{"id":2790,"date":"2025-12-25T08:48:26","date_gmt":"2025-12-25T08:48:26","guid":{"rendered":"https:\/\/nylonplastic.com\/?post_type=product&#038;p=2790"},"modified":"2025-12-25T10:06:19","modified_gmt":"2025-12-25T10:06:19","slug":"pa6-gf30-frv0","status":"publish","type":"product","link":"https:\/\/nylonplastic.com\/ja\/%e8%a3%bd%e5%93%81\/pa6-gf30-frv0\/","title":{"rendered":"PA6 GF30 FR(V0) \u9ad8\u6027\u80fdV-0\u30ca\u30a4\u30ed\u30f36\u30b0\u30ec\u30fc\u30c9"},"content":{"rendered":"<h2><a href=\"https:\/\/www.wanhan-plastic.com\/\"><img fetchpriority=\"high\" decoding=\"async\" class=\"alignnone wp-image-2406 size-full\" src=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_01-e1763968617686.jpg\" alt=\"\u4e07\u7ff0\u8be6\u60c5 01\" width=\"800\" height=\"937\"  title=\"PA6 GF30 FR(V0) \u9ad8\u6027\u80fdV-0\u30ca\u30a4\u30ed\u30f36\u30b0\u30ec\u30fc\u30c9\" srcset=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_01-e1763968617686.jpg 800w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_01-e1763968617686-256x300.jpg 256w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_01-e1763968617686-768x900.jpg 768w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_01-e1763968617686-600x703.jpg 600w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/a><\/h2>\n<h3><strong>PA6 GF30 FR(V0) Technical Data (Estimated Typical Values)<\/strong><\/h3>\n<div class=\"ds-scroll-area _1210dd7 c03cafe9\">\n<div class=\"ds-scroll-area__gutters\">\n<div class=\"ds-scroll-area__vertical-gutter\"><\/div>\n<\/div>\n<table>\n<thead>\n<tr>\n<th>\u30d7\u30ed\u30d1\u30c6\u30a3<\/th>\n<th>\u4fa1\u5024<\/th>\n<th>\u30c6\u30b9\u30c8\u57fa\u6e96<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>\u30ac\u30e9\u30b9\u7e4a\u7dad\u542b\u6709\u91cf<\/strong><\/td>\n<td>30%<\/td>\n<td>ISO 1172<\/td>\n<\/tr>\n<tr>\n<td><strong>\u96e3\u71c3\u6027<\/strong><\/td>\n<td>UL94 V-0\uff08\u898f\u5b9a\u539a\u3055\u306b\u304a\u3044\u3066\uff09<\/td>\n<td>UL 94<\/td>\n<\/tr>\n<tr>\n<td><strong>\u5f15\u5f35\u5f37\u5ea6<\/strong><\/td>\n<td>140 &#8211; 175 MPa<\/td>\n<td>ISO 527<\/td>\n<\/tr>\n<tr>\n<td><strong>\u66f2\u3052\u5f3e\u6027\u7387<\/strong><\/td>\n<td>7,000 &#8211; 9,000 MPa<\/td>\n<td>ISO 178<\/td>\n<\/tr>\n<tr>\n<td><strong>\u30ce\u30c3\u30c1\u4ed8\u304d\u885d\u6483\u5f37\u5ea6<\/strong><\/td>\n<td>10 - 14 kJ\/m\u00b2<\/td>\n<td>ISO 180<\/td>\n<\/tr>\n<tr>\n<td><strong>HDT @1.8 MPa<\/strong><\/td>\n<td>205 - 215 \u00b0C<\/td>\n<td>ISO 75<\/td>\n<\/tr>\n<tr>\n<td><strong>\u878d\u70b9<\/strong><\/td>\n<td>215 - 225 \u00b0C<\/td>\n<td>ISO 3146<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<h3><strong>PA6 FR\u30b7\u30ea\u30fc\u30ba\u6027\u80fd\u6bd4\u8f03\u8868\uff08\u66f4\u65b0\uff09<\/strong><\/h3>\n<div class=\"ds-scroll-area _1210dd7 c03cafe9\">\n<div class=\"ds-scroll-area__gutters\">\n<div class=\"ds-scroll-area__horizontal-gutter\">\n<div class=\"ds-scroll-area__horizontal-bar\"><\/div>\n<\/div>\n<\/div>\n<table>\n<thead>\n<tr>\n<th>\u30d7\u30ed\u30d1\u30c6\u30a3<\/th>\n<th><strong>PA6 FR(V0)<\/strong><\/th>\n<th><strong>PA6 GF15 FR(V0)<\/strong><\/th>\n<th><strong>PA6 GF25 FR(V0)<\/strong><\/th>\n<th><strong>PA6 GF30 FR(V0)<\/strong><\/th>\n<th><strong>PA6 GF50 FR(V0)<\/strong><\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>\u30ac\u30e9\u30b9\u7e4a\u7dad\u542b\u6709\u91cf<\/strong><\/td>\n<td>0%<\/td>\n<td>15%<\/td>\n<td>25%<\/td>\n<td><strong>30%<\/strong><\/td>\n<td>50%<\/td>\n<\/tr>\n<tr>\n<td><strong>\u96e3\u71c3\u6027<\/strong><\/td>\n<td>UL94 V-0<\/td>\n<td>UL94 V-0<\/td>\n<td>UL94 V-0<\/td>\n<td><strong>UL94 V-0<\/strong><\/td>\n<td>UL94 V-0<\/td>\n<\/tr>\n<tr>\n<td><strong>\u5f15\u5f35\u5f37\u5ea6<\/strong><\/td>\n<td>~65 MPa<\/td>\n<td>~110 MPa<\/td>\n<td>~140 MPa<\/td>\n<td><strong>~155 MPa<\/strong><\/td>\n<td>~195MPa\u307e\u3067<\/td>\n<\/tr>\n<tr>\n<td><strong>\u66f2\u3052\u5f3e\u6027\u7387<\/strong><\/td>\n<td>~2,800 MPa<\/td>\n<td>~5,000 MPa<\/td>\n<td>~7,500 MPa<\/td>\n<td><strong>~8,200 MPa<\/strong><\/td>\n<td>~12,500 MPa<\/td>\n<\/tr>\n<tr>\n<td><strong>\u30ce\u30c3\u30c1\u4ed8\u304d\u30a4\u30f3\u30d1\u30af\u30c8<\/strong><\/td>\n<td>~5 kJ\/m\u00b2<\/td>\n<td>~9 kJ\/m\u00b2<\/td>\n<td>~10 kJ\/m\u00b2<\/td>\n<td><strong>~11 kJ\/m\u00b2<\/strong><\/td>\n<td>~9 kJ\/m\u00b2<\/td>\n<\/tr>\n<tr>\n<td><strong>HDT @1.8MPa<\/strong><\/td>\n<td>~75 \u00b0C<\/td>\n<td>~200 \u00b0C<\/td>\n<td>~205 \u00b0C<\/td>\n<td><strong>~210 \u00b0C<\/strong><\/td>\n<td>~215 \u00b0C<\/td>\n<\/tr>\n<tr>\n<td><strong>\u4e3b\u306a\u30d7\u30ed\u30d5\u30a3\u30fc\u30eb<\/strong><\/td>\n<td>\u30d9\u30fc\u30b7\u30c3\u30af\u306aFR\u3001\u7d4c\u6e08\u7684<\/td>\n<td>\u30d0\u30e9\u30f3\u30b9\u306e\u53d6\u308c\u305fFR\u30d1\u30d5\u30a9\u30fc\u30de\u30fc<\/td>\n<td>\u9ad8\u525b\u6027FR\u30b0\u30ec\u30fc\u30c9<\/td>\n<td><strong>\u30d7\u30ec\u30df\u30a2\u30e0\u30fb\u30aa\u30fc\u30eb\u30e9\u30a6\u30f3\u30c9FR<\/strong><\/td>\n<td>\u8d85\u9ad8\u525b\u6027FR\u30b3\u30f3\u30dd\u30b8\u30c3\u30c8<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<h3><strong>Key Advantages of PA6 GF30 FR(V0)<\/strong><\/h3>\n<h4><img decoding=\"async\" class=\"emoji\" role=\"img\" draggable=\"false\" src=\"https:\/\/s.w.org\/images\/core\/emoji\/16.0.1\/svg\/2705.svg\" alt=\"\u2705\"  title=\"PA6 GF30 FR(V0) \u9ad8\u6027\u80fdV-0\u30ca\u30a4\u30ed\u30f36\u30b0\u30ec\u30fc\u30c9\" \/><strong>Unmatched All-Round Performance:<\/strong><\/h4>\n<p class=\"ds-markdown-paragraph\">Delivers the best-in-class combination of high tensile strength, stiffness, and heat deflection temperature within the PA6 FR series.<\/p>\n<h4><img decoding=\"async\" class=\"emoji\" role=\"img\" draggable=\"false\" src=\"https:\/\/s.w.org\/images\/core\/emoji\/16.0.1\/svg\/2705.svg\" alt=\"\u2705\"  title=\"PA6 GF30 FR(V0) \u9ad8\u6027\u80fdV-0\u30ca\u30a4\u30ed\u30f36\u30b0\u30ec\u30fc\u30c9\" \/><strong>Exceptional Reliability for Safety-Critical Parts:<\/strong><\/h4>\n<p class=\"ds-markdown-paragraph\">\u00a0Trusted for components where failure is not an option, such as in electrical systems, automotive functional parts, and industrial machinery.<\/p>\n<h4><img decoding=\"async\" class=\"emoji\" role=\"img\" draggable=\"false\" src=\"https:\/\/s.w.org\/images\/core\/emoji\/16.0.1\/svg\/2705.svg\" alt=\"\u2705\"  title=\"PA6 GF30 FR(V0) \u9ad8\u6027\u80fdV-0\u30ca\u30a4\u30ed\u30f36\u30b0\u30ec\u30fc\u30c9\" \/><strong>Excellent Resistance to Creep and Wear:<\/strong><\/h4>\n<p class=\"ds-markdown-paragraph\">Maintains its shape under long-term load and offers good abrasion resistance, extending the service life of gears, bearings, and moving parts.<\/p>\n<h4><img decoding=\"async\" class=\"emoji\" role=\"img\" draggable=\"false\" src=\"https:\/\/s.w.org\/images\/core\/emoji\/16.0.1\/svg\/2705.svg\" alt=\"\u2705\"  title=\"PA6 GF30 FR(V0) \u9ad8\u6027\u80fdV-0\u30ca\u30a4\u30ed\u30f36\u30b0\u30ec\u30fc\u30c9\" \/> <strong>Proven Material for Engineering Solutions:<\/strong><\/h4>\n<p class=\"ds-markdown-paragraph\">Widely specified and validated in demanding engineering applications, offering designers confidence and a wealth of application data.