT GF20<\/th>\n<th>PBT GF30<\/th>\n<th>PBT GF40<\/th>\n<th>PBT GF50<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>Glasfasergehalt<\/strong><\/td>\n<td>10%<\/td>\n<td>15%<\/td>\n<td>20%<\/td>\n<td><strong>30%<\/strong><\/td>\n<td>40%<\/td>\n<td>50%<\/td>\n<\/tr>\n<tr>\n<td><strong>Zugfestigkeit<\/strong><\/td>\n<td>70 - 85 MPa<\/td>\n<td>85 - 100 MPa<\/td>\n<td>100 - 120 MPa<\/td>\n<td><strong>120 - 140 MPa<\/strong><\/td>\n<td>135 - 155 MPa<\/td>\n<td>150 - 170 MPa<\/td>\n<\/tr>\n<tr>\n<td><strong>Biegemodus<\/strong><\/td>\n<td>5.000 - 6.500 MPa<\/td>\n<td>6.500 - 7.800 MPa<\/td>\n<td>7.500 - 9.000 MPa<\/td>\n<td><strong>9.000 - 11.000 MPa<\/strong><\/td>\n<td>11.000 - 13.000 MPa<\/td>\n<td>13.000 - 16.000 MPa<\/td>\n<\/tr>\n<tr>\n<td><strong>Kerbschlagz\u00e4higkeit<\/strong><\/td>\n<td>5 - 7 kJ\/m\u00b2<\/td>\n<td>5,5 - 7,5 kJ\/m\u00b2<\/td>\n<td>6 - 8 kJ\/m\u00b2<\/td>\n<td><strong>7 - 9 kJ\/m\u00b2<\/strong><\/td>\n<td>6,5 - 8,5 kJ\/m\u00b2<\/td>\n<td>6 - 8 kJ\/m\u00b2<\/td>\n<\/tr>\n<tr>\n<td><strong>HDT @1,8 MPa<\/strong><\/td>\n<td>180 - 195 \u00b0C<\/td>\n<td>190 - 205 \u00b0C<\/td>\n<td>200 - 210 \u00b0C<\/td>\n<td><strong>210 - 220 \u00b0C<\/strong><\/td>\n<td>215 - 225 \u00b0C<\/td>\n<td>220 - 230 \u00b0C<\/td>\n<\/tr>\n<tr>\n<td><strong>CTI (Comparative Tracking Index)<\/strong><\/td>\n<td>600 V<\/td>\n<td>600 V<\/td>\n<td>575 V<\/td>\n<td><strong>550 V<\/strong><\/td>\n<td>525 V<\/td>\n<td>500 V<\/td>\n<\/tr>\n<tr>\n<td><strong>Schl\u00fcsselprofil<\/strong><\/td>\n<td>Kosteng\u00fcnstige Steifigkeit &amp; schnelle Zyklen<\/td>\n<td>Ausgewogenes Einstiegsniveau f\u00fcr technische Teile<\/td>\n<td>Pr\u00e4zision und hervorragende Oberfl\u00e4cheng\u00fcte<\/td>\n<td><strong>Beste Balance zwischen Kraft, W\u00e4rme und Elektrizit\u00e4t<\/strong><\/td>\n<td>Hohe Steifigkeit f\u00fcr anspruchsvolle Strukturteile<\/td>\n<td>Maximale Steifigkeit f\u00fcr Metallersatz<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<h3><strong>PBT GF30 Hauptvorteile<\/strong><\/h3>\n<p>\u2705\u00a0<strong>Optimales strukturelles und elektrisches Gleichgewicht<\/strong>: Stellt den Industriestandard dar und bietet eine au\u00dfergew\u00f6hnliche Ausgewogenheit von hoher mechanischer Festigkeit, thermischer Best\u00e4ndigkeit und zuverl\u00e4ssigen dielektrischen Eigenschaften f\u00fcr anspruchsvolle technische Anwendungen.<br \/>\n\u2705\u00a0<strong>Hervorragende Kriechbest\u00e4ndigkeit und Langzeitstabilit\u00e4t<\/strong>: Hervorragende Verformungsbest\u00e4ndigkeit bei kontinuierlicher mechanischer und thermischer Beanspruchung, die die Integrit\u00e4t und Ma\u00dfhaltigkeit der Teile \u00fcber den gesamten Produktlebenszyklus gew\u00e4hrleistet.<br \/>\n\u2705\u00a0<strong>Verbesserte Leistung unter rauen Bedingungen<\/strong>: Kombiniert eine gute chemische Best\u00e4ndigkeit mit einer deutlich verbesserten W\u00e4rmeableitungstemperatur, wodurch es sich f\u00fcr den Einsatz unter der Motorhaube von Kraftfahrzeugen und f\u00fcr elektrische Hochtemperaturanwendungen eignet.<\/p>\n<h2><strong>Industrieanwendungen:<\/strong><\/h2>\n<p><img decoding=\"async\" class=\"alignnone wp-image-1751 size-full\" src=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/10\/The-Crucial-Role-of-Injection-Molding-in-Automotive-Industry.jpg\" alt=\"die entscheidende Rolle des Spritzgie\u00dfens in der Automobilindustrie\" width=\"1000\" height=\"571\"  title=\"PBT GF30 mit Glasfaserverst\u00e4rkung 30% - Nylon-Kunststoff\" srcset=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/10\/The-Crucial-Role-of-Injection-Molding-in-Automotive-Industry.jpg 1000w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/10\/The-Crucial-Role-of-Injection-Molding-in-Automotive-Industry-300x171.jpg 300w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/10\/The-Crucial-Role-of-Injection-Molding-in-Automotive-Industry-768x439.jpg 768w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/10\/The-Crucial-Role-of-Injection-Molding-in-Automotive-Industry-600x343.jpg 600w\" sizes=\"(max-width: 1000px) 100vw, 1000px\" \/><\/p>\n<h4><strong>\u00a0Entdecken Sie die PBT-Glasfaser-Serie im Detail<\/strong><\/h4>\n<p class=\"ds-markdown-paragraph\">Klicken Sie auf die nachstehenden Links, um umfassende technische Daten, Hauptvorteile und Anwendungsdetails f\u00fcr jede einzelne Sorte anzuzeigen.