{"id":2808,"date":"2025-12-30T08:45:20","date_gmt":"2025-12-30T08:45:20","guid":{"rendered":"https:\/\/nylonplastic.com\/?post_type=product&#038;p=2808"},"modified":"2026-01-04T08:15:06","modified_gmt":"2026-01-04T08:15:06","slug":"pa6-cf10","status":"publish","type":"product","link":"https:\/\/nylonplastic.com\/nl\/product\/pa6-cf10\/","title":{"rendered":"PA6 CF10 Nylon 6 met 10% Koolstofvezels | Nylon Plastiek"},"content":{"rendered":"<h2><a href=\"https:\/\/www.wanhan-plastic.com\/\"><img fetchpriority=\"high\" decoding=\"async\" class=\"alignnone wp-image-2406 size-full\" src=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_01-e1763968617686.jpg\" alt=\"\u4e07\u7ff0\u8be6\u60c5 01\" width=\"800\" height=\"937\"  title=\"PA6 CF10 Nylon 6 met 10% Koolstofvezels | Nylon Plastiek\" srcset=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_01-e1763968617686.jpg 800w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_01-e1763968617686-256x300.jpg 256w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_01-e1763968617686-768x900.jpg 768w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_01-e1763968617686-600x703.jpg 600w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/a><\/h2>\n<h3><strong>PA6 CF10 Technische gegevens (geschatte typische waarden)<\/strong><\/h3>\n<div class=\"ds-scroll-area _1210dd7 c03cafe9\">\n<table>\n<thead>\n<tr>\n<th>Eigendom<\/th>\n<th>Waarde<\/th>\n<th>Testnorm<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>Inhoud koolstofvezel<\/strong><\/td>\n<td>10%<\/td>\n<td>ISO 1172<\/td>\n<\/tr>\n<tr>\n<td><strong>Treksterkte<\/strong><\/td>\n<td>140 - 160 MPa<\/td>\n<td>ISO 527<\/td>\n<\/tr>\n<tr>\n<td><strong>Flexural Modulus<\/strong><\/td>\n<td>10.000 - 12.000 MPa<\/td>\n<td>ISO 178<\/td>\n<\/tr>\n<tr>\n<td><strong>Ingekorte schokweerstand<\/strong><\/td>\n<td>9 - 12 kJ\/m\u00b2<\/td>\n<td>ISO 180<\/td>\n<\/tr>\n<tr>\n<td><strong>HDT @1,8 MPa<\/strong><\/td>\n<td>215 - 225 \u00b0C<\/td>\n<td>ISO 75<\/td>\n<\/tr>\n<tr>\n<td><strong>Volumeweerstandsvermogen<\/strong><\/td>\n<td>10^3 - 10^5 \u03a9-cm<\/td>\n<td>IEC 60093<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<h3><strong>Tabel technische gegevens PA6 CF-serie (geschatte typische waarden)<\/strong><\/h3>\n<div class=\"ds-scroll-area _1210dd7 c03cafe9\">\n<table>\n<thead>\n<tr>\n<th>Eigendom<\/th>\n<th>Testnorm<\/th>\n<th>PA6 CF10<\/th>\n<th>PA6 CF20<\/th>\n<th>PA6 CF30<\/th>\n<th>PA6 CF40<\/th>\n<th>PA6 CF50<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>Inhoud koolstofvezel<\/strong><\/td>\n<td>ISO 1172<\/td>\n<td><strong>10%<\/strong><\/td>\n<td><strong>20%<\/strong><\/td>\n<td><strong>30%<\/strong><\/td>\n<td><strong>40%<\/strong><\/td>\n<td><strong>50%<\/strong><\/td>\n<\/tr>\n<tr>\n<td><strong>Treksterkte<\/strong><\/td>\n<td>ISO 527<\/td>\n<td><strong>140 - 160 MPa<\/strong><\/td>\n<td><strong>180 - 210 MPa<\/strong><\/td>\n<td><strong>220 - 250 MPa<\/strong><\/td>\n<td><strong>240 - 270 MPa<\/strong><\/td>\n<td><strong>260 - 290 MPa<\/strong><\/td>\n<\/tr>\n<tr>\n<td><strong>Flexural Modulus<\/strong><\/td>\n<td>ISO 178<\/td>\n<td><strong>10.000 - 12.000 MPa<\/strong><\/td>\n<td><strong>15.000 - 18.000 MPa<\/strong><\/td>\n<td><strong>20.000 - 23.000 MPa<\/strong><\/td>\n<td><strong>24.000 - 27.000 MPa<\/strong><\/td>\n<td><strong>28.000 - 32.000 MPa<\/strong><\/td>\n<\/tr>\n<tr>\n<td><strong>Ingekorte schokweerstand<\/strong><\/td>\n<td>ISO 180<\/td>\n<td><strong>9 - 12 kJ\/m\u00b2<\/strong><\/td>\n<td><strong>10 - 13 kJ\/m\u00b2<\/strong><\/td>\n<td><strong>11 - 14 kJ\/m\u00b2<\/strong><\/td>\n<td><strong>12 - 15 kJ\/m\u00b2<\/strong><\/td>\n<td><strong>13 - 16 kJ\/m\u00b2<\/strong><\/td>\n<\/tr>\n<tr>\n<td><strong>HDT @1,8 MPa<\/strong><\/td>\n<td>ISO 75<\/td>\n<td><strong>215 - 225 \u00b0C<\/strong><\/td>\n<td><strong>220 - 230 \u00b0C<\/strong><\/td>\n<td><strong>225 - 235 \u00b0C<\/strong><\/td>\n<td><strong>230 - 240 \u00b0C<\/strong><\/td>\n<td><strong>235 - 245 \u00b0C<\/strong><\/td>\n<\/tr>\n<tr>\n<td><strong>Volumeweerstandsvermogen<\/strong><\/td>\n<td>IEC 60093<\/td>\n<td><strong>10^3 - 10^5 \u03a9-cm<\/strong><\/td>\n<td><strong>10^2 - 10^4 \u03a9-cm<\/strong><\/td>\n<td><strong>10^1 - 10^3 \u03a9-cm<\/strong><\/td>\n<td><strong>10^0 - 10^2 \u03a9-cm<\/strong><\/td>\n<td><strong>10^-1 - 10^1 \u03a9-cm<\/strong><\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<h3><strong>PA6 CF10 Belangrijkste voordelen<\/strong><\/h3>\n<p class=\"ds-markdown-paragraph\">\u2705\u00a0<strong>Kosteneffectieve instap in koolstofvezelprestaties:<\/strong>\u00a0Biedt een aanzienlijke prestatieverbetering ten opzichte van standaard of glasgevulde kwaliteiten, waardoor geavanceerde composieten toegankelijk worden voor een breder scala aan toepassingen zonder hoge kosten.<br \/>\n\u2705\u00a0<strong>Verbeterde stijfheid met uitstekende verwerkbaarheid:<\/strong>\u00a0Biedt een merkbare toename in stijfheid en dimensionale stabiliteit met behoud van zeer goede vloei-eigenschappen, ideaal voor het vormen van complexe geometrie\u00ebn en dunwandige onderdelen.<br \/>\n\u2705\u00a0<strong>Inherente functionele eigenschappen:<\/strong>\u00a0Levert ingebouwde elektrostatische dissipatie (ESD) en verbeterde thermische geleidbaarheid in vergelijking met isolatiematerialen, waardoor waarde wordt toegevoegd aan elektronische en mechanische componenten.<\/p>\n<h2><strong>Industri\u00eble toepassingen:<\/strong><\/h2>\n<p><img decoding=\"async\" class=\"alignnone wp-image-1751 size-full\" src=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/10\/The-Crucial-Role-of-Injection-Molding-in-Automotive-Industry.jpg\" alt=\"de cruciale rol van spuitgieten in de auto-industrie\" width=\"1000\" height=\"571\"  title=\"PA6 CF10 Nylon 6 met 10% Koolstofvezels | Nylon Plastiek\" srcset=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/10\/The-Crucial-Role-of-Injection-Molding-in-Automotive-Industry.jpg 1000w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/10\/The-Crucial-Role-of-Injection-Molding-in-Automotive-Industry-300x171.jpg 300w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/10\/The-Crucial-Role-of-Injection-Molding-in-Automotive-Industry-768x439.jpg 768w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/10\/The-Crucial-Role-of-Injection-Molding-in-Automotive-Industry-600x343.jpg 600w\" sizes=\"(max-width: 1000px) 100vw, 1000px\" \/><\/p>\n<h3><strong>Ontdek de PA6 koolstofvezelserie in detail<\/strong><\/h3>\n<p class=\"ds-markdown-paragraph\">Klik op de links hieronder voor uitgebreide technische gegevens, belangrijke voordelen en toepassingsdetails voor elke specifieke soort.<\/p>\n<div class=\"ds-scroll-area _1210dd7 c03cafe9\">\n<table>\n<thead>\n<tr>\n<th>Rang<\/th>\n<th>Beste voor<\/th>\n<th>Overzicht<\/th>\n<th>Volledige details<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong>PA6 CF10<\/strong><\/td>\n<td>Koolstofvezelprestaties op instapniveau voor elektronische en precisieonderdelen.<\/td>\n<td>De meest toegankelijke CF-kwaliteit, met een duidelijke verbetering in stijfheid, maatvastheid en ESD-bescherming ten opzichte van standaardmaterialen.<\/td>\n<td><a href=\"https:\/\/nylonplastic.com\/nl\/product\/pa6-cf10\/\">Volledig gegevensblad PA6 CF10 bekijken \u2192<\/a><\/td>\n<\/tr>\n<tr>\n<td><strong>PA6 CF20<\/strong><\/td>\n<td>Veelzijdige metaalvervanger die sterkte, gewicht en geleidbaarheid vereist.<\/td>\n<td>Een uitgebalanceerde performer, ideaal voor algemene lichtgewicht toepassingen met een uitstekende sterkte-gewichtsverhouding en functionele geleidbaarheid.<\/td>\n<td><a href=\"https:\/\/nylonplastic.com\/nl\/product\/pa6-cf20\/\">Volledig gegevensblad PA6 CF20 bekijken \u2192<\/a><\/td>\n<\/tr>\n<tr>\n<td><strong>PA6 CF30<\/strong><\/td>\n<td>Constructiedelen onder hoge druk en dynamische belastingstoepassingen.