<\/p>\n<h2><strong>\u7523\u696d\u3078\u306e\u5fdc\u7528\uff1a<\/strong><\/h2>\n<p><img decoding=\"async\" class=\"alignnone wp-image-1751 size-full\" src=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/10\/The-Crucial-Role-of-Injection-Molding-in-Automotive-Industry.jpg\" alt=\"\u81ea\u52d5\u8eca\u7523\u696d\u306b\u304a\u3051\u308b\u5c04\u51fa\u6210\u5f62\u306e\u91cd\u8981\u306a\u5f79\u5272\" width=\"1000\" height=\"571\"  title=\"PA6 GF30 FR(V0) \u9ad8\u6027\u80fdV-0\u30ca\u30a4\u30ed\u30f36\u30b0\u30ec\u30fc\u30c9\" srcset=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/10\/The-Crucial-Role-of-Injection-Molding-in-Automotive-Industry.jpg 1000w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/10\/The-Crucial-Role-of-Injection-Molding-in-Automotive-Industry-300x171.jpg 300w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/10\/The-Crucial-Role-of-Injection-Molding-in-Automotive-Industry-768x439.jpg 768w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/10\/The-Crucial-Role-of-Injection-Molding-in-Automotive-Industry-600x343.jpg 600w\" sizes=\"(max-width: 1000px) 100vw, 1000px\" \/><\/p>\n<h3><strong>PA6 FR\u30b7\u30ea\u30fc\u30ba\u30a2\u30d7\u30ea\u30b1\u30fc\u30b7\u30e7\u30f3\u30b7\u30ca\u30ea\u30aa\u3068\u88fd\u54c1\u30ad\u30fc\u30ef\u30fc\u30c9<\/strong><\/h3>\n<div class=\"ds-scroll-area _1210dd7 c03cafe9\">\n<div class=\"ds-scroll-area__gutters\">\n<div class=\"ds-scroll-area__vertical-gutter\"><\/div>\n<\/div>\n<table>\n<thead>\n<tr>\n<th>\u30b0\u30ec\u30fc\u30c9<\/th>\n<th>\u4ee3\u8868\u7684\u306a\u30a2\u30d7\u30ea\u30b1\u30fc\u30b7\u30e7\u30f3\u30fb\u30b7\u30ca\u30ea\u30aa<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>PA6 FR(V0)<\/strong><\/td>\n<td><strong>\u4e00\u822c\u96fb\u6c17\u30fb\u6d88\u8cbb\u8005\u90e8\u54c1<\/strong>\u00a0\u30bd\u30b1\u30c3\u30c8\u3001\u30b9\u30a4\u30c3\u30c1\u30cf\u30a6\u30b8\u30f3\u30b0\u3001\u30e9\u30a4\u30c8\u30c7\u30a3\u30d5\u30e5\u30fc\u30b6\u30fc\u3001\u30b1\u30fc\u30d6\u30eb\u30de\u30cd\u30b8\u30e1\u30f3\u30c8\u30af\u30ea\u30c3\u30d7\u3001\u5c0f\u578b\u5bb6\u96fb\u30cf\u30a6\u30b8\u30f3\u30b0\u3001\u96fb\u5b50\u6a5f\u5668\u30a8\u30f3\u30af\u30ed\u30fc\u30b8\u30e3\u30fc\u3001\u5185\u90e8\u7d76\u7e01\u4f53\u3002.<\/td>\n<\/tr>\n<tr>\n<td><strong>PA6 GF15 FR(V0)<\/strong><\/td>\n<td><strong>\u8010\u4e45\u6d88\u8cbb\u8ca1\u304a\u3088\u3073\u8efd\u5de5\u696d\u90e8\u54c1\uff1a<\/strong>\u00a0\u96fb\u52d5\u5de5\u5177\u306e\u30cf\u30a6\u30b8\u30f3\u30b0\uff08\u672c\u4f53\uff09\u3001\u5bb6\u96fb\u88fd\u54c1\u306e\u69cb\u9020\u90e8\u54c1\u3001\u96fb\u6c17\u63a5\u7d9a\u7bb1\u3001\u63db\u6c17\u6247\u306e\u7fbd\u6839\u3001\u81ea\u52d5\u8eca\u5185\u88c5\u30c8\u30ea\u30e0\u30af\u30ea\u30c3\u30d7\u3001\u30b3\u30cd\u30af\u30bf\u30fc\u306e\u30cf\u30a6\u30b8\u30f3\u30b0.<\/td>\n<\/tr>\n<tr>\n<td><strong>PA6 GF25 FR(V0)<\/strong><\/td>\n<td><strong>\u5f37\u5316\u69cb\u9020\u90e8\u54c1\uff1a<\/strong>\u00a0\u7523\u696d\u7528\u5236\u5fa1\u7b50\u4f53\u3001\u96fb\u6e90\u7b50\u4f53\u3001\u81ea\u52d5\u8eca\u7528\u30d2\u30e5\u30fc\u30ba\u30dc\u30c3\u30af\u30b9\u7b50\u4f53\u3001\u30dd\u30f3\u30d7\u30ab\u30d0\u30fc\u3001\u4e2d\u8ca0\u8377\u30ae\u30a2\u304a\u3088\u3073\u30ec\u30d0\u30fc\u3001\u5bb6\u96fb\u88fd\u54c1\u306e\u6a5f\u80fd\u30d6\u30e9\u30b1\u30c3\u30c8\u3002.<\/td>\n<\/tr>\n<tr>\n<td><strong>PA6 GF30 FR(V0)<\/strong><\/td>\n<td><strong>\u9ad8\u6027\u80fd\u7523\u696d\u304a\u3088\u3073\u81ea\u52d5\u8eca\u90e8\u54c1\uff1a<\/strong>\u00a0\u6a5f\u68b0\u306e\u30ae\u30a2\u30db\u30a4\u30fc\u30eb\u3001\u30d9\u30a2\u30ea\u30f3\u30b0\u30b1\u30fc\u30b8\u3001\u9ad8\u5f37\u5ea6\u30b3\u30cd\u30af\u30bf\u30fc\u3068\u30dc\u30d3\u30f3\u3001\u96fb\u6c17\u81ea\u52d5\u8eca\u5145\u96fb\u30ac\u30f3\u90e8\u54c1\u3001\u5de5\u696d\u7528\u30d5\u30a1\u30f3\u30a4\u30f3\u30da\u30e9\u3001\u81ea\u52d5\u8eca\u30a8\u30f3\u30b8\u30f3\u51b7\u5374\u30d5\u30a1\u30f3\u30b7\u30e5\u30e9\u30a6\u30c9\u3002.<\/td>\n<\/tr>\n<tr>\n<td><strong>PA6 GF50 FR(V0)<\/strong><\/td>\n<td><strong>\u8d85\u9ad8\u525b\u6027\u30b9\u30da\u30b7\u30e3\u30e9\u30a4\u30ba\u30c9\u30fb\u30d1\u30fc\u30c4\uff1a<\/strong>\u00a0\u8efd\u91cf\u69cb\u9020\u30d5\u30ec\u30fc\u30e0\u304a\u3088\u3073\u30d6\u30e9\u30b1\u30c3\u30c8\uff08\u30c9\u30ed\u30fc\u30f3\u3084\u6a5f\u5668\u7528\u306a\u3069\uff09\u3001\u9ad8\u8377\u91cd\u30d9\u30a2\u30ea\u30f3\u30b0\u90e8\u54c1\u3001\u7523\u696d\u30aa\u30fc\u30c8\u30e1\u30fc\u30b7\u30e7\u30f3\u7528\u30ac\u30a4\u30c9\u304a\u3088\u3073\u30ec\u30fc\u30eb\u3001\u30ed\u30dc\u30c3\u30c8\u30a2\u30fc\u30e0\u30ea\u30f3\u30af\u3001\u7279\u6b8a\u5de5\u5177\u304a\u3088\u3073\u6cbb\u5177\u3002.<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<h3><strong> \u696d\u754c\u3092\u8d85\u3048\u305f\u30a4\u30ce\u30d9\u30fc\u30b7\u30e7\u30f3\u306e\u539f\u52d5\u529b<\/strong><\/h3>\n<div class=\"ds-scroll-area _1210dd7 c03cafe9\">\n<div class=\"ds-scroll-area__gutters\">\n<div class=\"ds-scroll-area__vertical-gutter\"><\/div>\n<\/div>\n<table>\n<thead>\n<tr>\n<th>\u7523\u696d<\/th>\n<th>\u4e3b\u306a\u7528\u9014<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong> \u81ea\u52d5\u8eca<\/strong><\/td>\n<td>\u30a8\u30f3\u30b8\u30f3\u30ab\u30d0\u30fc\u3001\u30a4\u30f3\u30c6\u30fc\u30af\u30de\u30cb\u30db\u30fc\u30eb\u30c9\u3001\u69cb\u9020\u7528\u30d6\u30e9\u30b1\u30c3\u30c8\u3001\u30bb\u30f3\u30b5\u30fc\u30cf\u30a6\u30b8\u30f3\u30b0\u3001\u30b3\u30cd\u30af\u30bf\u30fc\u3002.<br \/>\n<strong><a href=\"https:\/\/nylonplastic.com\/ja\/automotive-industry\/\" target=\"_blank\" rel=\"noopener noreferrer\">\u81ea\u52d5\u8eca\u3078\u306e\u5fdc\u7528\u3092\u63a2\u308b<\/a><\/strong><\/td>\n<\/tr>\n<tr>\n<td><strong> \u96fb\u6c17\u30fb\u96fb\u5b50<\/strong><\/td>\n<td>\u30b5\u30fc\u30ad\u30c3\u30c8\u30d6\u30ec\u30fc\u30ab\u30fc\u3001\u30b9\u30a4\u30c3\u30c1\u3001\u30b3\u30cd\u30af\u30bf\u30fc\u30cf\u30a6\u30b8\u30f3\u30b0\u3001\u7d76\u7e01\u90e8\u54c1.<br \/>\n<strong><a href=\"https:\/\/nylonplastic.com\/ja\/electronic-devices\/\" target=\"_blank\" rel=\"noopener noreferrer\">E&amp;E\u30bd\u30ea\u30e5\u30fc\u30b7\u30e7\u30f3\u306e\u767a\u898b \u2192 E&amp;E\u30bd\u30ea\u30e5\u30fc\u30b7\u30e7\u30f3\u306e\u767a\u898b<\/a><\/strong><\/td>\n<\/tr>\n<tr>\n<td><strong> \u7523\u696d\u6a5f\u5668<\/strong><\/td>\n<td>\u30ae\u30a2\u3001\u30d9\u30a2\u30ea\u30f3\u30b0\u3001\u6a5f\u68b0\u30cf\u30a6\u30b8\u30f3\u30b0\u3001\u30ed\u30fc\u30e9\u30fc\u3001\u6a5f\u68b0\u90e8\u54c1\u3002.