<\/p>\n<div class=\"ds-scroll-area _1210dd7 c03cafe9\">\n<table>\n<thead>\n<tr>\n<th>Klasse<\/th>\n<th>Am besten f\u00fcr<\/th>\n<th>\u00dcbersicht<\/th>\n<th>Vollst\u00e4ndige Details<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>PBT GF10<\/strong><\/td>\n<td>Kosteneffiziente Verbesserung von Steifigkeit, Formstabilit\u00e4t und Geschwindigkeit bei elektrischen Komponenten.<\/td>\n<td>Der am besten zug\u00e4ngliche GF-Typ, der im Vergleich zu ungef\u00fclltem PBT schnellere Zykluszeiten, h\u00f6here Steifigkeit und ausgezeichnete elektrische Isolierung bietet.<\/td>\n<td><a href=\"https:\/\/nylonplastic.com\/de\/product\/pbt-gf10\/\"><strong>Vollst\u00e4ndiges Datenblatt PBT GF10 \u2192 ansehen<\/strong><\/a><\/td>\n<\/tr>\n<tr>\n<td><strong>PBT GF20<\/strong><\/td>\n<td>Hochpr\u00e4zise Strukturteile, die Stabilit\u00e4t, glatte Oberfl\u00e4chen und gute elektrische Eigenschaften erfordern.<\/td>\n<td>Eine ausgewogene Leistung, die sich durch Ma\u00dfgenauigkeit, Oberfl\u00e4chenqualit\u00e4t und ein robustes Eigenschaftsprofil f\u00fcr technische Komponenten auszeichnet.<\/td>\n<td><a href=\"https:\/\/nylonplastic.com\/de\/product\/pbt-gf20\/\"><strong>Vollst\u00e4ndiges Datenblatt PBT GF20 \u2192 ansehen<\/strong><\/a><\/td>\n<\/tr>\n<tr>\n<td><strong>PBT GF30<\/strong><\/td>\n<td>Hochfeste Komponenten unter thermischer und mechanischer Belastung mit strengen elektrischen Anforderungen.<\/td>\n<td>Der Industriestandard, der ein optimales Gleichgewicht zwischen hoher mechanischer Festigkeit, thermischer Best\u00e4ndigkeit und unersch\u00fctterlichen dielektrischen Eigenschaften bietet.<\/td>\n<td><a href=\"https:\/\/nylonplastic.com\/de\/product\/pbt-gf30\/\"><strong>Vollst\u00e4ndiges Datenblatt PBT GF30 \u2192 ansehen<\/strong><\/a><\/td>\n<\/tr>\n<tr>\n<td><strong>PBT GF40<\/strong><\/td>\n<td>Ultrasteife, hochbelastete Anwendungen, bei denen minimales Kriechen und maximale Dimensionsstabilit\u00e4t entscheidend sind.<\/td>\n<td>Entwickelt f\u00fcr maximale Steifigkeit und langfristige Formstabilit\u00e4t unter Dauerbelastung, auch bei hohen Temperaturen.<\/td>\n<td><a href=\"https:\/\/nylonplastic.com\/de\/product\/pbt-gf40\/\"><strong>Vollst\u00e4ndiges Datenblatt PBT GF40 \u2192 ansehen<\/strong><\/a><\/td>\n<\/tr>\n<tr>\n<td><strong>PBT GF50<\/strong><\/td>\n<td>Maximale mechanische Leistung f\u00fcr Metallersatz in anspruchsvollen elektrischen\/strukturellen Anwendungen.<\/td>\n<td>Die Spitzenqualit\u00e4t, die h\u00f6chste Festigkeit, Steifigkeit und Hitzebest\u00e4ndigkeit f\u00fcr die anspruchsvollsten technischen Anwendungen bietet.<\/td>\n<td><a href=\"https:\/\/nylonplastic.com\/de\/product\/pbt-gf50\/\"><strong>Vollst\u00e4ndiges Datenblatt PBT GF50 \u2192 ansehen<\/strong><\/a><\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<h3><strong> Branchen\u00fcbergreifende Innovationskraft<\/strong><\/h3>\n<div class=\"ds-scroll-area _1210dd7 c03cafe9\">\n<div class=\"ds-scroll-area__gutters\">\n<div class=\"ds-scroll-area__vertical-gutter\"><\/div>\n<\/div>\n<table>\n<thead>\n<tr>\n<th>Industrie<\/th>\n<th>Wichtige Anwendungen<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong> Automobilindustrie<\/strong><\/td>\n<td>Motorabdeckungen, Ansaugkr\u00fcmmer, Strukturhalterungen, Sensorgeh\u00e4use, Steckverbinder.<br \/>\n<strong><a href=\"https:\/\/nylonplastic.com\/de\/automotive-industry\/\" target=\"_blank\" rel=\"noopener noreferrer\">Entdecken Sie Anwendungen im Automobilbereich \u2192<\/a><\/strong><\/td>\n<\/tr>\n<tr>\n<td><strong> Elektrotechnik und Elektronik<\/strong><\/td>\n<td>Leistungsschalter, Schalter, Steckergeh\u00e4use, isolierende Bauteile.<br \/>\n<strong><a href=\"https:\/\/nylonplastic.com\/de\/electronic-devices\/\" target=\"_blank\" rel=\"noopener noreferrer\">E&amp;E-L\u00f6sungen entdecken \u2192<\/a><\/strong><\/td>\n<\/tr>\n<tr>\n<td><strong> Industrielle Ausr\u00fcstung<\/strong><\/td>\n<td>Zahnr\u00e4der, Lager, Maschinengeh\u00e4use, Walzen, mechanische Komponenten.