<\/td>\n<td>De eerste keuze voor structurele integriteit, met bijna-metalen stijfheid, hoge weerstand tegen vermoeiing en precisiestabiliteit.<\/td>\n<td><a href=\"https:\/\/nylonplastic.com\/nl\/product\/pa6-cf30\/\">Volledig gegevensblad PA6 CF30 bekijken \u2192<\/a><\/td>\n<\/tr>\n<tr>\n<td><strong>PA6 CF40<\/strong><\/td>\n<td>Stijfheidskritische ontwerpen waarbij minimale doorbuiging van het grootste belang is.<\/td>\n<td>Ontworpen voor maximale stijfheid en uitzonderlijke dimensionale stabiliteit onder extreme belastingen in geavanceerde industri\u00eble sectoren.<\/td>\n<td><a href=\"https:\/\/nylonplastic.com\/nl\/product\/pa6-cf40\/\">Volledig gegevensblad PA6 CF40 bekijken \u2192<\/a><\/td>\n<\/tr>\n<tr>\n<td><strong>PA6 CF50<\/strong><\/td>\n<td>Bedrijfskritische toepassingen in de voorhoede van lichtgewicht engineering.<\/td>\n<td>De ultieme kwaliteit, die piekspecifieke prestaties levert voor de ruimtevaart, motorsport en elite automatiseringstoepassingen.<\/td>\n<td><a href=\"https:\/\/nylonplastic.com\/nl\/product\/pa6-cf50\/\">Volledig gegevensblad PA6 CF50 bekijken \u2192<\/a><\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<\/div>\n<h3><strong> Aansturen van innovatie in verschillende sectoren<\/strong><\/h3>\n<div class=\"ds-scroll-area _1210dd7 c03cafe9\">\n<div class=\"ds-scroll-area__gutters\">\n<div class=\"ds-scroll-area__vertical-gutter\"><\/div>\n<\/div>\n<table>\n<thead>\n<tr>\n<th>Industrie<\/th>\n<th>Belangrijkste toepassingen<\/th>\n<\/tr>\n<\/thead>\n<tbody>\n<tr>\n<td><strong> Automotive<\/strong><\/td>\n<td>Motorkappen, inlaatspruitstukken, structurele steunen, sensorbehuizingen, connectoren.<br \/>\n<strong><a href=\"https:\/\/nylonplastic.com\/nl\/automotive-industry\/\" target=\"_blank\" rel=\"noopener noreferrer\">Ontdek Automobieltoepassingen \u2192<\/a><\/strong><\/td>\n<\/tr>\n<tr>\n<td><strong> Elektrisch &amp; elektronica<\/strong><\/td>\n<td>Stroomonderbrekers, schakelaars, connectorbehuizingen, isolerende componenten.<br \/>\n<strong><a href=\"https:\/\/nylonplastic.com\/nl\/electronic-devices\/\" target=\"_blank\" rel=\"noopener noreferrer\">Ontdek E&amp;E-oplossingen \u2192<\/a><\/strong><\/td>\n<\/tr>\n<tr>\n<td><strong> Industri\u00eble apparatuur<\/strong><\/td>\n<td>Tandwielen, lagers, machinebehuizingen, rollen, mechanische onderdelen.<br \/>\n<strong><a href=\"https:\/\/nylonplastic.com\/nl\/industriele-uitrusting\/\" target=\"_blank\" rel=\"noopener noreferrer\">Zie Industrieel gebruik \u2192<\/a><\/strong><\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<figure id=\"attachment_2409\" aria-describedby=\"caption-attachment-2409\" style=\"width: 800px\" class=\"wp-caption alignnone\"><a href=\"https:\/\/nylonplastic.com\/nl\/industrieen\/\"><img decoding=\"async\" class=\"wp-image-2409 size-full\" src=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_06.jpg\" alt=\"Verschillende toepassingsscenario&#039;s van PA-kunststoffen\" width=\"800\" height=\"740\"  title=\"PA6 CF10 Nylon 6 met 10% Koolstofvezels | Nylon Plastiek\" srcset=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_06.jpg 800w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_06-300x278.jpg 300w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_06-768x710.jpg 768w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_06-600x555.jpg 600w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/a><figcaption id=\"caption-attachment-2409\" class=\"wp-caption-text\">Verschillende toepassingsscenario's van PA-kunststoffen<\/figcaption><\/figure>\n<\/div>\n<h3><strong>Hoe kies je de juiste PA6 CF-kwaliteit?<\/strong><\/h3>\n<p class=\"ds-markdown-paragraph\">Eenvoudig gezegd:<\/p>\n<p class=\"ds-markdown-paragraph\"><strong>Voor een toegankelijke instap in koolstofvezelprestaties<\/strong>\u00a0met verbeterde stijfheid, dimensionale stabiliteit en statische controle, overweeg dan\u00a0<strong>PA6 CF10<\/strong>. Het biedt een duidelijke upgrade ten opzichte van standaardmaterialen tegen een bescheiden prijs.