<br \/>\n<strong><a href=\"https:\/\/nylonplastic.com\/ja\/industrial-equipment\/\" target=\"_blank\" rel=\"noopener noreferrer\">\u5de5\u696d\u7528\u3092\u53c2\u7167 \u2192\u5de5\u696d\u7528<\/a><\/strong><\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<figure id=\"attachment_2409\" aria-describedby=\"caption-attachment-2409\" style=\"width: 800px\" class=\"wp-caption alignnone\"><a href=\"https:\/\/nylonplastic.com\/ja\/industries\/\"><img decoding=\"async\" class=\"wp-image-2409 size-full\" src=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_06.jpg\" alt=\"PA\u30d7\u30e9\u30b9\u30c1\u30c3\u30af\u306e\u69d8\u3005\u306a\u5fdc\u7528\u30b7\u30fc\u30f3\" width=\"800\" height=\"740\"  title=\"PA6 GF30 FR(V0) \u9ad8\u6027\u80fdV-0\u30ca\u30a4\u30ed\u30f36\u30b0\u30ec\u30fc\u30c9\" srcset=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_06.jpg 800w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_06-300x278.jpg 300w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_06-768x710.jpg 768w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_06-600x555.jpg 600w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/a><figcaption id=\"caption-attachment-2409\" class=\"wp-caption-text\">PA\u30d7\u30e9\u30b9\u30c1\u30c3\u30af\u306e\u69d8\u3005\u306a\u5fdc\u7528\u30b7\u30fc\u30f3<\/figcaption><\/figure>\n<\/div>\n<h3><strong>\u6b63\u3057\u3044PA6\u96e3\u71c3\u30b0\u30ec\u30fc\u30c9\u306e\u9078\u3073\u65b9<\/strong><\/h3>\n<p class=\"ds-markdown-paragraph\"><strong>\u308f\u304b\u308a\u3084\u3059\u304f\u8a00\u3048\u3070\u3001\"\u30f4\u30a7\u30cb\u30e5\u30fc \"\u3067\u3042\u308b\uff1a<\/strong><\/p>\n<p class=\"ds-markdown-paragraph\">\u306b\u3064\u3044\u3066\u00a0<strong>\u57fa\u672c\u7684\u306a\u96e3\u71c3\u6027\u3068\u512a\u308c\u305f\u976d\u6027\u3001\u305d\u3057\u3066\u6700\u3082\u4f4e\u3044\u30b3\u30b9\u30c8<\/strong>, \u3068\u8003\u3048\u308b\u3002\u00a0<strong>PA6 FR(V0)<\/strong>\u00a0\u307e\u305f\u306f\u00a0<strong>PA6 GF15 FR(V0)<\/strong>. .\u4e00\u822c\u7684\u306a\u96fb\u6c17\u30cf\u30a6\u30b8\u30f3\u30b0\u3001\u5bb6\u96fb\u90e8\u54c1\u3001\u52a0\u5de5\u306e\u3057\u3084\u3059\u3055\u304c\u91cd\u8981\u306a\u7528\u9014\u306b\u6700\u9069\u3067\u3059\u3002.<\/p>\n<p class=\"ds-markdown-paragraph\">\u306b\u3064\u3044\u3066\u00a0<strong>\u708e\u306b\u5bfe\u3059\u308b\u5b89\u5168\u6027\u3001\u6a5f\u68b0\u7684\u5f37\u5ea6\u3001\u71b1\u7684\u6027\u80fd\u306e\u30d0\u30e9\u30f3\u30b9\u304c\u6700\u3082\u512a\u308c\u3066\u3044\u308b\u3002<\/strong>, \u3092\u9078\u629e\u3059\u308b\u3002\u00a0<strong>PA6 GF30 FR(V0)<\/strong>. .\u30ae\u30a2\u3001\u5de5\u696d\u7528\u30a8\u30f3\u30af\u30ed\u30fc\u30b8\u30e3\u30fc\u3001\u81ea\u52d5\u8eca\u7528\u30a2\u30f3\u30c0\u30fc\u30d5\u30fc\u30c9\u30d5\u30a1\u30f3\u306a\u3069\u3001\u4fe1\u983c\u6027\u306e\u9ad8\u3044\u8010\u4e45\u6027\u304c\u8981\u6c42\u3055\u308c\u308b\u90e8\u54c1\u306b\u9069\u3057\u305f\u30b0\u30ec\u30fc\u30c9\u3067\u3059\u3002.<\/p>\n<p class=\"ds-markdown-paragraph\">\u306b\u3064\u3044\u3066\u00a0<strong>\u6700\u5927\u9650\u306e\u525b\u6027\u3068\u5bf8\u6cd5\u5b89\u5b9a\u6027\u304c\u8981\u6c42\u3055\u308c\u308b\u7528\u9014\u3067\u3001V-0\u898f\u683c\u306b\u9069\u5408\u3002<\/strong>, \u3068\u8003\u3048\u308b\u3002\u00a0<strong>PA6 GF50 FR(V0)<\/strong>. .\u3053\u306e\u8d85\u9ad8\u5f3e\u6027\u7387\u30b0\u30ec\u30fc\u30c9\u306f\u3001\u8efd\u91cf\u5316\u304c\u91cd\u8981\u306a\u69cb\u9020\u8a2d\u8a08\u306b\u304a\u3044\u3066\u91d1\u5c5e\u306e\u4ee3\u66ff\u3092\u53ef\u80fd\u306b\u3059\u308b\u3002.<\/p>\n<p class=\"ds-markdown-paragraph\"><strong>\u3069\u308c\u304c\u3042\u306a\u305f\u306e\u30d1\u30fc\u30c8\u306b\u6700\u9069\u304b\u308f\u304b\u3089\u306a\u3044\uff1f<\/strong>\u00a0\u304a\u5ba2\u69d8\u306e\u7528\u9014\u3092\u5f53\u793e\u306e\u30a8\u30f3\u30b8\u30cb\u30a2\u306b\u3054\u8aac\u660e\u304f\u3060\u3055\u3044\uff1a\u00a0<strong><a href=\"https:\/\/nylonplastic.com\/ja\/contact\/\" target=\"_blank\" rel=\"noopener noreferrer\">https:\/\/nylonplastic.com\/contact\/<\/a><\/strong><\/p>\n<p class=\"ds-markdown-paragraph\"><strong style=\"font-size: 1.7em;\">\u5f53\u793e\u3092\u9078\u3076\u7406\u7531<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone wp-image-2407 size-full\" src=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_03.jpg\" alt=\"\u4e07\u7ff0\u8be6\u60c5 03\" width=\"800\" height=\"673\"  title=\"PA6 GF30 FR(V0) \u9ad8\u6027\u80fdV-0\u30ca\u30a4\u30ed\u30f36\u30b0\u30ec\u30fc\u30c9\" srcset=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_03.jpg 800w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_03-300x252.jpg 300w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_03-768x646.jpg 768w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_03-600x505.jpg 600w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone wp-image-2408 size-full\" src=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_04.jpg\" alt=\"\u4e07\u7ff0\u8be6\u60c5 04\" width=\"800\" height=\"576\"  title=\"PA6 GF30 FR(V0) \u9ad8\u6027\u80fdV-0\u30ca\u30a4\u30ed\u30f36\u30b0\u30ec\u30fc\u30c9\" srcset=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_04.jpg 800w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_04-300x216.jpg 300w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_04-768x553.jpg 768w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_04-600x432.jpg 600w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/p>\n<h3><strong>PA6 FR\u30b7\u30ea\u30fc\u30ba\u3088\u304f\u3042\u308b\u8cea\u554f\uff08FAQ\uff09<\/strong><\/h3>\n<p class=\"ds-markdown-paragraph\"><strong>Q1: PA6 FR(V0)\u6750\u3068\u306f\u4f55\u3067\u3059\u304b\uff1f<\/strong><br \/>\n<strong>A1:<\/strong>\u00a0PA6 FR(V0)\u306f\u3001\u30ca\u30a4\u30ed\u30f36\uff08\u30dd\u30ea\u30a2\u30df\u30c96\uff09\u306e\u96e3\u71c3\u30b0\u30ec\u30fc\u30c9\u3067\u3001\u6b21\u306e\u3088\u3046\u306a\u53b3\u3057\u3044\u6761\u4ef6\u3092\u6e80\u305f\u3057\u3066\u3044\u307e\u3059\u3002\u00a0<strong>UL94 V-0\u898f\u683c<\/strong>, \u3064\u307e\u308a\u3001\u5782\u76f4\u71c3\u713c\u8a66\u9a13\u3067\u6570\u79d2\u4ee5\u5185\u306b\u71c3\u713c\u3092\u505c\u6b62\u3055\u305b\u308b\u3053\u3068\u304c\u3067\u304d\u308b\u3002\u4e3b\u306a\u7279\u5fb4\u306f\u4ee5\u4e0b\u306e\u901a\u308a\u3002\u00a0<strong>\u976d\u6027\u3068\u512a\u308c\u305f\u96fb\u6c17\u7d76\u7e01\u6027\u306e\u30d0\u30e9\u30f3\u30b9\u304c\u826f\u304f\u3001\u6bd4\u8f03\u7684\u5b89\u4fa1\u3067\u3042\u308b\u3002<\/strong>\u00a0\u3088\u308a\u9ad8\u6027\u80fd\u306a\u30a8\u30f3\u30b8\u30cb\u30a2\u30ea\u30f3\u30b0\u30fb\u30d7\u30e9\u30b9\u30c1\u30c3\u30af\u306b\u6bd4\u3079\u96fb\u6c17\u30fb\u96fb\u5b50\u90e8\u54c1\u306b\u5e83\u304f\u4f7f\u7528\u3055\u308c\u3066\u3044\u308b\u3002.<\/p>\n<p class=\"ds-markdown-paragraph\"><strong>Q2: PA6 FR(V0)\u3001PA6 GF30 FR(V0)\u3001PA6 GF50 FR(V0)\u306e\u9055\u3044\u306f\u4f55\u3067\u3059\u304b\uff1f<\/strong><br \/>\n<strong>A2:<\/strong>\u00a0\u6838\u5fc3\u7684\u306a\u9055\u3044\u306f\u6b21\u306e\u70b9\u306b\u3042\u308b\u3002\u00a0<strong>\u30ac\u30e9\u30b9\u7e4a\u7dad\uff08GF\uff09\u542b\u6709\u91cf<\/strong>\u00a0\u3068\u3001\u305d\u306e\u7d50\u679c\u5f97\u3089\u308c\u308b\u6a5f\u68b0\u7684\u7279\u6027\uff1a<\/p>\n<ul>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong>PA6 FR(V0)<\/strong>:\u5185\u5bb9\u00a0<strong>0%\u30b0\u30e9\u30b9\u30d5\u30a1\u30a4\u30d0\u30fc<\/strong>. .\u4ee5\u4e0b\u306e\u3088\u3046\u306a\u7528\u9014\u306b\u6700\u9069\u3067\u3059\u3002\u00a0<strong>\u96e3\u71c3\u6027\u3068\u826f\u597d\u306a\u52a0\u5de5\u6027\u304c\u4e3b\u306a\u8981\u4ef6\u3067\u3042\u308b\u3002<\/strong>, \u9ad8\u3044\u69cb\u9020\u5f37\u5ea6\u3092\u5fc5\u8981\u3068\u3057\u306a\u3044\u3002.<\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong>PA6 GF30 FR(V0)<\/strong>:\u3067\u88dc\u5f37\u00a0<strong>30%\u30ac\u30e9\u30b9\u7e4a\u7dad<\/strong>. .