<br \/>\n<strong><a href=\"https:\/\/nylonplastic.com\/de\/industrieanlagen\/\" target=\"_blank\" rel=\"noopener noreferrer\">Siehe Industrielle Nutzung \u2192<\/a><\/strong><\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<figure id=\"attachment_2409\" aria-describedby=\"caption-attachment-2409\" style=\"width: 800px\" class=\"wp-caption alignnone\"><a href=\"https:\/\/nylonplastic.com\/de\/industries\/\"><img decoding=\"async\" class=\"wp-image-2409 size-full\" src=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_06.jpg\" alt=\"Verschiedene Anwendungsszenarien von PA-Kunststoffen\" width=\"800\" height=\"740\"  title=\"PBT GF30 mit Glasfaserverst\u00e4rkung 30% - Nylon-Kunststoff\" srcset=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_06.jpg 800w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_06-300x278.jpg 300w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_06-768x710.jpg 768w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_06-600x555.jpg 600w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/a><figcaption id=\"caption-attachment-2409\" class=\"wp-caption-text\">Verschiedene Anwendungsszenarien von PA-Kunststoffen<\/figcaption><\/figure>\n<\/div>\n<h3><strong>Wie w\u00e4hlt man die richtige PBT-GF-Sorte?<\/strong><\/h3>\n<p class=\"ds-markdown-paragraph\"><strong>In einfachen Worten:<\/strong><\/p>\n<p class=\"ds-markdown-paragraph\"><strong>F\u00fcr eine kosteneffiziente Verbesserung der Steifigkeit, Dimensionsstabilit\u00e4t und schnellere Zykluszeiten<\/strong>\u00a0in elektrischen Geh\u00e4usen, Steckverbindern oder grundlegenden Strukturteilen, sollten Sie\u00a0<strong>PBT GF10<\/strong>.<\/p>\n<p class=\"ds-markdown-paragraph\"><strong>F\u00fcr ein optimales Gleichgewicht von Festigkeit, Pr\u00e4zision, Oberfl\u00e4cheng\u00fcte und hervorragenden elektrischen Eigenschaften<\/strong>\u00a0bei anspruchsvollen technischen Komponenten wie Getrieben, Kfz-Sensoren oder hochwertigen Steckverbindern, w\u00e4hlen Sie\u00a0<strong>PBT GF30<\/strong>. Sie ist der Leistungsma\u00dfstab f\u00fcr die meisten strukturellen elektrischen Anwendungen.<\/p>\n<p class=\"ds-markdown-paragraph\"><strong>F\u00fcr h\u00f6chste Steifigkeit, Festigkeit und langfristige Formstabilit\u00e4t bei hoher Dauerbelastung und Hitze<\/strong>\u00a0f\u00fcr Metallersatz oder hochbelastete strukturelle Anwendungen, sollten Sie\u00a0<strong>PBT GF50<\/strong>.<\/p>\n<p class=\"ds-markdown-paragraph\"><strong>Sie sind sich nicht sicher, welche f\u00fcr Ihre Rolle perfekt ist?<\/strong>\u00a0Beschreiben Sie unseren Ingenieuren Ihre Anwendung, um eine ma\u00dfgeschneiderte Empfehlung zu erhalten:\u00a0<code>https:\/\/nylonplastic.com\/contact\/<\/code><\/p>\n<p class=\"ds-markdown-paragraph\"><strong style=\"font-size: 1.7em;\">Warum uns w\u00e4hlen?<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone wp-image-2407 size-full\" src=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_03.jpg\" alt=\"\u4e07\u7ff0\u8be6\u60c5 03\" width=\"800\" height=\"673\"  title=\"PBT GF30 mit Glasfaserverst\u00e4rkung 30% - Nylon-Kunststoff\" srcset=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_03.jpg 800w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_03-300x252.jpg 300w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_03-768x646.jpg 768w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_03-600x505.jpg 600w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone wp-image-2408 size-full\" src=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_04.jpg\" alt=\"\u4e07\u7ff0\u8be6\u60c5 04\" width=\"800\" height=\"576\"  title=\"PBT GF30 mit Glasfaserverst\u00e4rkung 30% - Nylon-Kunststoff\" srcset=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_04.jpg 800w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_04-300x216.jpg 300w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_04-768x553.jpg 768w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_04-600x432.jpg 600w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/p>\n<p class=\"ds-markdown-paragraph\"><strong>PBT GF30 FAQ<\/strong><\/p>\n<p class=\"ds-markdown-paragraph\"><strong>F1: Warum gilt PBT GF30 als \u2018Benchmark\u2018?<\/strong><br \/>\nPBT GF30 gilt weithin als Ma\u00dfstab, weil es die\u00a0<strong>optimale Ausgewogenheit der wichtigsten technischen Eigenschaften<\/strong>Hohe mechanische Festigkeit und Steifigkeit, gute thermische Best\u00e4ndigkeit, ausgezeichnete Dimensionsstabilit\u00e4t und gleichbleibende elektrische Isolierung (CTI). Es bietet das vielseitigste Leistungsprofil f\u00fcr eine breite Palette von anspruchsvollen strukturellen und elektrischen Anwendungen.<\/p>\n<p class=\"ds-markdown-paragraph\"><strong>F2: Ist PBT GF30 f\u00fcr d\u00fcnnwandige Steckverbinder geeignet?<\/strong><br \/>\n<strong>Ja, es ist eine ausgezeichnete Wahl.<\/strong>\u00a0Seine\u00a0<strong>schnelle Kristallisationsgeschwindigkeit, hohe Flie\u00dfl\u00e4nge und geringer Verzug<\/strong>\u00a0machen PBT GF30 besonders geeignet f\u00fcr das Gie\u00dfen komplexer, d\u00fcnnwandiger Komponenten, wie z. B. miniaturisierte Steckverbinder, bei denen die Einhaltung der Ma\u00dfgenauigkeit und eine hohe Pin-Haltekraft entscheidend sind.