<\/p>\n<p class=\"ds-markdown-paragraph\"><strong>Voor een optimale balans tussen hoge sterkte, lichtgewicht ontwerp en functionele geleidbaarheid<\/strong>\u00a0in veeleisende metaalvervangingstoepassingen, kies\u00a0<strong>PA6 CF30<\/strong>. Het is de prestatiestandaard voor de meeste structurele toepassingen.<\/p>\n<p class=\"ds-markdown-paragraph\"><strong>Voor de ultieme stijfheid, sterkte en thermische\/elektrische prestaties<\/strong>\u00a0waar gewichtsbesparing en betrouwbaarheid van cruciaal belang zijn en de kosten minder gevoelig zijn, overweeg dan\u00a0<strong>PA6 CF50<\/strong>. Een hoger koolstofvezelgehalte maximaliseert deze geavanceerde eigenschappen.<\/p>\n<p class=\"ds-markdown-paragraph\"><strong style=\"font-size: 1.7em;\">Waarom voor ons kiezen?<\/strong><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone wp-image-2407 size-full\" src=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_03.jpg\" alt=\"\u4e07\u7ff0\u8be6\u60c5 03\" width=\"800\" height=\"673\"  title=\"PA6 CF10 Nylon 6 met 10% Koolstofvezels | Nylon Plastiek\" srcset=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_03.jpg 800w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_03-300x252.jpg 300w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_03-768x646.jpg 768w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_03-600x505.jpg 600w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"alignnone wp-image-2408 size-full\" src=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_04.jpg\" alt=\"\u4e07\u7ff0\u8be6\u60c5 04\" width=\"800\" height=\"576\"  title=\"PA6 CF10 Nylon 6 met 10% Koolstofvezels | Nylon Plastiek\" srcset=\"https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_04.jpg 800w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_04-300x216.jpg 300w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_04-768x553.jpg 768w, https:\/\/nylonplastic.com\/wp-content\/uploads\/2025\/11\/\u4e07\u7ff0\u8be6\u60c5_04-600x432.jpg 600w\" sizes=\"(max-width: 800px) 100vw, 800px\" \/><\/p>\n<h2><strong>FAQ <\/strong><strong>Sectie<\/strong><strong>:<\/strong><\/h2>\n<p class=\"ds-markdown-paragraph\"><strong>V1: Wat zijn de voordelen van PA6 CF10 ten opzichte van standaard PA6?<\/strong><br \/>\nPA6 CF10 biedt een aanzienlijke upgrade met 10% koolstofvezelversterking. De belangrijkste voordelen zijn:<\/p>\n<ul>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong>Verbeterde stijfheid en kracht:<\/strong>\u00a0Verbeterde mechanische eigenschappen voor robuustere onderdelen.<\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong>Dimensionale stabiliteit:<\/strong>\u00a0Lagere thermische uitzetting en vochtabsorptie voor betrouwbare prestaties.<\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong>Statische dissipatie:<\/strong>\u00a0Inherente geleidbaarheid beschermt gevoelige elektronische onderdelen.<\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\">Het is de ideale\u00a0<strong>kosteneffectief toegangspunt<\/strong>\u00a0in koolstofvezelcomposieten.<\/p>\n<\/li>\n<\/ul>\n<p class=\"ds-markdown-paragraph\"><strong>V2: Is PA6 CF10 geschikt voor elektronische behuizingen?<\/strong><br \/>\nJa, het is een uitstekende keuze. Naast goede structurele eigenschappen\u00a0<strong>natuurlijk ESD-vermogen (elektrostatische ontlading)<\/strong>\u00a0helpt statische schade aan interne componenten te voorkomen, waardoor het geschikt is voor connectoren, behuizingen en frames in elektronische apparaten.<\/p>\n<p class=\"ds-markdown-paragraph\"><strong>V3: Hoe moet ik PA6 CF10 verwerken?<\/strong><br \/>\nVoor de beste resultaten:<\/p>\n<ul>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong>Grondig drogen<\/strong>\u00a0bij 80-90\u00b0C gedurende 4-6 uur voor het gieten.