\u3092\u63d0\u4f9b\u3059\u308b\u3002\u00a0<strong>\u9ad8\u5f37\u5ea6\u3001\u9ad8\u525b\u6027\u3001\u8010\u71b1\u6027\uff08HDT &gt;200\u2103\uff09\u3001V-0\u30ec\u30fc\u30c6\u30a3\u30f3\u30b0\u306e\u512a\u308c\u305f\u30d0\u30e9\u30f3\u30b9<\/strong>, \u305d\u306e\u305f\u3081\u3001\u8981\u6c42\u306e\u53b3\u3057\u3044\u69cb\u9020\u90e8\u54c1\u7528\u3068\u3057\u3066\u6700\u3082\u6c4e\u7528\u6027\u306e\u9ad8\u3044\u30b0\u30ec\u30fc\u30c9\u3068\u306a\u3063\u3066\u3044\u308b\u3002.<\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong>PA6 GF50 FR(V0)<\/strong>:\u5185\u5bb9\u00a0<strong>50%\u30ac\u30e9\u30b9\u7e4a\u7dad<\/strong>, \u3092\u63d0\u4f9b\u3059\u308b\u3002\u00a0<strong>\u6700\u9ad8\u306e\u525b\u6027\u3068\u5bf8\u6cd5\u5b89\u5b9a\u6027<\/strong>\u00a0\u306e\u30b7\u30ea\u30fc\u30ba\u306b\u542b\u307e\u308c\u308b\u3002\u3053\u308c\u306f\u00a0<strong>\u91d1\u5c5e\u4ea4\u63db<\/strong>\u00a0\u9632\u706b\u5b89\u5168\u6027\u3068\u3068\u3082\u306b\u6975\u3081\u3066\u9ad8\u3044\u525b\u6027\u304c\u8981\u6c42\u3055\u308c\u308b\u7528\u9014\u3067\u4f7f\u7528\u3055\u308c\u308b\u3002.<\/p>\n<\/li>\n<\/ul>\n<p class=\"ds-markdown-paragraph\"><strong>Q3: \u81ea\u5206\u306e\u7528\u9014\u306b\u9069\u3057\u305fPA6 FR\u30b0\u30ec\u30fc\u30c9\u3092\u9078\u3076\u306b\u306f\u3069\u3046\u3059\u308c\u3070\u3088\u3044\u3067\u3059\u304b\uff1f<\/strong><br \/>\n<strong>A3:<\/strong>\u00a0\u3042\u306a\u305f\u306e\u4e3b\u306a\u5fc5\u8981\u6027\u306b\u57fa\u3065\u3044\u3066\u3001\u3053\u306e\u30b7\u30f3\u30d7\u30eb\u306a\u30ac\u30a4\u30c9\u30e9\u30a4\u30f3\u306b\u5f93\u3063\u3066\u304f\u3060\u3055\u3044\uff1a<\/p>\n<ul>\n<li>\n<p class=\"ds-markdown-paragraph\">\u306b\u3064\u3044\u3066\u00a0<strong>\u57fa\u672c\u7684\u306a\u708e\u306e\u5b89\u5168\u6027\u3068\u6700\u4f4e\u30b3\u30b9\u30c8<\/strong>\u00a0\u975e\u69cb\u9020\u90e8\u54c1\uff08\u4f8b\uff1a\u30cf\u30a6\u30b8\u30f3\u30b0\u3001\u30ab\u30d0\u30fc\uff09\u3067\u306f\u3001\u4ee5\u4e0b\u3092\u9078\u629e\u3059\u308b\u3002\u00a0<strong>PA6 FR(V0)<\/strong>.<\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\">\u306b\u3064\u3044\u3066\u306f\u00a0<strong>\u30d9\u30b9\u30c8\u30fb\u30aa\u30fc\u30eb\u30e9\u30a6\u30f3\u30c9\u30fb\u30d1\u30d5\u30a9\u30fc\u30de\u30f3\u30b9<\/strong>\u00a0\u5f37\u5ea6\u3001\u8010\u71b1\u6027\u3001\u96e3\u71c3\u6027\uff08\u4f8b\uff1a\u30ae\u30a2\u3001\u30b3\u30cd\u30af\u30bf\u30fc\u3001\u30a8\u30f3\u30af\u30ed\u30fc\u30b8\u30e3\u30fc\uff09\u306e\u89b3\u70b9\u304b\u3089\u3001\u4ee5\u4e0b\u306e\u3082\u306e\u3092\u9078\u629e\u3059\u308b\u3002\u00a0<strong>PA6 GF30 FR(V0)<\/strong>.<\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\">\u306b\u3064\u3044\u3066\u00a0<strong>\u6700\u5927\u525b\u6027\u3068\u8010\u8377\u91cd<\/strong>\u00a0\u90e8\u54c1\u306e\u305f\u308f\u307f\u3092\u6700\u5c0f\u306b\u3057\u306a\u3051\u308c\u3070\u306a\u3089\u306a\u3044\u5834\u5408\u306f\u3001\u6b21\u306e\u3088\u3046\u306b\u9078\u3076\u3002\u00a0<strong>PA6 GF50 FR(V0)<\/strong>.<br \/>\n\u6b63\u78ba\u306a\u63a8\u5968\u3092\u3054\u5e0c\u671b\u306e\u5834\u5408\u306f\u3001\u5177\u4f53\u7684\u306a\u90e8\u54c1\u8a2d\u8a08\u3068\u8981\u4ef6\u3092\u5f0a\u793e\u30a8\u30f3\u30b8\u30cb\u30a2\u30ea\u30f3\u30b0\u30fb\u30c1\u30fc\u30e0\u307e\u3067\u3054\u9023\u7d61\u304f\u3060\u3055\u3044\u3002.<\/p>\n<\/li>\n<\/ul>\n<p class=\"ds-markdown-paragraph\"><strong>Q4: PA6 FR\u30b0\u30ec\u30fc\u30c9\u306f\u91d1\u5c5e\u90e8\u54c1\u306e\u4ee3\u66ff\u306b\u306a\u308a\u307e\u3059\u304b\uff1f<\/strong><br \/>\n<strong>A4\uff1a\u306f\u3044\u3001\u7279\u306b\u30ac\u30e9\u30b9\u5f37\u5316\u30b0\u30ec\u30fc\u30c9\u306f\u305d\u3046\u3067\u3059\u3002.<\/strong>\u00a0<strong>PA6 GF50 FR(V0)<\/strong>, \u305d\u306e\u8d85\u9ad8\u5f3e\u6027\u7387\u306f\u3001\u7279\u306b\u6b21\u306e\u3088\u3046\u306a\u7528\u9014\u306b\u8a2d\u8a08\u3055\u308c\u3066\u3044\u308b\u3002\u00a0<strong>\u8efd\u91cf\u91d1\u5c5e\u4ea4\u63db<\/strong>. .\u7279\u5b9a\u306e\u69cb\u9020\u7528\u9014\u306b\u304a\u3044\u3066\u30a2\u30eb\u30df\u30cb\u30a6\u30e0\u306e\u3088\u3046\u306a\u91d1\u5c5e\u306b\u53d6\u3063\u3066\u4ee3\u308f\u308b\u3053\u3068\u304c\u3067\u304d\u3001\u5927\u5e45\u306a\u8efd\u91cf\u5316\u3001\u8010\u98df\u6027\u3001\u8a2d\u8a08\u306e\u81ea\u7531\u5ea6\u3092\u63d0\u4f9b\u3059\u308b\u4e00\u65b9\u3067\u3001\u305d\u306e\u6027\u80fd\u306f\u7dad\u6301\u3055\u308c\u308b\u3002\u00a0<strong>V-0\u96e3\u71c3\u6027<\/strong>. .\u305d\u306e\u9078\u629e\u306f\u3001\u7279\u5b9a\u306e\u8ca0\u8377\u3001\u6e29\u5ea6\u3001\u74b0\u5883\u6761\u4ef6\u306b\u3088\u3063\u3066\u7570\u306a\u308b\u3002.<\/p>\n<p class=\"ds-markdown-paragraph\"><strong>Q5: PA6 FR\u6750\u306f\u85ac\u54c1\u3084\u9ad8\u6e29\u306b\u5f37\u3044\u306e\u3067\u3059\u304b\uff1f<\/strong><br \/>\n<strong>A5:<\/strong>\u00a0PA6 FR\u30b0\u30ec\u30fc\u30c9\u306f\u3001\u591a\u304f\u306e\u6750\u6599\u306b\u5bfe\u3059\u308b\u512a\u308c\u305f\u8010\u6027\u3092\u53d7\u3051\u7d99\u3044\u3067\u3044\u308b\u3002\u00a0<strong>\u30aa\u30a4\u30eb\u3001\u30b0\u30ea\u30fc\u30b9\u3001\u70ad\u5316\u6c34\u7d20<\/strong>\u00a0\u30d9\u30fc\u30b9\u306e\u30ca\u30a4\u30ed\u30f36\u304b\u3089\u3002\u6e29\u5ea6\u306b\u3064\u3044\u3066<\/p>\n<ul>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong>\u9023\u7d9a\u4f7f\u7528\u6e29\u5ea6<\/strong>:\u96fb\u6c17\u304a\u3088\u3073\u81ea\u52d5\u8eca\u7528\u9014\u3067\u4e00\u822c\u7684\u306a\u9ad8\u6e29\u74b0\u5883\u3067\u306e\u9577\u671f\u4f7f\u7528\u306b\u9069\u3057\u3066\u3044\u308b\u3002.<\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong>\u71b1\u504f\u5411\u6e29\u5ea6\uff08HDT\uff09<\/strong>:\u3053\u308c\u306f\u30ac\u30e9\u30b9\u7e4a\u7dad\u306e\u542b\u6709\u91cf\u306b\u3088\u3063\u3066\u5897\u52a0\u3059\u308b\u3002\u4f8b\u3048\u3070,\u00a0<strong>PA6 GF30 FR(V0)<\/strong>\u00a0\u306f\u3001\u975e\u5f37\u5316FR(V0)\u30b0\u30ec\u30fc\u30c9\u3088\u308a\u3082HDT\u304c\u8457\u3057\u304f\u9ad8\u304f\u3001\u3088\u308a\u9ad8\u3044\u71b1\u8ca0\u8377\u4e0b\u3067\u3082\u5b89\u5b9a\u3057\u3066\u3044\u308b\u3002.<br \/>\n\u6b63\u78ba\u306a\u5316\u5b66\u7684\u9069\u5408\u6027\u3068\u71b1\u6027\u80fd\u306e\u30c7\u30fc\u30bf\u306b\u3064\u3044\u3066\u306f\u3001\u5fc5\u305a\u7279\u5b9a\u306e\u6750\u6599\u306e\u30c7\u30fc\u30bf\u30b7\u30fc\u30c8\u3092\u53c2\u7167\u3057\u3066\u304f\u3060\u3055\u3044\u3002.<\/p>\n<\/li>\n<\/ul>\n<p class=\"ds-markdown-paragraph\"><strong>Q6: PA6 FR\u6750\u3092\u52a0\u5de5\uff08\u5c04\u51fa\u6210\u5f62\uff09\u3059\u308b\u969b\u306e\u6ce8\u610f\u70b9\u306f\uff1f<\/strong><br \/>\n<strong>A6:<\/strong>\u00a0\u4e3b\u306a\u51e6\u7406\u4e0a\u306e\u6ce8\u610f\u70b9\u306f\u4ee5\u4e0b\u306e\u901a\u308a\uff1a<\/p>\n<ol start=\"1\">\n<li>\n<p class=\"ds-markdown-paragraph\"><strong>\u4e7e\u71e5<\/strong>:PA6\u306f\u5438\u6e7f\u6027\u304c\u3042\u308b\u3002.\u00a0<strong>\u9069\u5207\u306a\u4e7e\u71e5<\/strong>\u00a0(\u4f8b\u3048\u3070\u300180\uff5e90\u2103\u30674\u6642\u9593\u4ee5\u4e0a\uff09\u306f\u00a0<strong>\u5fc5\u8981\u4e0d\u53ef\u6b20<\/strong>\u00a0\u52a0\u6c34\u5206\u89e3\u3092\u9632\u304e\u3001\u6700\u9069\u306a\u7279\u6027\u3068\u8868\u9762\u4ed5\u4e0a\u3052\u3092\u4fdd\u8a3c\u3059\u308b\u305f\u3081\u306b\u3001\u52a0\u5de5\u524d\u306b\u3002.