<\/p>\n<p class=\"ds-markdown-paragraph\"><strong>F3: Wie ist der CTI im Vergleich zu niedrigeren GF-Qualit\u00e4ten?<\/strong><br \/>\nPBT GF30 bietet zwar immer noch eine hervorragende Isolierung, aber der CTI von PBT GF30 (typischerweise ~550 V) ist\u00a0<strong>etwas niedriger als die von GF10 oder ungef\u00fclltem PBT<\/strong>\u00a0aufgrund des h\u00f6heren Glasfaseranteils. Er liegt deutlich \u00fcber dem Grenzwert f\u00fcr viele sicherheitskritische Anwendungen (die oft &gt;250V oder &gt;400V erfordern), aber f\u00fcr maximale Kriechstromfestigkeit k\u00f6nnen ungef\u00fcllte oder niedriger gef\u00fcllte Typen bevorzugt werden.<\/p>\n\t\t\t<div class=\"srfm-form-container srfm-form-container-305 srfm-bg-color\">\n\t\t\t<style>\n\t\t\t\t\/* Need to check and remove the input variables related to the Style Tab. *\/\n\t\t\t\t.srfm-form-container-305 {\n\t\t\t\t\t\/* New test variables *\/\n\t\t\t\t\t--srfm-color-scheme-primary: var(--ast-global-color-0);\n\t\t\t\t\t--srfm-color-scheme-text-on-primary: var(--ast-global-color-2);\n\t\t\t\t\t--srfm-color-scheme-text: var(--ast-global-color-2);\n\t\t\t\t\t--srfm-quill-editor-color: var(--ast-global-color-0);\n\n\t\t\t\t\t--srfm-color-input-label: var(--ast-global-color-2);\n\t\t\t\t\t--srfm-color-input-description: hsl( from var(--ast-global-color-2) h s l \/ 0.65 );\n\t\t\t\t\t--srfm-color-input-placeholder: hsl( from var(--ast-global-color-2) h s l \/ 0.5 );\n\t\t\t\t\t--srfm-color-input-text: var(--ast-global-color-2);\n\t\t\t\t\t--srfm-color-input-prefix: hsl( from var(--ast-global-color-2) h s l \/ 0.65 );\n\t\t\t\t\t--srfm-color-input-background: hsl( from var(--ast-global-color-2) h s l \/ 0.02 );\n\t\t\t\t\t--srfm-color-input-background-hover: hsl( from var(--ast-global-color-2) h s l \/ 0.05 );\n\t\t\t\t\t--srfm-color-input-background-disabled: hsl( from var(--ast-global-color-2) h s l \/ 0.07 );\n\t\t\t\t\t--srfm-color-input-border: hsl( from var(--ast-global-color-2) h s l \/ 0.25 );\n\t\t\t\t\t--srfm-color-input-border-disabled: hsl( from var(--ast-global-color-2) h s l \/ 0.15 );\n\t\t\t\t\t--srfm-color-multi-choice-svg: hsl( from var(--ast-global-color-2) h s l \/ 0.7 );\n\t\t\t\t\t--srfm-color-input-border-hover: hsl( from var(--ast-global-color-0) h s l \/ 0.65 );\n\t\t\t\t\t--srfm-color-input-border-focus-glow: hsl( from var(--ast-global-color-0) h s l \/ 0.15 );\n\t\t\t\t\t--srfm-color-input-selected: hsl( from var(--ast-global-color-0) h s l \/ 0.1 );\n\t\t\t\t\t--srfm-btn-color-hover: hsl( from var(--ast-global-color-0) h s l \/ 0.9 );\n\t\t\t\t\t--srfm-btn-color-disabled: hsl( from var(--ast-global-color-0) h s l \/ 0.25 );\n\n\t\t\t\t\t\/* Dropdown Variables *\/\n\t\t\t\t\t--srfm-dropdown-input-background-hover: hsl( from var(--ast-global-color-2) h s l \/ 0.05 );\n\t\t\t\t\t--srfm-dropdown-option-background-hover: hsl( from var(--ast-global-color-2) h s l \/ 0.10 );\n\t\t\t\t\t--srfm-dropdown-option-background-selected: hsl( from var(--ast-global-color-2) h s l \/ 0.05 );\n\t\t\t\t\t--srfm-dropdown-option-selected-icon: hsl( from var(--ast-global-color-2) h s l \/ 0.65 );\n\t\t\t\t\t--srfm-dropdown-option-text-color: hsl( from var(--ast-global-color-2) h s l \/ 0.80 );\n\t\t\t\t\t--srfm-dropdown-option-selected-text: var(--ast-global-color-2);\n\t\t\t\t\t--srfm-dropdown-badge-background: hsl( from var(--ast-global-color-2) h s l \/ 0.05 );\n\t\t\t\t\t--srfm-dropdown-badge-background-hover: hsl( from var(--ast-global-color-2) h s l \/ 0.10 );\n\t\t\t\t\t--srfm-dropdown-menu-border-color: hsl( from var(--ast-global-color-2) h s l \/ 0.10 );\n\t\t\t\t\t--srfm-dropdown-placeholder-color: hsl( from var(--ast-global-color-2) h s l \/ 0.50 );\n\t\t\t\t\t--srfm-dropdown-icon-color: hsl( from var(--ast-global-color-2) h s l \/ 0.65 );\n\t\t\t\t\t--srfm-dropdown-icon-disabled: hsl( from var(--ast-global-color-2) h s l \/ 0.25 );\n\n\t\t\t\t\t\/* Background Control Variables *\/\n\t\t\t\t\t--srfm-instant-form-padding-top: 32px;--srfm-instant-form-padding-right: 32px;--srfm-instant-form-padding-bottom: 32px;--srfm-instant-form-padding-left: 32px;--srfm-instant-form-border-radius-top: 12px;--srfm-instant-form-border-radius-right: 12px;--srfm-instant-form-border-radius-bottom: 12px;--srfm-instant-form-border-radius-left: 12px;--srfm-form-padding-top: 0px;--srfm-form-padding-right: 