<\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\">Gebruik aanbevolen smelttemperaturen (meestal 280-300\u00b0C).<\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\"><strong>Schimmeltemperatuur<\/strong>\u00a0moet 80-100\u00b0C zijn voor een optimale oppervlakteafwerking.<\/p>\n<\/li>\n<li>\n<p class=\"ds-markdown-paragraph\">Deze instellingen zorgen voor een sterke vezelbinding en consistentie van het werkstuk.<\/p>\n<\/li>\n<\/ul>\n\t\t\t<div class=\"srfm-form-container srfm-form-container-305 srfm-bg-color\">\n\t\t\t<style>\n\t\t\t\t\/* Need to check and remove the input variables related to the Style Tab. *\/\n\t\t\t\t.srfm-form-container-305 {\n\t\t\t\t\t\/* New test variables *\/\n\t\t\t\t\t--srfm-color-scheme-primary: var(--ast-global-color-0);\n\t\t\t\t\t--srfm-color-scheme-text-on-primary: var(--ast-global-color-2);\n\t\t\t\t\t--srfm-color-scheme-text: var(--ast-global-color-2);\n\t\t\t\t\t--srfm-quill-editor-color: var(--ast-global-color-0);\n\n\t\t\t\t\t--srfm-color-input-label: var(--ast-global-color-2);\n\t\t\t\t\t--srfm-color-input-description: hsl( from var(--ast-global-color-2) h s l \/ 0.65 );\n\t\t\t\t\t--srfm-color-input-placeholder: hsl( from var(--ast-global-color-2) h s l \/ 0.5 );\n\t\t\t\t\t--srfm-color-input-text: var(--ast-global-color-2);\n\t\t\t\t\t--srfm-color-input-prefix: hsl( from var(--ast-global-color-2) h s l \/ 0.65 );\n\t\t\t\t\t--srfm-color-input-background: hsl( from var(--ast-global-color-2) h s l \/ 0.02 );\n\t\t\t\t\t--srfm-color-input-background-hover: hsl( from var(--ast-global-color-2) h s l \/ 0.05 );\n\t\t\t\t\t--srfm-color-input-background-disabled: hsl( from var(--ast-global-color-2) h s l \/ 0.07 );\n\t\t\t\t\t--srfm-color-input-border: hsl( from var(--ast-global-color-2) h s l \/ 0.25 );\n\t\t\t\t\t--srfm-color-input-border-disabled: hsl( from var(--ast-global-color-2) h s l \/ 0.15 );\n\t\t\t\t\t--srfm-color-multi-choice-svg: hsl( from var(--ast-global-color-2) h s l \/ 0.7 );\n\t\t\t\t\t--srfm-color-input-border-hover: hsl( from var(--ast-global-color-0) h s l \/ 0.65 );\n\t\t\t\t\t--srfm-color-input-border-focus-glow: hsl( from var(--ast-global-color-0) h s l \/ 0.15 );\n\t\t\t\t\t--srfm-color-input-selected: hsl( from var(--ast-global-color-0) h s l \/ 0.1 );\n\t\t\t\t\t--srfm-btn-color-hover: hsl( from var(--ast-global-color-0) h s l \/ 0.9 );\n\t\t\t\t\t--srfm-btn-color-disabled: hsl( from var(--ast-global-color-0) h s l \/ 0.25 );\n\n\t\t\t\t\t\/* Dropdown Variables *\/\n\t\t\t\t\t--srfm-dropdown-input-background-hover: hsl( from var(--ast-global-color-2) h s l \/ 0.05 );\n\t\t\t\t\t--srfm-dropdown-option-background-hover: hsl( from var(--ast-global-color-2) h s l \/ 0.10 );\n\t\t\t\t\t--srfm-dropdown-option-background-selected: hsl( from var(--ast-global-color-2) h s l \/ 0.05 );\n\t\t\t\t\t--srfm-dropdown-option-selected-icon: hsl( from var(--ast-global-color-2) h s l \/ 0.65 );\n\t\t\t\t\t--srfm-dropdown-option-text-color: hsl( from var(--ast-global-color-2) h s l \/ 0.80 );\n\t\t\t\t\t--srfm-dropdown-option-selected-text: var(--ast-global-color-2);\n\t\t\t\t\t--srfm-dropdown-badge-background: hsl( from var(--ast-global-color-2) h s l \/ 0.05 );\n\t\t\t\t\t--srfm-dropdown-badge-background-hover: hsl( from var(--ast-global-color-2) h s l \/ 0.10 );\n\t\t\t\t\t--srfm-dropdown-menu-border-color: hsl( from var(--ast-global-color-2) h s l \/ 0.10 );\n\t\t\t\t\t--srfm-dropdown-placeholder-color: hsl( from var(--ast-global-color-2) h s l \/ 0.50 );\n\t\t\t\t\t--srfm-dropdown-icon-color: hsl( from var(--ast-global-color-2) h s l \/ 0.65 );\n\t\t\t\t\t--srfm-dropdown-icon-disabled: hsl( from var(--ast-global-color-2) h s l \/ 0.25 );\n\n\t\t\t\t\t\/* Background Control Variables *\/\n\t\t\t\t\t--srfm-instant-form-padding-top: 32px;--srfm-instant-form-padding-right: 