Carbon fiber reinforced nylon combines the processability of nylon with the exceptional stiffness and strength of carbon fiber. This advanced composite material delivers performance approaching that of metals.
What is Carbon Fiber Reinforced Nylon?
Carbon fiber reinforced nylon is a composite material where short carbon fibers (typically 15-40% by weight) are dispersed within a nylon matrix, dramatically improving stiffness, strength, and thermal properties.
Mechanical Properties: Near-Metal Performance
| Eigendom | PA6 Unfilled | PA6 CF20 | PA6 CF30 | Aluminum 6061 |
|---|---|---|---|---|
| Treksterkte (MPa) | 75 | 190 | 230 | 310 |
| Flexural Modulus (GPa) | 2.7 | 14.0 | 18.0 | 69.0 |
| Dichtheid (g/cm³) | 1.14 | 1.23 | 1.28 | 2.70 |
| HDT at 1.8 MPa (°C) | 65 | 250 | 255 | N/A |

Carbon Fiber vs Glass Fiber Reinforcement
CF nylon offers ~35% higher tensile strength and significantly better stiffness-to-weight ratio than GF nylon. However, CF nylon is semi-conductive (useful for ESD) and more expensive.
Belangrijkste voordelen
Exceptional Stiffness-to-Weight Ratio
CF nylon achieves specific stiffness rivaling aluminum at half the weight.

Thermal Stability
Carbon fibers reduce nylon’s CTE dramatically. HDT values exceed 250°C, suitable for high-temperature applications.
Slijtvastheid
Carbon fibers provide solid lubricity, making CF nylon excellent for bearings, gears, and sliding components.
Processing Challenges
CF nylon requires hardened tool steels, bimetallic barrels, higher injection pressures, and careful shear control to avoid fiber degradation.

Toepassingen
- Automotive: structural brackets, engine covers, transmission components
- Aerospace: interior brackets, cable management
- Sports: bicycle components, drone frames
Onze mogelijkheden
Met meer dan 300 CNC machines, produceren we meer dan 10.000 stuks per dag met toleranties zo nauw als ±0,005mm. Wij accepteren MOQ vanaf 1 stuk, met levertijden variërend van 24 uur tot 15 dagen. We work with carbon fiber reinforced nylon for demanding applications. Ontvang binnen 24 uur een offerte.
FAQ
How do you know whether Carbon Fiber Reinforced Nylon: Properties, Processing, and Applications fits a part?
Carbon Fiber Reinforced Nylon: Properties, Processing, and Applications fits a part when its load capacity, temperature range, moisture exposure, wear behavior, and processing method match the real service conditions.
What properties should be checked for Carbon Fiber Reinforced Nylon: Properties, Processing, and Applications?
Check strength, stiffness, impact resistance, heat resistance, moisture absorption, dimensional stability, friction, wear, and chemical compatibility.
What is the biggest selection risk for Carbon Fiber Reinforced Nylon: Properties, Processing, and Applications?
The biggest risk is choosing from a datasheet value without considering actual environment, processing method, part geometry, and long-term use.