<\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong>\u91d1\u578b\u6e29\u5ea6<\/strong>:\u5185\u90e8\u5fdc\u529b\u3092\u4f4e\u6e1b\u3057\u3001\u7d50\u6676\u5316\u5ea6\u3092\u5411\u4e0a\u3055\u305b\u3001\u8868\u9762\u5916\u89b3\u3092\u5411\u4e0a\u3055\u305b\u308b\u305f\u3081\u306b\u306f\u3001\u91d1\u578b\u6e29\u5ea6\u3092\u9ad8\u304f\u3059\u308b\uff08\u4f8b\u3048\u3070\u300180\uff5e100\u2103\uff09\u3053\u3068\u304c\u63a8\u5968\u3055\u308c\u308b\u3002.<\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong>\u30b9\u30af\u30ea\u30e5\u30fc\uff06\u30d0\u30ec\u30eb<\/strong>:\u6c4e\u7528\u306e\u30cd\u30b8\u3092\u4f7f\u7528\u3057\u3066\u304f\u3060\u3055\u3044\u3002\u30d5\u30a3\u30e9\u30fc\u3092\u4f7f\u7528\u3057\u3066\u3044\u308b\u305f\u3081\u3001\u6642\u9593\u306e\u7d4c\u904e\u3068\u3068\u3082\u306b\u6469\u8017\u304c\u767a\u751f\u3059\u308b\u3053\u3068\u304c\u3042\u308a\u307e\u3059\u3002.<br \/>\n\u5f53\u793e\u306e\u6280\u8853\u30c7\u30fc\u30bf\u30b7\u30fc\u30c8\u306b\u306f\u3001\u8a73\u7d30\u306a\u52a0\u5de5\u30ac\u30a4\u30c9\u30e9\u30a4\u30f3\u304c\u8a18\u8f09\u3055\u308c\u3066\u3044\u307e\u3059\u3002.<\/p>\n<\/li>\n<\/ol>\n<p class=\"ds-markdown-paragraph\"><strong>Q7: PA6 FR\u6750\u306e\u30c6\u30af\u30cb\u30ab\u30eb\u30c7\u30fc\u30bf\u30b7\u30fc\u30c8(TDS)\u306e\u5165\u624b\u3084\u30b5\u30f3\u30d7\u30eb\u8acb\u6c42\u306f\u3069\u3053\u3067\u3067\u304d\u307e\u3059\u304b\uff1f<\/strong><br \/>\n<strong>A7:<\/strong>\u00a0\u30c6\u30af\u30cb\u30ab\u30eb\u30c7\u30fc\u30bf\u30b7\u30fc\u30c8\u306f\u3001\u88fd\u54c1\u30da\u30fc\u30b8\u304b\u3089\u30c0\u30a6\u30f3\u30ed\u30fc\u30c9\u3067\u304d\u307e\u3059\u3002\u6b63\u5f0f\u306a\u30ed\u30c3\u30c8\u5225\u30c7\u30fc\u30bf\u30b7\u30fc\u30c8\u307e\u305f\u306f\u00a0<strong>\u30b5\u30f3\u30d7\u30eb\u8acb\u6c42<\/strong>\u00a0\u30c6\u30b9\u30c8\u3068\u691c\u8a3c\u3092\u3054\u5e0c\u671b\u306e\u65b9\u306f\u3001\u5f53\u793e\u306e\u55b6\u696d\u307e\u305f\u306f\u6280\u8853\u30b5\u30dd\u30fc\u30c8\u30c1\u30fc\u30e0\u307e\u3067\u304a\u554f\u3044\u5408\u308f\u305b\u304f\u3060\u3055\u3044\uff1a\u00a0<strong><a href=\"https:\/\/nylonplastic.com\/ja\/contact\/\" target=\"_blank\" rel=\"noopener noreferrer\">https:\/\/nylonplastic.com\/contact\/<\/a><\/strong><\/p>\n\t\t\t<div class=\"srfm-form-container srfm-form-container-305 srfm-bg-color\">\n\t\t\t<style>\n\t\t\t\t\/* Need to check and remove the input variables related to the Style Tab. *\/\n\t\t\t\t.srfm-form-container-305 {\n\t\t\t\t\t\/* New test variables *\/\n\t\t\t\t\t--srfm-color-scheme-primary: #111C44;\n\t\t\t\t\t--srfm-color-scheme-text-on-primary: #FFFFFF;\n\t\t\t\t\t--srfm-color-scheme-text: #1E1E1E;\n\t\t\t\t\t--srfm-quill-editor-color: #111C44;\n\n\t\t\t\t\t--srfm-color-input-label: #1E1E1E;\n\t\t\t\t\t--srfm-color-input-description: hsl( from #1E1E1E h s l \/ 0.65 );\n\t\t\t\t\t--srfm-color-input-placeholder: hsl( from #1E1E1E h s l \/ 0.5 );\n\t\t\t\t\t--srfm-color-input-text: #1E1E1E;\n\t\t\t\t\t--srfm-color-input-prefix: hsl( from #1E1E1E h s l \/ 0.65 );\n\t\t\t\t\t--srfm-color-input-background: hsl( from #1E1E1E h s l \/ 0.02 );\n\t\t\t\t\t--srfm-color-input-background-hover: hsl( from #1E1E1E h s l \/ 0.05 );\n\t\t\t\t\t--srfm-color-input-background-disabled: hsl( from #1E1E1E h s l \/ 0.07 );\n\t\t\t\t\t--srfm-color-input-border: hsl( from #1E1E1E h s l \/ 0.25 );\n\t\t\t\t\t--srfm-color-input-border-disabled: hsl( from #1E1E1E h s l \/ 0.15 );\n\t\t\t\t\t--srfm-color-multi-choice-svg: hsl( from #1E1E1E h s l \/ 0.7 );\n\t\t\t\t\t--srfm-color-input-border-hover: hsl( from #111C44 h s l \/ 0.65 );\n\t\t\t\t\t--srfm-color-input-border-focus-glow: hsl( from #111C44 h s l \/ 0.15 );\n\t\t\t\t\t--srfm-color-input-selected: hsl( from #111C44 h s l \/ 0.1 );\n\t\t\t\t\t--srfm-btn-color-hover: hsl( from #111C44 h s l \/ 0.9 );\n\t\t\t\t\t--srfm-btn-color-disabled: hsl( from #111C44 h s l \/ 0.25 );\n\n\t\t\t\t\t\/* Dropdown Variables *\/\n\t\t\t\t\t--srfm-dropdown-input-background-hover: hsl( from #1E1E1E h s l \/ 0.05 );\n\t\t\t\t\t--srfm-dropdown-option-background-hover: hsl( from #1E1E1E h s l \/ 0.10 );\n\t\t\t\t\t--srfm-dropdown-option-background-selected: hsl( from #1E1E1E h s l \/ 0.05 );\n\t\t\t\t\t--srfm-dropdown-option-selected-icon: hsl( from #1E1E1E h s l \/ 0.65 );\n\t\t\t\t\t--srfm-dropdown-option-text-color: hsl( from #1E1E1E h s l \/ 0.80 );\n\t\t\t\t\t--srfm-dropdown-option-selected-text: #1E1E1E;\n\t\t\t\t\t--srfm-dropdown-badge-background: hsl( from #1E1E1E h s l \/ 0.05 );\n\t\t\t\t\t--srfm-dropdown-badge-background-hover: hsl( from #1E1E1E h s l \/ 0.10 );\n\t\t\t\t\t--srfm-dropdown-menu-border-color: hsl( from #1E1E1E h s l \/ 0.10 );\n\t\t\t\t\t--srfm-dropdown-placeholder-color: hsl( from #1E1E1E h s l \/ 0.50 );\n\t\t\t\t\t--srfm-dropdown-icon-color: hsl( from #1E1E1E h s l \/ 0.65 );\n\t\t\t\t\t--srfm-dropdown-icon-disabled: hsl( from #1E1E1E h s l \/ 0.25 );\n\n\t\t\t\t\t\/* Background Control Variables *\/\n\t\t\t\t\t--srfm-instant-form-padding-top: 32px;--srfm-instant-form-padding-right: 32px;--srfm-instant-form-padding-bottom: 32px;--srfm-instant-form-padding-left: 32px;--srfm-instant-form-border-radius-top: 12px;--srfm-instant-form-border-radius-right: 12px;--srfm-instant-form-border-radius-bottom: 12px;--srfm-instant-form-border-radius-left: 12px;--srfm-form-padding-top: 0px;--srfm-form-padding-right: 0px;--srfm-form-padding-bottom: 0px;--srfm-form-padding-left: 0px;--srfm-form-border-radius-top: 99px;--srfm-form-border-radius-right: 99px;--srfm-form-border-radius-bottom: 99px;--srfm-form-border-radius-left: 99px;--srfm-bg-color: #FFFFFF;--srfm-bg-overlay-opacity: 1;\t\t\t\t\t--srfm-row-gap-between-blocks: 18px;--srfm-address-label-font-size: 16px;--srfm-address-label-line-height: 24px;--srfm-address-description-font-size: 14px;--srfm-address-description-line-height: 20px;--srfm-col-gap-between-fields: 16px;--srfm-row-gap-between-fields: 16px;--srfm-gap-below-address-label: 14px;--srfm-dropdown-font-size: 14px;--srfm-dropdown-gap-between-input-menu: 4px;--srfm-dropdown-badge-padding: 2px 6px;--srfm-dropdown-multiselect-font-size: 12px;--srfm-dropdown-multiselect-line-height: 16px;--srfm-dropdown-padding-right: 12px;--srfm-dropdown-padding-right-icon: calc( var( --srfm-dropdown-padding-right ) + 20px );--srfm-dropdown-multiselect-padding: 8px var( --srfm-dropdown-padding-right-icon ) 8px 8px;--srfm-input-height: 44px;--srfm-input-field-padding: 10px 12px;--srfm-input-field-font-size: 16px;--srfm-input-field-line-height: 24px;--srfm-input-field-margin-top: 6px;--srfm-input-field-margin-bottom: 6px;--srfm-checkbox-label-font-size: 16px;--srfm-checkbox-label-line-height: 24px;--srfm-checkbox-description-font-size: 14px;--srfm-checkbox-description-line-height: 20px;--srfm-check-ctn-width: 16px;--srfm-check-ctn-height: 16px;--srfm-check-svg-size: 10px;--srfm-checkbox-margin-top-frontend: 4px;--srfm-checkbox-margin-top-editor: 6px;--srfm-check-gap: 8px;--srfm-checkbox-description-margin-left: 24px;--srfm-flag-section-padding: 10px 0 10px 12px;--srfm-gap-between-icon-text: 8px;--srfm-label-font-size: 16px;--srfm-label-line-height: 24px;--srfm-description-font-size: 14px;--srfm-description-line-height: 20px;--srfm-btn-padding: 10px 14px;--srfm-btn-font-size: 16px;--srfm-btn-line-height: 