32px;--srfm-instant-form-padding-bottom: 32px;--srfm-instant-form-padding-left: 32px;--srfm-instant-form-border-radius-top: 12px;--srfm-instant-form-border-radius-right: 12px;--srfm-instant-form-border-radius-bottom: 12px;--srfm-instant-form-border-radius-left: 12px;--srfm-form-padding-top: 0px;--srfm-form-padding-right: 0px;--srfm-form-padding-bottom: 0px;--srfm-form-padding-left: 0px;--srfm-form-border-radius-top: 99px;--srfm-form-border-radius-right: 99px;--srfm-form-border-radius-bottom: 99px;--srfm-form-border-radius-left: 99px;--srfm-bg-overlay-opacity: 1;\t\t\t\t\t--srfm-row-gap-between-blocks: 18px;--srfm-address-label-font-size: 16px;--srfm-address-label-line-height: 24px;--srfm-address-description-font-size: 14px;--srfm-address-description-line-height: 20px;--srfm-col-gap-between-fields: 16px;--srfm-row-gap-between-fields: 16px;--srfm-gap-below-address-label: 14px;--srfm-dropdown-font-size: 14px;--srfm-dropdown-gap-between-input-menu: 4px;--srfm-dropdown-badge-padding: 2px 6px;--srfm-dropdown-multiselect-font-size: 12px;--srfm-dropdown-multiselect-line-height: 16px;--srfm-dropdown-padding-right: 12px;--srfm-dropdown-padding-right-icon: calc( var( --srfm-dropdown-padding-right ) + 20px );--srfm-dropdown-multiselect-padding: 8px var( --srfm-dropdown-padding-right-icon ) 8px 8px;--srfm-input-height: 44px;--srfm-input-field-padding: 10px 12px;--srfm-input-field-font-size: 16px;--srfm-input-field-line-height: 24px;--srfm-input-field-margin-top: 6px;--srfm-input-field-margin-bottom: 6px;--srfm-checkbox-label-font-size: 16px;--srfm-checkbox-label-line-height: 24px;--srfm-checkbox-description-font-size: 14px;--srfm-checkbox-description-line-height: 20px;--srfm-check-ctn-width: 16px;--srfm-check-ctn-height: 16px;--srfm-check-svg-size: 10px;--srfm-checkbox-margin-top-frontend: 4px;--srfm-checkbox-margin-top-editor: 6px;--srfm-check-gap: 8px;--srfm-checkbox-description-margin-left: 24px;--srfm-flag-section-padding: 10px 0 10px 12px;--srfm-gap-between-icon-text: 8px;--srfm-label-font-size: 16px;--srfm-label-line-height: 24px;--srfm-description-font-size: 14px;--srfm-description-line-height: 20px;--srfm-btn-padding: 10px 14px;--srfm-btn-font-size: 16px;--srfm-btn-line-height: 24px;--srfm-multi-choice-horizontal-padding: 20px;--srfm-multi-choice-vertical-padding: 20px;--srfm-multi-choice-internal-option-gap: 8px;--srfm-multi-choice-vertical-svg-size: 40px;--srfm-multi-choice-horizontal-image-size: 24px;--srfm-multi-choice-vertical-image-size: 120px;--srfm-multi-choice-outer-padding: 2px;\t\t\t\t}\n\t\t\t<\/style>\n\t\t\t\t\t\t\t<form method=\"post\" enctype=\"multipart\/form-data\" id=\"srfm-form-305\" class=\"srfm-form\"\n\t\t\t\tform-id=\"305\" after-submission=\"hide form\" message-type=\"same page\" success-url=\"\" ajaxurl=\"https:\/\/nylonplastic.com\/wp-admin\/admin-ajax.php\" data-submit-token=\"d6a1fe6a4a336615a96db9d7bff1c92f1259f25ce094c9d639c799ca80577d95\" action=\"\"\n\t\t\t\t>\n\t\t\t\t\n\t\t\t\t<input type=\"hidden\" value=\"305\" name=\"form-id\">\n\t\t\t\t<input type=\"hidden\" value=\"\" name=\"srfm-sender-email-field\" id=\"srfm-sender-email\">\n\t\t\t\t<input type=\"hidden\" value=\"\" id=\"srfm-page-break\">\n\t\t\t\t\t\t<p id=\"srfm-error-message\" class=\"srfm-common-error-message srfm-error-message srfm-head-error\" hidden>\t\t<span class=\"srfm-icon\" aria-hidden=\"true\">\n\t\t\t<svg xmlns=\"http:\/\/www.w3.org\/2000\/svg\" width=\"20\" height=\"20\" fill=\"none\"><path d=\"M9.99935 18.3327C14.6017 18.3327 18.3327 14.6017 18.3327 9.99935C18.3327 5.39698 14.6017 1.66602 9.99935 1.66602C5.39698 1.66602 1.66602 5.39698 1.66602 9.99935C1.66602 14.6017 5.39698 18.3327 9.99935 18.3327Z\" stroke=\"currentColor\" stroke-width=\"1.5\" stroke-linecap=\"round\" stroke-linejoin=\"round\" \/><path d=\"M10 6.66602V9.99935\" stroke=\"currentColor\" stroke-width=\"1.5\" stroke-linecap=\"round\" stroke-linejoin=\"round\" \/><path d=\"M10 13.334H10.0083\" stroke=\"currentColor\" stroke-width=\"1.5\" stroke-linecap=\"round\" stroke-linejoin=\"round\" \/><\/svg>\t\t<\/span>\n\t\t<span class=\"srfm-error-content\">Er is een fout opgetreden bij het verzenden van je formulier. Probeer het opnieuw.