0px;--srfm-form-padding-bottom: 0px;--srfm-form-padding-left: 0px;--srfm-form-border-radius-top: 99px;--srfm-form-border-radius-right: 99px;--srfm-form-border-radius-bottom: 99px;--srfm-form-border-radius-left: 99px;--srfm-bg-overlay-opacity: 1;\t\t\t\t\t--srfm-row-gap-between-blocks: 18px;--srfm-address-label-font-size: 16px;--srfm-address-label-line-height: 24px;--srfm-address-description-font-size: 14px;--srfm-address-description-line-height: 20px;--srfm-col-gap-between-fields: 16px;--srfm-row-gap-between-fields: 16px;--srfm-gap-below-address-label: 14px;--srfm-dropdown-font-size: 14px;--srfm-dropdown-gap-between-input-menu: 4px;--srfm-dropdown-badge-padding: 2px 6px;--srfm-dropdown-multiselect-font-size: 12px;--srfm-dropdown-multiselect-line-height: 16px;--srfm-dropdown-padding-right: 12px;--srfm-dropdown-padding-right-icon: calc( var( --srfm-dropdown-padding-right ) + 20px );--srfm-dropdown-multiselect-padding: 8px var( --srfm-dropdown-padding-right-icon ) 8px 8px;--srfm-input-height: 44px;--srfm-input-field-padding: 10px 12px;--srfm-input-field-font-size: 16px;--srfm-input-field-line-height: 24px;--srfm-input-field-margin-top: 6px;--srfm-input-field-margin-bottom: 6px;--srfm-checkbox-label-font-size: 16px;--srfm-checkbox-label-line-height: 24px;--srfm-checkbox-description-font-size: 14px;--srfm-checkbox-description-line-height: 20px;--srfm-check-ctn-width: 16px;--srfm-check-ctn-height: 16px;--srfm-check-svg-size: 10px;--srfm-checkbox-margin-top-frontend: 4px;--srfm-checkbox-margin-top-editor: 6px;--srfm-check-gap: 8px;--srfm-checkbox-description-margin-left: 24px;--srfm-flag-section-padding: 10px 0 10px 12px;--srfm-gap-between-icon-text: 8px;--srfm-label-font-size: 16px;--srfm-label-line-height: 24px;--srfm-description-font-size: 14px;--srfm-description-line-height: 20px;--srfm-btn-padding: 10px 14px;--srfm-btn-font-size: 16px;--srfm-btn-line-height: 24px;--srfm-multi-choice-horizontal-padding: 20px;--srfm-multi-choice-vertical-padding: 20px;--srfm-multi-choice-internal-option-gap: 8px;--srfm-multi-choice-vertical-svg-size: 40px;--srfm-multi-choice-horizontal-image-size: 24px;--srfm-multi-choice-vertical-image-size: 120px;--srfm-multi-choice-outer-padding: 2px;\t\t\t\t}\n\t\t\t<\/style>\n\t\t\t\t\t\t\t<form method=\"post\" enctype=\"multipart\/form-data\" id=\"srfm-form-305\" class=\"srfm-form\"\n\t\t\t\tform-id=\"305\" after-submission=\"hide form\" message-type=\"same page\" success-url=\"\" ajaxurl=\"https:\/\/nylonplastic.com\/wp-admin\/admin-ajax.php\" data-submit-token=\"d6a1fe6a4a336615a96db9d7bff1c92f1259f25ce094c9d639c799ca80577d95\" action=\"\"\n\t\t\t\t>\n\t\t\t\t\n\t\t\t\t<input type=\"hidden\" value=\"305\" name=\"form-id\">\n\t\t\t\t<input type=\"hidden\" value=\"\" name=\"srfm-sender-email-field\" id=\"srfm-sender-email\">\n\t\t\t\t<input type=\"hidden\" value=\"\" id=\"srfm-page-break\">\n\t\t\t\t\t\t<p id=\"srfm-error-message\" class=\"srfm-common-error-message srfm-error-message srfm-head-error\" hidden>\t\t<span class=\"srfm-icon\" aria-hidden=\"true\">\n\t\t\t<svg xmlns=\"http:\/\/www.w3.org\/2000\/svg\" width=\"20\" height=\"20\" fill=\"none\"><path d=\"M9.99935 18.3327C14.6017 18.3327 18.3327 14.6017 18.3327 9.99935C18.3327 5.39698 14.6017 1.66602 9.99935 1.66602C5.39698 1.66602 1.66602 5.39698 1.66602 9.99935C1.66602 14.6017 5.39698 18.3327 9.99935 18.3327Z\" stroke=\"currentColor\" stroke-width=\"1.5\" stroke-linecap=\"round\" stroke-linejoin=\"round\" \/><path d=\"M10 6.66602V9.99935\" stroke=\"currentColor\" stroke-width=\"1.5\" stroke-linecap=\"round\" stroke-linejoin=\"round\" \/><path d=\"M10 13.334H10.0083\" stroke=\"currentColor\" stroke-width=\"1.5\" stroke-linecap=\"round\" stroke-linejoin=\"round\" \/><\/svg>\t\t<\/span>\n\t\t<span class=\"srfm-error-content\">Bei der \u00dcbermittlung Ihres Formulars ist ein Fehler aufgetreten. Bitte versuchen Sie es erneut.