24px;--srfm-multi-choice-horizontal-padding: 20px;--srfm-multi-choice-vertical-padding: 20px;--srfm-multi-choice-internal-option-gap: 8px;--srfm-multi-choice-vertical-svg-size: 40px;--srfm-multi-choice-horizontal-image-size: 24px;--srfm-multi-choice-vertical-image-size: 120px;--srfm-multi-choice-outer-padding: 2px;--srfm-upload-vertical-padding: 28px;--srfm-upload-inner-gap: 12px;--srfm-upload-text-line-height: 24px;--srfm-upload-file-margin-top: 16px;--srfm-upload-preview-size: 42px;--srfm-slider-label-font-size: 12px;--srfm-slider-label-line-height: 16px;--srfm-slider-label-top-padding: 8px;--srfm-slider-error-gap: 6px;--srfm-page-break-row-gap: 28px;--srfm-rating-icon-size: 28px;--srfm-rating-icon-gap: 6px;--srfm-datepicker-dropdown-input-gap: 4px;--srfm-login-row-gap: 14px;--srfm-signature-canvas-height: 140px;--srfm-signature-button-bottom: 14px;\t\t--srfm-page-break-back-btn-text-color: hsl( from #1E1E1E h s l \/ 0.80 );\n\t\t--srfm-page-break-back-btn-background: hsl( from #1E1E1E h s l \/ 0.05 );\n\t\t--srfm-page-break-unfilled-progress: hsl( from #1E1E1E h s l \/ 0.15 );\n\t\t--srfm-page-break-indicator-text-color: hsl( from #1E1E1E h s l \/ 0.50 );\n\t\t--srfm-page-break-connector-checked: hsl( from #1E1E1E h s l \/ 0.15 );\n\t\t--srfm-page-break-connector-pending: hsl( from #1E1E1E h s l \/ 0.25 );\n\t\t--srfm-page-break-connector-active: hsl( from #111C44 h s l \/ 0.50 );\n\t\t--srfm-page-break-steps-unfilled: hsl( from #1E1E1E h s l \/ 0.50 );\n\t\t--srfm-page-break-steps-filled: hsl( from #1E1E1E h s l \/ 0.25 );\n\t\t--srfm-page-break-steps-progress: hsl( from #1E1E1E h s l \/ 0.15 );\n\t\t--srfm-page-break-steps-pending-text-color: hsl( from #1E1E1E h s l \/ 0.80 );\n\t\t--srfm-password-strength-weak: #DC2626;--srfm-password-strength-weak-border-glow: hsl( from var(--srfm-password-strength-weak) h s l \/ 0.15 );--srfm-password-strength-weak-border-color: hsl( from var(--srfm-password-strength-weak) h s l \/ 0.65 );--srfm-password-strength-medium: #D97706;--srfm-password-strength-medium-border-glow: hsl( from var(--srfm-password-strength-medium) h s l \/ 0.15 );--srfm-password-strength-medium-border-color: hsl( from var(--srfm-password-strength-medium) h s l \/ 0.65 );--srfm-password-strength-strong: #16A34A;--srfm-password-strength-strong-border-glow: hsl( from var(--srfm-password-strength-strong) h s l \/ 0.15 );--srfm-password-strength-strong-border-color: hsl( from var(--srfm-password-strength-strong) h s l \/ 0.65 );\t\t\t\t}\n\t\t\t<\/style>\n\t\t\t\t\t\t\t<form method=\"post\" enctype=\"multipart\/form-data\" id=\"srfm-form-305\" class=\"srfm-form\"\n\t\t\t\tform-id=\"305\" after-submission=\"hide form\" message-type=\"same page\" success-url=\"\" ajaxurl=\"https:\/\/nylonplastic.com\/wp-admin\/admin-ajax.php\" data-submit-token=\"cb4c6d2a5acc5675d4b82718cb949cbc4fdf265fc4d16738e67536b1b3fe0fbc\" action=\"\"\n\t\t\t\t>\n\t\t\t\t\n\t\t\t\t<input type=\"hidden\" value=\"305\" name=\"form-id\">\n\t\t\t\t\t\t\t\t<input type=\"hidden\" value=\"\" name=\"srfm-form-language\">\n\t\t\t\t<input type=\"hidden\" value=\"\" name=\"srfm-sender-email-field\" id=\"srfm-sender-email\">\n\t\t\t\t<input type=\"hidden\" value=\"\" id=\"srfm-page-break\">\n\t\t\t\t\t\t<p id=\"srfm-error-message\" class=\"srfm-common-error-message srfm-error-message srfm-head-error\" hidden>\t\t<span class=\"srfm-icon\" aria-hidden=\"true\">\n\t\t\t<svg xmlns=\"http:\/\/www.w3.org\/2000\/svg\" width=\"20\" height=\"20\" fill=\"none\"><path d=\"M9.99935 18.3327C14.6017 18.3327 18.3327 14.6017 18.3327 9.99935C18.3327 5.39698 14.6017 1.66602 9.99935 1.66602C5.39698 1.66602 1.66602 5.39698 1.66602 9.99935C1.66602 14.6017 5.39698 18.3327 9.99935 18.3327Z\" stroke=\"currentColor\" stroke-width=\"1.5\" stroke-linecap=\"round\" stroke-linejoin=\"round\" \/><path d=\"M10 6.66602V9.99935\" stroke=\"currentColor\" stroke-width=\"1.5\" stroke-linecap=\"round\" stroke-linejoin=\"round\" \/><path d=\"M10 13.334H10.0083\" stroke=\"currentColor\" stroke-width=\"1.5\" stroke-linecap=\"round\" stroke-linejoin=\"round\" \/><\/svg>\t\t<\/span>\n\t\t<span class=\"srfm-error-content\">\u30d5\u30a9\u30fc\u30e0\u3092\u9001\u4fe1\u3057\u3088\u3046\u3068\u3057\u3066\u30a8\u30e9\u30fc\u304c\u767a\u751f\u3057\u307e\u3057\u305f\u3002\u3082\u3046\u4e00\u5ea6\u304a\u8a66\u3057\u304f\u3060\u3055\u3044\u3002.<\/span><\/p>\n\t\t\t\t\t\t<div data-block-id=\"7fa370fa\" class=\"wp-block-uagb-advanced-heading uagb-block uagb-block-7fa370fa\" >\n\t\t\t\t\t<h2 class=\"uagb-heading-text\">\u30ab\u30b9\u30bf\u30e0\u30bd\u30ea\u30e5\u30fc\u30b7\u30e7\u30f3\u3092\u4f5c\u308a\u307e\u3057\u3087\u3046<\/h2>\t\t\t\t<\/div>\n\t\t\t\n\n\t\t\t<div data-block-id=\"bb2839a9\" class=\"srfm-block-single srfm-block srfm-input-block srf-input-bb2839a9-block  srfm-block-width-50 srfm-slug-text-field\" >\n\t\t\t\t\t\t\t\t<label id=\"srfm-label-bb2839a9-lbl-Rmlyc3QgTmFtZQ\" for=\"srfm-input-bb2839a9-lbl-Rmlyc3QgTmFtZQ\" class=\"srfm-block-label\">\n\t\t\t\t\t\t\u540d\u524d\t\t\t\t\t\t\t\t\t\t\t\t\t<span class=\"srfm-required\" aria-hidden=\"true\"> *<\/span>\n\t\t\t\t\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-block-wrap\">\n\t\t\t\t<input class=\"srfm-input-common srfm-input-input\" type=\"text\" name=\"srfm-input-bb2839a9-lbl-Rmlyc3QgTmFtZQ-text-field\" id=\"srfm-input-bb2839a9-lbl-Rmlyc3QgTmFtZQ\"\n\t\t\t\t\taria-describedby='srfm-error-bb2839a9'\t\t\t\t\tdata-required=\"true\" aria-required=\"true\" data-unique=\"false\" maxlength=\"100\" value=\"\"  data-srfm-mask=\"none\"   \/>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"srfm-error-wrap\">\n\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-error-message\" data-srfm-id=\"srfm-error-bb2839a9\" data-error-msg=\"This field is required.\" data-unique-msg=\"Value needs to be unique.\">\n\t\t\t\t\t\t\u3053\u306e\u30d5\u30a3\u30fc\u30eb\u30c9\u306f\u5fc5\u9808\u3067\u3059\u3002.\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t<\/div>\n\t\t\n\n\t\t\t<div data-block-id=\"dbaa04c6\" class=\"srfm-block-single srfm-block srfm-input-block srf-input-dbaa04c6-block  srfm-block-width-50 srfm-slug-last-name\" >\n\t\t\t\t\t\t\t\t<label id=\"srfm-label-dbaa04c6-lbl-TGFzdCBOYW1l\" for=\"srfm-input-dbaa04c6-lbl-TGFzdCBOYW1l\" class=\"srfm-block-label\">\n\t\t\t\t\t\t\u30e9\u30b9\u30c8\u30cd\u30fc\u30e0\t\t\t\t\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-block-wrap\">\n\t\t\t\t<input class=\"srfm-input-common srfm-input-input\" type=\"text\" name=\"srfm-input-dbaa04c6-lbl-TGFzdCBOYW1l-last-name\" id=\"srfm-input-dbaa04c6-lbl-TGFzdCBOYW1l\"\n\t\t\t\t\taria-describedby='srfm-error-dbaa04c6'\t\t\t\t\tdata-required=\"false\" aria-required=\"false\" data-unique=\"false\" maxlength=\"100\" value=\"\"  data-srfm-mask=\"none\"   \/>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"srfm-error-wrap\">\n\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-error-message\" data-srfm-id=\"srfm-error-dbaa04c6\" data-error-msg=\"This field is required.\" data-unique-msg=\"Value needs to be unique.\">\n\t\t\t\t\t\t\u3053\u306e\u30d5\u30a3\u30fc\u30eb\u30c9\u306f\u5fc5\u9808\u3067\u3059\u3002.