<\/span><\/p>\n\t\t\t\t\t\t<div data-block-id=\"7fa370fa\" class=\"wp-block-uagb-advanced-heading uagb-block uagb-block-7fa370fa 305\" >\n\t\t\t\t\t<h2 class=\"uagb-heading-text\">Laten we een oplossing op maat maken<\/h2>\t\t\t\t<\/div>\n\t\t\t\n\n\t\t\t<div data-block-id=\"bb2839a9\" class=\"srfm-block-single srfm-block srfm-input-block srf-input-bb2839a9-block  srfm-block-width-50 srfm-slug-text-field 305\" >\n\t\t\t\t\t\t\t\t<label id=\"srfm-label-bb2839a9-lbl-Rmlyc3QgTmFtZQ\" for=\"srfm-input-bb2839a9-lbl-Rmlyc3QgTmFtZQ\" class=\"srfm-block-label\">\n\t\t\t\t\t\tVoornaam\t\t\t\t\t\t\t\t\t\t\t\t\t<span class=\"srfm-required\" aria-hidden=\"true\"> *<\/span>\n\t\t\t\t\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-block-wrap\">\n\t\t\t\t<input class=\"srfm-input-common srfm-input-input\" type=\"text\" name=\"srfm-input-bb2839a9-lbl-Rmlyc3QgTmFtZQ-text-field\" id=\"srfm-input-bb2839a9-lbl-Rmlyc3QgTmFtZQ\"\n\t\t\t\t\taria-describedby='srfm-error-bb2839a9'\t\t\t\t\tdata-required=\"true\" aria-required=\"true\" data-unique=\"false\" maxlength=\"100\" value=\"\"  data-srfm-mask=\"none\"   \/>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"srfm-error-wrap\">\n\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-error-message\" data-srfm-id=\"srfm-error-bb2839a9\" data-error-msg=\"Dit veld is vereist.\" data-unique-msg=\"Waarde moet uniek zijn.\">\n\t\t\t\t\t\tDit veld is vereist.\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t<\/div>\n\t\t\n\n\t\t\t<div data-block-id=\"dbaa04c6\" class=\"srfm-block-single srfm-block srfm-input-block srf-input-dbaa04c6-block  srfm-block-width-50 srfm-slug-last-name 305\" >\n\t\t\t\t\t\t\t\t<label id=\"srfm-label-dbaa04c6-lbl-TGFzdCBOYW1l\" for=\"srfm-input-dbaa04c6-lbl-TGFzdCBOYW1l\" class=\"srfm-block-label\">\n\t\t\t\t\t\tAchternaam\t\t\t\t\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-block-wrap\">\n\t\t\t\t<input class=\"srfm-input-common srfm-input-input\" type=\"text\" name=\"srfm-input-dbaa04c6-lbl-TGFzdCBOYW1l-last-name\" id=\"srfm-input-dbaa04c6-lbl-TGFzdCBOYW1l\"\n\t\t\t\t\taria-describedby='srfm-error-dbaa04c6'\t\t\t\t\tdata-required=\"false\" aria-required=\"false\" data-unique=\"false\" maxlength=\"100\" value=\"\"  data-srfm-mask=\"none\"   \/>\n\t\t\t\t<\/div>\n\t\t\t\t<div class=\"srfm-error-wrap\">\n\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-error-message\" data-srfm-id=\"srfm-error-dbaa04c6\" data-error-msg=\"Dit veld is vereist.\" data-unique-msg=\"Waarde moet uniek zijn.\">\n\t\t\t\t\t\tDit veld is vereist.\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t<\/div>\n\t\t\n\n\t\t\t<div data-block-id=\"80af9bb9\" class=\"srfm-block-single srfm-block srfm-email-block srf-email-80af9bb9-block  srfm-block-width-50 srfm-slug-email 305 srfm-email-block-wrap\">\n\t\t\t\t<div class=\"srfm-email-block srf-email-80af9bb9-block\">\n\t\t\t\t\t\t\t\t\t\t<label id=\"srfm-label-80af9bb9-lbl-RW1haWw\" for=\"srfm-email-80af9bb9-lbl-RW1haWw\" class=\"srfm-block-label\">\n\t\t\t\t\t\tE-mail\t\t\t\t\t\t\t\t\t\t\t\t\t<span class=\"srfm-required\" aria-hidden=\"true\"> *<\/span>\n\t\t\t\t\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-block-wrap\">\n\t\t\t\t\t\t<input class=\"srfm-input-common srfm-input-email\" type=\"email\" name=\"srfm-email-80af9bb9-lbl-RW1haWw-email\" id=\"srfm-email-80af9bb9-lbl-RW1haWw\"\n\t\t\t\t\t\taria-describedby='srfm-error-80af9bb9'\t\t\t\t\t\tdata-required=\"true\" aria-required=\"true\" data-unique=\"false\" value=\"\"   \/>\n\t\t\t\t\t<\/div>\n\t\t\t\t\t<div class=\"srfm-error-wrap\">\n\t\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-error-message\" data-srfm-id=\"srfm-error-80af9bb9\" data-error-msg=\"Dit veld is vereist.