<\/span><\/p>\n\t\t\t\t\t\t<div data-block-id=\"7fa370fa\" class=\"wp-block-uagb-advanced-heading uagb-block uagb-block-7fa370fa 305\" >\n\t\t\t\t\t<h2 class=\"uagb-heading-text\">Entwerfen wir Ihre individuelle L\u00f6sung<\/h2>\t\t\t\t<\/div>\n\t\t\t\n\n\t\t\t<div data-block-id=\"bb2839a9\" class=\"srfm-block-single srfm-block srfm-input-block srf-input-bb2839a9-block  srfm-block-width-50 srfm-slug-text-field 305\" >\n\t\t\t\t\t\t\t\t<label id=\"srfm-label-bb2839a9-lbl-Rmlyc3QgTmFtZQ\" for=\"srfm-input-bb2839a9-lbl-Rmlyc3QgTmFtZQ\" class=\"srfm-block-label\">\n\t\t\t\t\t\tVorname\t\t\t\t\t\t\t\t\t\t\t\t\t<span class=\"srfm-required\" aria-hidden=\"true\"> *<\/span>\n\t\t\t\t\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-block-wrap\">\n\t\t\t\t<input class=\"srfm-input-common srfm-input-input\" type=\"text\" name=\"srfm-input-bb2839a9-lbl-Rmlyc3QgTmFtZQ-text-field\" id=\"srfm-input-bb2839a9-lbl-Rmlyc3QgTmFtZQ\"\n\t\t\t\t\taria-describedby='srfm-error-bb2839a9'\t\t\t\t\tdata-required=\"true\" aria-required=\"true\" data-unique=\"false\" maxlength=\"100\" value=\"\"  data-srfm-mask=\"none\"   \/>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"srfm-error-wrap\">\n\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-error-message\" data-srfm-id=\"srfm-error-bb2839a9\" data-error-msg=\"This field is required.\" data-unique-msg=\"Value needs to be unique.\">\n\t\t\t\t\t\tDieses Feld ist erforderlich.\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t<\/div>\n\t\t\n\n\t\t\t<div data-block-id=\"dbaa04c6\" class=\"srfm-block-single srfm-block srfm-input-block srf-input-dbaa04c6-block  srfm-block-width-50 srfm-slug-last-name 305\" >\n\t\t\t\t\t\t\t\t<label id=\"srfm-label-dbaa04c6-lbl-TGFzdCBOYW1l\" for=\"srfm-input-dbaa04c6-lbl-TGFzdCBOYW1l\" class=\"srfm-block-label\">\n\t\t\t\t\t\tNachname\t\t\t\t\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-block-wrap\">\n\t\t\t\t<input class=\"srfm-input-common srfm-input-input\" type=\"text\" name=\"srfm-input-dbaa04c6-lbl-TGFzdCBOYW1l-last-name\" id=\"srfm-input-dbaa04c6-lbl-TGFzdCBOYW1l\"\n\t\t\t\t\taria-describedby='srfm-error-dbaa04c6'\t\t\t\t\tdata-required=\"false\" aria-required=\"false\" data-unique=\"false\" maxlength=\"100\" value=\"\"  data-srfm-mask=\"none\"   \/>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"srfm-error-wrap\">\n\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-error-message\" data-srfm-id=\"srfm-error-dbaa04c6\" data-error-msg=\"This field is required.\" data-unique-msg=\"Value needs to be unique.\">\n\t\t\t\t\t\tDieses Feld ist erforderlich.\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t<\/div>\n\t\t\n\n\t\t\t<div data-block-id=\"80af9bb9\" class=\"srfm-block-single srfm-block srfm-email-block srf-email-80af9bb9-block  srfm-block-width-50 srfm-slug-email 305 srfm-email-block-wrap\">\n\t\t\t\t<div class=\"srfm-email-block srf-email-80af9bb9-block\">\n\t\t\t\t\t\t\t\t\t\t<label id=\"srfm-label-80af9bb9-lbl-RW1haWw\" for=\"srfm-email-80af9bb9-lbl-RW1haWw\" class=\"srfm-block-label\">\n\t\t\t\t\t\tE-Mail\t\t\t\t\t\t\t\t\t\t\t\t\t<span class=\"srfm-required\" aria-hidden=\"true\"> *<\/span>\n\t\t\t\t\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-block-wrap\">\n\t\t\t\t\t\t<input class=\"srfm-input-common srfm-input-email\" type=\"email\" name=\"srfm-email-80af9bb9-lbl-RW1haWw-email\" id=\"srfm-email-80af9bb9-lbl-RW1haWw\"\n\t\t\t\t\t\taria-describedby='srfm-error-80af9bb9'\t\t\t\t\t\tdata-required=\"true\" aria-required=\"true\" data-unique=\"false\" value=\"\"   \/>\n\t\t\t\t\t<\/div>\n\t\t\t\t\t<div class=\"srfm-error-wrap\">\n\t\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-error-message\" data-srfm-id=\"srfm-error-80af9bb9\" data-error-msg=\"This field is required.\" data-unique-msg=\"Value needs to be unique.\">\n\t\t\t\t\t\tDieses Feld ist erforderlich.\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t\t\t<\/div>\n\t\t\n\n\t\t<div data-block-id=\"0c6821ab\" class=\"srfm-block-single srfm-block srfm-phone-block srf-phone-0c6821ab-block srfm-block-width-50 305\">\n\t\t\t\t\t\t\t\t<label id=\"srfm-label-0c6821ab-lbl-UGhvbmUgTnVtYmVy\" for=\"srfm-phone-0c6821ab-lbl-UGhvbmUgTnVtYmVy\" class=\"srfm-block-label\">\n\t\t\t\t\t\tRufnummer\t\t\t\t\t\t\t\t\t\t\t\t\t<span class=\"srfm-required\" aria-hidden=\"true\"> *<\/span>\n\t\t\t\t\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-block-wrap\">\n\t\t\t\t<input type=\"tel\"\n\t\t\t\t\tclass=\"srfm-input-common srfm-input-phone\"\n\t\t\t\t\tname=\"srfm-phone-0c6821ab-lbl-UGhvbmUgTnVtYmVy-phone-number\"\n\t\t\t\t\tid=\"srfm-phone-0c6821ab-lbl-UGhvbmUgTnVtYmVy\"\n\t\t\t\t\taria-describedby='srfm-error-0c6821ab'\t\t\t\t\tdata-required=\"true\"\n\t\t\t\t\taria-required=\"true\"\n\t\t\t\t\tdefault-country=\"us\"\n\t\t\t\t\t\t\t\t\t\tvalue=\"\"\n\t\t\t\t\t\t\t\t\t\tdata-unique=\"false\">\n\t\t\t<\/div>\n\t\t\t<div class=\"srfm-error-wrap\">\n\t\t\t\t\t\t\t\t\t<div class=\"srfm-error-message\" data-srfm-id=\"srfm-error-0c6821ab\" data-error-msg=\"This field is required.\" data-unique-msg=\"Value needs to be unique.