\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t<\/div>\n\t\t\n\n\t\t\t<div data-block-id=\"80af9bb9\" class=\"srfm-block-single srfm-block srfm-email-block srf-email-80af9bb9-block  srfm-block-width-50 srfm-slug-email srfm-email-block-wrap\">\n\t\t\t\t<div class=\"srfm-email-block srf-email-80af9bb9-block\">\n\t\t\t\t\t\t\t\t\t\t<label id=\"srfm-label-80af9bb9-lbl-RW1haWw\" for=\"srfm-email-80af9bb9-lbl-RW1haWw\" class=\"srfm-block-label\">\n\t\t\t\t\t\t\u96fb\u5b50\u30e1\u30fc\u30eb\t\t\t\t\t\t\t\t\t\t\t\t\t<span class=\"srfm-required\" aria-hidden=\"true\"> *<\/span>\n\t\t\t\t\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-block-wrap\">\n\t\t\t\t\t\t<input class=\"srfm-input-common srfm-input-email\" type=\"email\" name=\"srfm-email-80af9bb9-lbl-RW1haWw-email\" id=\"srfm-email-80af9bb9-lbl-RW1haWw\"\n\t\t\t\t\t\taria-describedby='srfm-error-80af9bb9'\t\t\t\t\t\tdata-required=\"true\" aria-required=\"true\" data-unique=\"false\" value=\"\"   \/>\n\t\t\t\t\t<\/div>\n\t\t\t\t\t<div class=\"srfm-error-wrap\">\n\t\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-error-message\" data-srfm-id=\"srfm-error-80af9bb9\" data-error-msg=\"This field is required.\" data-unique-msg=\"Value needs to be unique.\">\n\t\t\t\t\t\t\u3053\u306e\u30d5\u30a3\u30fc\u30eb\u30c9\u306f\u5fc5\u9808\u3067\u3059\u3002.\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t\t\t<\/div>\n\t\t\n\n\t\t<div data-block-id=\"0c6821ab\" class=\"srfm-block-single srfm-block srfm-phone-block srf-phone-0c6821ab-block srfm-block-width-50\">\n\t\t\t\t\t\t\t\t<label id=\"srfm-label-0c6821ab-lbl-UGhvbmUgTnVtYmVy\" for=\"srfm-phone-0c6821ab-lbl-UGhvbmUgTnVtYmVy\" class=\"srfm-block-label\">\n\t\t\t\t\t\t\u96fb\u8a71\u756a\u53f7\t\t\t\t\t\t\t\t\t\t\t\t\t<span class=\"srfm-required\" aria-hidden=\"true\"> *<\/span>\n\t\t\t\t\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-block-wrap\">\n\t\t\t\t<input type=\"tel\"\n\t\t\t\t\tclass=\"srfm-input-common srfm-input-phone\"\n\t\t\t\t\tname=\"srfm-phone-0c6821ab-lbl-UGhvbmUgTnVtYmVy-phone-number\"\n\t\t\t\t\tid=\"srfm-phone-0c6821ab-lbl-UGhvbmUgTnVtYmVy\"\n\t\t\t\t\taria-describedby='srfm-error-0c6821ab'\t\t\t\t\tdata-required=\"true\"\n\t\t\t\t\taria-required=\"true\"\n\t\t\t\t\tdefault-country=\"us\"\n\t\t\t\t\t\t\t\t\t\t\tdata-auto-country=\"true\"\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\tvalue=\"\"\n\t\t\t\t\t\t\t\t\t\tdata-unique=\"false\">\n\t\t\t<\/div>\n\t\t\t<div class=\"srfm-error-wrap\">\n\t\t\t\t\t\t\t\t\t<div class=\"srfm-error-message\" data-srfm-id=\"srfm-error-0c6821ab\" data-error-msg=\"This field is required.\" data-unique-msg=\"Value needs to be unique.\">\n\t\t\t\t\t\t\u3053\u306e\u30d5\u30a3\u30fc\u30eb\u30c9\u306f\u5fc5\u9808\u3067\u3059\u3002.\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\n\n\t\t\t<div data-block-id=\"b05f96f8\" class=\"srfm-block-single srfm-block srfm-upload-block srf-upload-b05f96f8-block srfm-block-width-100\">\n\t\t\t\t\t\t\t\t\t<label id=\"srfm-label-b05f96f8\" for=\"srfm-upload-b05f96f8\" class=\"srfm-block-label\">\n\t\t\t\t\t\tUpload\t\t\t\t\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-block-wrap\">\n\t\t\t\t\t<span class=\"srfm-icon srfm-upload-icon\" aria-hidden=\"true\"><svg width='24' height='24' viewbox='0 0 24 24' fill='none' xmlns='http:\/\/www.w3.org\/2000\/svg'><path d='M21 15V19C21 19.5304 20.7893 20.0391 20.4142 20.4142C20.0391 20.7893 19.5304 21 19 21H5C4.46957 21 3.96086 20.7893 3.58579 20.4142C3.21071 20.0391 3 19.5304 3 19V15' stroke='#1E1E1E' stroke-opacity='0.65' stroke-width='1.5' stroke-linecap='round' stroke-linejoin='round'\/><path d='M17 8L12 3L7 8' stroke='#1E1E1E' stroke-opacity='0.65' stroke-width='1.5' stroke-linecap='round' stroke-linejoin='round'\/><path d='M12 3V15' stroke='#1E1E1E' stroke-opacity='0.65' stroke-width='1.5' stroke-linecap='round' stroke-linejoin='round'\/><\/svg><\/span>\t\t\t\t\t<div class=\"srfm-upload-wrap\">\n\t\t\t\t\t\t<input class=\"srfm-upload-size\" value=\"10\" type=\"hidden\" \/>\n\t\t\t\t\t\t<label class=\"srfm-classic-upload-label\">\n\t\t\t\t\t\t\tClick to upload or drag and drop\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t<input\n\t\t\t\t\t\t\tid=\"srfm-upload-b05f96f8\"\n\t\t\t\t\t\t\tclass=\"srfm-input-upload\"\n\t\t\t\t\t\t\tname=\"srfm-upload-b05f96f8-lbl-VXBsb2Fk-srfm-upload[]\"\n\t\t\t\t\t\t\ttype=\"file\"\n\t\t\t\t\t\t\t\t\t\t\t\t\t\taria-describedby='srfm-error-b05f96f8'\t\t\t\t\t\t\tdata-required=\"false\"\n\t\t\t\t\t\t\taria-required=\"false\"\n\t\t\t\t\t\t\taccept=\".jpg, .jpeg, .gif, .png, .pdf\"\n\t\t\t\t\t\t>\n\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"srfm-upload-data\"><\/div>\n\t\t\t\t<div class=\"srfm-error-wrap\">\t\t\t\t\t<div class=\"srfm-error-message\" data-srfm-id=\"srfm-error-b05f96f8\" data-error-msg=\"This field is required.\">\n\t\t\t\t\t\t\u3053\u306e\u30d5\u30a3\u30fc\u30eb\u30c9\u306f\u5fc5\u9808\u3067\u3059\u3002.\t\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t<\/div>\n\t\t\n\n\t\t<div data-block-id=\"fabb13d5\" class=\"srfm-block-single srfm-block srfm-textarea-block srf-textarea-fabb13d5-block  srfm-block-width-100\">\n\t\t\t\t\t\t\t\t<label id=\"srfm-label-fabb13d5-lbl-WW91ciBNZXNzYWdl-1359\" for=\"srfm-textarea-fabb13d5-lbl-WW91ciBNZXNzYWdl-1359\" class=\"srfm-block-label\">\n\t\t\t\t\t\t\u3042\u306a\u305f\u306e\u30e1\u30c3\u30bb\u30fc\u30b8\t\t\t\t\t\t\t\t\t\t\t\t\t<span class=\"srfm-required\" aria-hidden=\"true\"> *<\/span>\n\t\t\t\t\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-block-wrap\">\n\t\t\t\t<textarea\n\t\t\t\t\tclass=\"srfm-input-common srfm-input-textarea\"\n\t\t\t\t\tname=\"srfm-textarea-fabb13d5-lbl-WW91ciBNZXNzYWdl-your-message\"\n\t\t\t\t\tid=\"srfm-textarea-fabb13d5-lbl-WW91ciBNZXNzYWdl-1359\"\n\t\t\t\t\taria-describedby='srfm-error-fabb13d5'\t\t\t\t\tdata-required=\"true\" aria-required=\"true\"  rows=\"4\"  \t\t\t\t\t\t\t\t\t\t\t\t\t\t\t><\/textarea>\n\t\t\t\t\t\t\t<\/div>\n\t\t\t<div class=\"srfm-error-wrap\">\n\t\t\t\t\t\t\t\t\t<div class=\"srfm-error-message\" data-srfm-id=\"srfm-error-fabb13d5\" data-error-msg=\"This field is required.\">\n\t\t\t\t\t\t\u3053\u306e\u30d5\u30a3\u30fc\u30eb\u30c9\u306f\u5fc5\u9808\u3067\u3059\u3002.\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t<\/div>\n\n\t\t\t\t\t\t\t\n\t\t\t\t\t\n\t\t\t\t\t<div class=\"srfm-submit-container\" style=\"\">\n\t\t\t\t\t\t<div style=\"width: ; text-align: left\" class=\"wp-block-button\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<button style=\"\" id=\"srfm-submit-btn\" class=\"srfm-btn-frontend srfm-button srfm-submit-button\"\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t>\n\t\t\t\t\t\t\t\t<div class=\"srfm-submit-wrap\">\n\t\t\t\t\t\t\t\t\t\u6295\u7a3f\u3059\u308b\t\t\t\t\t\t\t\t<div class=\"srfm-loader\"><\/div>\n\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t<\/button>\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t<p id=\"srfm-error-message\" class=\"srfm-common-error-message srfm-error-message srfm-footer-error\" hidden>\t\t<span class=\"srfm-icon\" aria-hidden=\"true\">\n\t\t\t<svg xmlns=\"http:\/\/www.w3.org\/2000\/svg\" width=\"20\" height=\"20\" fill=\"none\"><path d=\"M9.99935 18.3327C14.6017 18.3327 18.3327 14.6017 18.3327 9.99935C18.3327 5.39698 14.6017 1.66602 9.99935 1.66602C5.39698 1.66602 1.66602 5.39698 1.66602 9.99935C1.66602 14.6017 5.39698 18.3327 9.99935 18.3327Z\" stroke=\"currentColor\" stroke-width=\"1.5\" stroke-linecap=\"round\" stroke-linejoin=\"round\" \/><path d=\"M10 6.66602V9.99935\" stroke=\"currentColor\" stroke-width=\"1.5\" stroke-linecap=\"round\" stroke-linejoin=\"round\" \/><path d=\"M10 13.334H10.0083\" stroke=\"currentColor\" stroke-width=\"1.5\" stroke-linecap=\"round\" stroke-linejoin=\"round\" \/><\/svg>\t\t<\/span>\n\t\t<span class=\"srfm-error-content\">\u30d5\u30a9\u30fc\u30e0\u3092\u9001\u4fe1\u3057\u3088\u3046\u3068\u3057\u3066\u30a8\u30e9\u30fc\u304c\u767a\u751f\u3057\u307e\u3057\u305f\u3002\u3082\u3046\u4e00\u5ea6\u304a\u8a66\u3057\u304f\u3060\u3055\u3044\u3002.