{"id":62,"count":6,"description":"Combining the low moisture absorption, excellent chemical resistance, and good low-temperature toughness of PA12 with the enhanced stiffness from glass fibers. This material is suited for stable, durable parts exposed to humid or chemical environments.\r\nKey Applications: Fluid handling components (valves, connectors), external automotive parts, specialized gears, and housings for outdoor use.","link":"https:\/\/nylonplastic.com\/ko\/product-category\/%ed%8f%b4%eb%a6%ac%ec%95%84%eb%af%b8%eb%93%9c-12\/nylon12-glass-fiber\/","name":"PA12+\uc720\ub9ac \uc12c\uc720","slug":"nylon12-glass-fiber","taxonomy":"product_cat","parent":60,"meta":[],"menu_order":17,"_links":{"self":[{"href":"https:\/\/nylonplastic.com\/ko\/wp-json\/wp\/v2\/product_cat\/62","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nylonplastic.com\/ko\/wp-json\/wp\/v2\/product_cat"}],"about":[{"href":"https:\/\/nylonplastic.com\/ko\/wp-json\/wp\/v2\/taxonomies\/product_cat"}],"up":[{"embeddable":true,"href":"https:\/\/nylonplastic.com\/ko\/wp-json\/wp\/v2\/product_cat\/60"}],"wp:post_type":[{"href":"https:\/\/nylonplastic.com\/ko\/wp-json\/wp\/v2\/product?product_cat=62"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}