\">\n\t\t\t\t\t\tDieses Feld ist erforderlich.\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\n\n\t\t<div data-block-id=\"fabb13d5\" class=\"srfm-block-single srfm-block srfm-textarea-block srf-textarea-fabb13d5-block  srfm-block-width-100 305\">\n\t\t\t\t\t\t\t\t<label id=\"srfm-label-fabb13d5-lbl-WW91ciBNZXNzYWdl-7960\" for=\"srfm-textarea-fabb13d5-lbl-WW91ciBNZXNzYWdl-7960\" class=\"srfm-block-label\">\n\t\t\t\t\t\tIhre Nachricht\t\t\t\t\t\t\t\t\t\t\t\t\t<span class=\"srfm-required\" aria-hidden=\"true\"> *<\/span>\n\t\t\t\t\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-block-wrap\">\n\t\t\t\t<textarea\n\t\t\t\t\tclass=\"srfm-input-common srfm-input-textarea\"\n\t\t\t\t\tname=\"srfm-textarea-fabb13d5-lbl-WW91ciBNZXNzYWdl-your-message\"\n\t\t\t\t\tid=\"srfm-textarea-fabb13d5-lbl-WW91ciBNZXNzYWdl-7960\"\n\t\t\t\t\taria-describedby='srfm-error-fabb13d5'\t\t\t\t\tdata-required=\"true\" aria-required=\"true\"  rows=\"4\"  \t\t\t\t\t\t\t\t\t\t\t\t\t\t\t><\/textarea>\n\t\t\t\t\t\t\t<\/div>\n\t\t\t\t\t\t<div class=\"srfm-error-wrap\">\n\t\t\t\t\t\t\t\t\t<div class=\"srfm-error-message\" data-srfm-id=\"srfm-error-fabb13d5\" data-error-msg=\"This field is required.\">\n\t\t\t\t\t\tDieses Feld ist erforderlich.\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t<\/div>\n\t\t<\/div>\n\n\t\t\t\t\t\t\t\n\t\t\t\t\t\n\t\t\t\t\t<div class=\"srfm-submit-container\" style=\"\">\n\t\t\t\t\t\t<div style=\"width: ; text-align: left\" class=\"wp-block-button\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<button style=\"\" id=\"srfm-submit-btn\" class=\"srfm-btn-frontend srfm-button srfm-submit-button\"\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t>\n\t\t\t\t\t\t\t\t<div class=\"srfm-submit-wrap\">\n\t\t\t\t\t\t\t\t\tEinreichen\t\t\t\t\t\t\t\t<div class=\"srfm-loader\"><\/div>\n\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t<\/button>\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t<p id=\"srfm-error-message\" class=\"srfm-common-error-message srfm-error-message srfm-footer-error\" hidden>\t\t<span class=\"srfm-icon\" aria-hidden=\"true\">\n\t\t\t<svg xmlns=\"http:\/\/www.w3.org\/2000\/svg\" width=\"20\" height=\"20\" fill=\"none\"><path d=\"M9.99935 18.3327C14.6017 18.3327 18.3327 14.6017 18.3327 9.99935C18.3327 5.39698 14.6017 1.66602 9.99935 1.66602C5.39698 1.66602 1.66602 5.39698 1.66602 9.99935C1.66602 14.6017 5.39698 18.3327 9.99935 18.3327Z\" stroke=\"currentColor\" stroke-width=\"1.5\" stroke-linecap=\"round\" stroke-linejoin=\"round\" \/><path d=\"M10 6.66602V9.99935\" stroke=\"currentColor\" stroke-width=\"1.5\" stroke-linecap=\"round\" stroke-linejoin=\"round\" \/><path d=\"M10 13.334H10.0083\" stroke=\"currentColor\" stroke-width=\"1.5\" stroke-linecap=\"round\" stroke-linejoin=\"round\" \/><\/svg>\t\t<\/span>\n\t\t<span class=\"srfm-error-content\">Bei der \u00dcbermittlung Ihres Formulars ist ein Fehler aufgetreten. Bitte versuchen Sie es erneut.<\/span><\/p>\n\t\t\t\t\t<input type=\"hidden\" name=\"trp-form-language\" value=\"de\"\/><\/form>\n\t\t\t<div class=\"srfm-single-form srfm-success-box in-page\">\n\t\t\t\t<div aria-live=\"polite\" aria-atomic=\"true\" role=\"alert\" id=\"srfm-success-message-page-305\" class=\"srfm-success-box-description\"><\/div>\n\t\t\t<\/div>\n\t\t\t\t\t\t<\/div>","protected":false},"excerpt":{"rendered":"<h3><\/h3>\n<p class=\"ds-markdown-paragraph\"><strong>PBT GF30 ist ein technischer Thermoplast auf Basis von Polybutylenterephthalat (PBT), verst\u00e4rkt mit 30%-Glasfasern. Dieser Hochleistungsthermoplast ist die endg\u00fcltige Wahl f\u00fcr Komponenten, die eine robuste Kombination aus struktureller Integrit\u00e4t, thermischer Belastbarkeit und unersch\u00fctterlicher elektrischer Sicherheit in schwierigen Umgebungen erfordern.<\/strong><\/p>\n<p class=\"ds-markdown-paragraph\"><strong>Warum sollten Sie sich f\u00fcr unser PBT GF30 entscheiden?<\/strong><br \/>\n\u2705\u00a0<strong>Die endg\u00fcltige Qualit\u00e4t f\u00fcr anspruchsvolle Anwendungen<\/strong>: Wir liefern das Benchmark-Material, bei dem es keine Kompromisse bei der Leistung gibt und das die ideale Synergie aus Festigkeit, Stabilit\u00e4t und elektrischer Isolierung bietet.<br \/>\n\u2705\u00a0<strong>Entwickelt f\u00fcr Zuverl\u00e4ssigkeit unter Stress<\/strong>: Unser PBT GF30 ist so formuliert, dass es bei Dauerbelastung und hohen Temperaturen eine gleichbleibende Leistung erbringt und die Haltbarkeit Ihrer kritischen Konstruktionen garantiert.