<\/span><\/p>\n\t\t\t\t\t<input type=\"hidden\" name=\"trp-form-language\" value=\"ja\"\/><\/form>\n\t\t\t<div class=\"srfm-single-form srfm-success-box in-page\">\n\t\t\t\t<div aria-live=\"polite\" aria-atomic=\"true\" role=\"alert\" id=\"srfm-success-message-page-305\" class=\"srfm-success-box-description\"><\/div>\n\t\t\t<\/div>\n\t\t\t\t\t\t<\/div>","protected":false},"excerpt":{"rendered":"<h3><\/h3>\n<p class=\"ds-markdown-paragraph\"><strong>What is PA6 GF30 FR(V0)?<\/strong><br \/>\nPA6 GF30 FR(V0) is a high-performance, flame-retardant engineering thermoplastic. It is based on nylon 6 (PA6) reinforced with 30% glass fibers and formulated with additives to achieve the UL94 V-0 fire safety rating. This grade is engineered to provide an\u00a0<strong>exceptional balance of mechanical strength, rigidity, thermal stability, and certified flame retardancy<\/strong>. As the industry-standard reinforced FR material, it is designed for structural components that must reliably perform under stress, heat, and in safety-critical environments where fire resistance is mandatory.<\/p>\n<p class=\"ds-markdown-paragraph\"><strong>Why Choose Nylon Plastic\u2019s PA6 GF30 FR(V0)?<\/strong><br \/>\n\u2705\u00a0<strong>Proven Reliability for Demanding Applications:<\/strong>\u00a0Our PA6 GF30 FR(V0) delivers a robust combination of tensile strength, stiffness, and heat deflection temperature, making it the trusted choice for critical parts in automotive, electrical, and industrial equipment.<br \/>\n\u2705\u00a0<strong>Consistent Safety and Quality Assurance:<\/strong>\u00a0We ensure our material consistently meets the UL94 V-0 standard. Our controlled manufacturing process guarantees batch-to-batch uniformity in both flame-retardant performance and mechanical properties.<br \/>\n\u2705\u00a0<strong>Optimized Processability and Technical Support:<\/strong>\u00a0We provide expert guidance on processing parameters to ensure efficient molding, excellent surface finish, and maximum property retention for your parts, reducing development time and risk.<br \/>\n\u2705\u00a0<strong>Trusted Partnership and Supply Stability:<\/strong>\u00a0As a reliable supplier, we offer dependable material availability and dedicated support, from sample evaluation to production scale-up, ensuring your project timelines and performance requirements are met.<\/p>\n<div data-elementor-type=\"page\" data-elementor-id=\"3469\" class=\"elementor elementor-3469\" data-elementor-post-type=\"elementor_library\">\n<div class=\"elementor-element elementor-element-753a2e7 e-grid e-con-boxed e-con e-parent\" data-id=\"753a2e7\" data-element_type=\"container\" data-e-type=\"container\">\n<div class=\"e-con-inner\">\n<div class=\"elementor-element elementor-element-aaa8317 elementor-button-warning elementor-widget elementor-widget-button\" data-id=\"aaa8317\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"button.default\">\n<div class=\"elementor-widget-container\">\n<div class=\"elementor-button-wrapper\">\n\t\t\t\t\t<a class=\"elementor-button elementor-button-link elementor-size-sm\" href=\"#elementor-action%3Aaction%3Dpopup%3Aopen%26settings%3DeyJpZCI6IjI0MDQiLCJ0b2dnbGUiOmZhbHNlfQ%3D%3D\"><br \/>\n\t\t\t\t\t\t<span class=\"elementor-button-content-wrapper\"><br \/>\n\t\t\t\t\t\t\t\t\t<span class=\"elementor-button-text\">\u30d5\u30a1\u30a4\u30eb\u3092\u9001\u4fe1\u3059\u308b<\/span><br \/>\n\t\t\t\t\t<\/span><br \/>\n\t\t\t\t\t<\/a>\n\t\t\t\t<\/div>\n<\/p><\/div>\n<\/p><\/div>\n<div class=\"elementor-element elementor-element-69ce54b elementor-button-success elementor-widget elementor-widget-button\" data-id=\"69ce54b\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"button.default\">\n<div class=\"elementor-widget-container\">\n<div class=\"elementor-button-wrapper\">\n\t\t\t\t\t<a class=\"elementor-button elementor-button-link elementor-size-sm\" href=\"https:\/\/nylonplastic.com\/ja\/contact\/\"><br \/>\n\t\t\t\t\t\t<span class=\"elementor-button-content-wrapper\"><br \/>\n\t\t\t\t\t\t\t\t\t<span class=\"elementor-button-text\">\u304a\u554f\u3044\u5408\u308f\u305b<\/span><br \/>\n\t\t\t\t\t<\/span><br \/>\n\t\t\t\t\t<\/a>\n\t\t\t\t<\/div>\n<\/p><\/div>\n<\/p><\/div>\n<\/p><\/div>\n<\/p><\/div>\n<\/p><\/div>","protected":false},"featured_media":1302,"comment_status":"closed","ping_status":"closed","template":"","meta":{"rop_custom_images_group":[],"rop_custom_messages_group":[],"rop_publish_now":"initial","rop_publish_now_accounts":{"facebook_846085238273622_899381133262461":""},"rop_publish_now_history":[],"rop_publish_now_status":"pending","site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"default","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","ast-disable-related-posts":"","theme-transparent-header-meta":"default","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"set","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}}},"product_brand":[43],"product_cat":[56],"product_tag":[],"class_list":["post-2790","product","type-product","status-publish","has-post-thumbnail","product_brand-nylon-plastic","product_cat-pa6-flame-retardant","desktop-align-left","tablet-align-left","mobile-align-left","first","instock","shipping-taxable","product-type-simple"],"_links":{"self":[{"href":"https:\/\/nylonplastic.com\/ja\/wp-json\/wp\/v2\/product\/2790","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nylonplastic.com\/ja\/wp-json\/wp\/v2\/product"}],"about":[{"href":"https:\/\/nylonplastic.com\/ja\/wp-json\/wp\/v2\/types\/product"}],"replies":[{"embeddable":true,"href":"https:\/\/nylonplastic.com\/ja\/wp-json\/wp\/v2\/comments?post=2790"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nylonplastic.com\/ja\/wp-json\/wp\/v2\/media\/1302"}],"wp:attachment":[{"href":"https:\/\/nylonplastic.com\/ja\/wp-json\/wp\/v2\/media?parent=2790"}],"wp:term":[{"taxonomy":"product_brand","embeddable":true,"href":"https:\/\/nylonplastic.com\/ja\/wp-json\/wp\/v2\/product_brand?post=2790"},{"taxonomy":"product_cat","embeddable":true,"href":"https:\/\/nylonplastic.com\/ja\/wp-json\/wp\/v2\/product_cat?post=2790"},{"taxonomy":"product_tag","embeddable":true,"href":"https:\/\/nylonplastic.com\/ja\/wp-json\/wp\/v2\/product_tag?post=2790"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}