<br \/>\n\u2705\u00a0<strong>Kompetente Partnerschaft f\u00fcr komplexe L\u00f6sungen<\/strong>: Wir bieten umfassende technische Unterst\u00fctzung, um die Verarbeitung und Anwendung von PBT GF30 zu optimieren und den Erfolg Ihrer anspruchsvollsten Projekte zu gew\u00e4hrleisten.<br \/>\n\u2705\u00a0<strong>Innovationsf\u00f6rderung in kritischen Sektoren<\/strong>: Wir erm\u00f6glichen Fortschritte in der Automobilindustrie, der industriellen Automatisierung und der Energieverteilung, indem wir ein Material liefern, das strenge technische und Sicherheitsstandards erf\u00fcllt.<\/p>\n<div data-elementor-type=\"page\" data-elementor-id=\"3469\" class=\"elementor elementor-3469\" data-elementor-post-type=\"elementor_library\">\n<div class=\"elementor-element elementor-element-753a2e7 e-grid e-con-boxed e-con e-parent\" data-id=\"753a2e7\" data-element_type=\"container\" data-e-type=\"container\">\n<div class=\"e-con-inner\">\n<div class=\"elementor-element elementor-element-aaa8317 elementor-button-warning elementor-widget elementor-widget-button\" data-id=\"aaa8317\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"button.default\">\n<div class=\"elementor-widget-container\">\n<div class=\"elementor-button-wrapper\">\n\t\t\t\t\t<a class=\"elementor-button elementor-button-link elementor-size-sm\" href=\"#elementor-action%3Aaction%3Dpopup%3Aopen%26settings%3DeyJpZCI6IjI0MDQiLCJ0b2dnbGUiOmZhbHNlfQ%3D%3D\"><br \/>\n\t\t\t\t\t\t<span class=\"elementor-button-content-wrapper\"><br \/>\n\t\t\t\t\t\t\t\t\t<span class=\"elementor-button-text\">Senden Sie Ihre Datei<\/span><br \/>\n\t\t\t\t\t<\/span><br \/>\n\t\t\t\t\t<\/a>\n\t\t\t\t<\/div>\n<\/p><\/div>\n<\/p><\/div>\n<div class=\"elementor-element elementor-element-69ce54b elementor-button-success elementor-widget elementor-widget-button\" data-id=\"69ce54b\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"button.default\">\n<div class=\"elementor-widget-container\">\n<div class=\"elementor-button-wrapper\">\n\t\t\t\t\t<a class=\"elementor-button elementor-button-link elementor-size-sm\" href=\"https:\/\/nylonplastic.com\/de\/kontakt\/\"><br \/>\n\t\t\t\t\t\t<span class=\"elementor-button-content-wrapper\"><br \/>\n\t\t\t\t\t\t\t\t\t<span class=\"elementor-button-text\">Kontakt<\/span><br \/>\n\t\t\t\t\t<\/span><br \/>\n\t\t\t\t\t<\/a>\n\t\t\t\t<\/div>\n<\/p><\/div>\n<\/p><\/div>\n<\/p><\/div>\n<\/p><\/div>\n<\/p><\/div>","protected":false},"featured_media":1313,"comment_status":"closed","ping_status":"closed","template":"","meta":{"rop_custom_images_group":[],"rop_custom_messages_group":[],"rop_publish_now":"initial","rop_publish_now_accounts":{"facebook_846085238273622_899381133262461":""},"rop_publish_now_history":[],"rop_publish_now_status":"pending","site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"default","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","ast-disable-related-posts":"","theme-transparent-header-meta":"default","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"set","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}}},"product_brand":[43],"product_cat":[67],"product_tag":[],"class_list":["post-2924","product","type-product","status-publish","has-post-thumbnail","product_brand-nylon-plastic","product_cat-polybutylene-terephthalate","desktop-align-left","tablet-align-left","mobile-align-left","first","instock","shipping-taxable","product-type-simple"],"_links":{"self":[{"href":"https:\/\/nylonplastic.com\/de\/wp-json\/wp\/v2\/product\/2924","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nylonplastic.com\/de\/wp-json\/wp\/v2\/product"}],"about":[{"href":"https:\/\/nylonplastic.com\/de\/wp-json\/wp\/v2\/types\/product"}],"replies":[{"embeddable":true,"href":"https:\/\/nylonplastic.com\/de\/wp-json\/wp\/v2\/comments?post=2924"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nylonplastic.com\/de\/wp-json\/wp\/v2\/media\/1313"}],"wp:attachment":[{"href":"https:\/\/nylonplastic.com\/de\/wp-json\/wp\/v2\/media?parent=2924"}],"wp:term":[{"taxonomy":"product_brand","embeddable":true,"href":"https:\/\/nylonplastic.com\/de\/wp-json\/wp\/v2\/product_brand?post=2924"},{"taxonomy":"product_cat","embeddable":true,"href":"https:\/\/nylonplastic.com\/de\/wp-json\/wp\/v2\/product_cat?post=2924"},{"taxonomy":"product_tag","embeddable":true,"href":"https:\/\/nylonplastic.com\/de\/wp-json\/wp\/v2\/product_tag?post=2924"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}