\" data-unique-msg=\"Waarde moet uniek zijn.\">\n\t\t\t\t\t\tDit veld is vereist.\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t<\/div>\n\t\t\t\t\t\t\t<\/div>\n\t\t\n\n\t\t<div data-block-id=\"0c6821ab\" class=\"srfm-block-single srfm-block srfm-phone-block srf-phone-0c6821ab-block srfm-block-width-50 305\">\n\t\t\t\t\t\t\t\t<label id=\"srfm-label-0c6821ab-lbl-UGhvbmUgTnVtYmVy\" for=\"srfm-phone-0c6821ab-lbl-UGhvbmUgTnVtYmVy\" class=\"srfm-block-label\">\n\t\t\t\t\t\tTelefoonnummer\t\t\t\t\t\t\t\t\t\t\t\t\t<span class=\"srfm-required\" aria-hidden=\"true\"> *<\/span>\n\t\t\t\t\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-block-wrap\">\n\t\t\t\t<input type=\"tel\"\n\t\t\t\t\tclass=\"srfm-input-common srfm-input-phone\"\n\t\t\t\t\tname=\"srfm-phone-0c6821ab-lbl-UGhvbmUgTnVtYmVy-phone-number\"\n\t\t\t\t\tid=\"srfm-phone-0c6821ab-lbl-UGhvbmUgTnVtYmVy\"\n\t\t\t\t\taria-describedby='srfm-error-0c6821ab'\t\t\t\t\tdata-required=\"true\"\n\t\t\t\t\taria-required=\"true\"\n\t\t\t\t\tdefault-country=\"us\"\n\t\t\t\t\t\t\t\t\t\tvalue=\"\"\n\t\t\t\t\t\t\t\t\t\tdata-unique=\"false\">\n\t\t\t<\/div>\n\t\t\t<div class=\"srfm-error-wrap\">\n\t\t\t\t\t\t\t\t\t<div class=\"srfm-error-message\" data-srfm-id=\"srfm-error-0c6821ab\" data-error-msg=\"Dit veld is vereist.\" data-unique-msg=\"Waarde moet uniek zijn.\">\n\t\t\t\t\t\tDit veld is vereist.\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t<\/div>\n\t\t<\/div>\n\t\t\n\n\t\t<div data-block-id=\"fabb13d5\" class=\"srfm-block-single srfm-block srfm-textarea-block srf-textarea-fabb13d5-block  srfm-block-width-100 305\">\n\t\t\t\t\t\t\t\t<label id=\"srfm-label-fabb13d5-lbl-WW91ciBNZXNzYWdl-8852\" for=\"srfm-textarea-fabb13d5-lbl-WW91ciBNZXNzYWdl-8852\" class=\"srfm-block-label\">\n\t\t\t\t\t\tUw bericht\t\t\t\t\t\t\t\t\t\t\t\t\t<span class=\"srfm-required\" aria-hidden=\"true\"> *<\/span>\n\t\t\t\t\t\t\t\t\t\t\t<\/label>\n\t\t\t\t\t\t\t\t\t\t\t<div class=\"srfm-block-wrap\">\n\t\t\t\t<textarea\n\t\t\t\t\tclass=\"srfm-input-common srfm-input-textarea\"\n\t\t\t\t\tname=\"srfm-textarea-fabb13d5-lbl-WW91ciBNZXNzYWdl-your-message\"\n\t\t\t\t\tid=\"srfm-textarea-fabb13d5-lbl-WW91ciBNZXNzYWdl-8852\"\n\t\t\t\t\taria-describedby='srfm-error-fabb13d5'\t\t\t\t\tdata-required=\"true\" aria-required=\"true\"  rows=\"4\"  \t\t\t\t\t\t\t\t\t\t\t\t\t\t\t><\/textarea>\n\t\t\t\t\t\t\t<\/div>\n\t\t\t\t\t\t<div class=\"srfm-error-wrap\">\n\t\t\t\t\t\t\t\t\t<div class=\"srfm-error-message\" data-srfm-id=\"srfm-error-fabb13d5\" data-error-msg=\"Dit veld is vereist.\">\n\t\t\t\t\t\tDit veld is vereist.\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t\t<\/div>\n\t\t<\/div>\n\n\t\t\t\t\t\t\t\n\t\t\t\t\t\n\t\t\t\t\t<div class=\"srfm-submit-container\" style=\"\">\n\t\t\t\t\t\t<div style=\"width: ; text-align: left\" class=\"wp-block-button\">\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<button style=\"\" id=\"srfm-submit-btn\" class=\"srfm-btn-frontend srfm-button srfm-submit-button\"\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t>\n\t\t\t\t\t\t\t\t<div class=\"srfm-submit-wrap\">\n\t\t\t\t\t\t\t\t\tStuur  in\t\t\t\t\t\t\t\t<div class=\"srfm-loader\"><\/div>\n\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t<\/button>\n\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t\t<\/div>\n\t\t\t\t\t<\/div>\n\t\t\t\t\t\t\t<p id=\"srfm-error-message\" class=\"srfm-common-error-message srfm-error-message srfm-footer-error\" hidden>\t\t<span class=\"srfm-icon\" aria-hidden=\"true\">\n\t\t\t<svg xmlns=\"http:\/\/www.w3.org\/2000\/svg\" width=\"20\" height=\"20\" fill=\"none\"><path d=\"M9.99935 18.3327C14.6017 18.3327 18.3327 14.6017 18.3327 9.99935C18.3327 5.39698 14.6017 1.66602 9.99935 1.66602C5.39698 1.66602 1.66602 5.39698 1.66602 9.99935C1.66602 14.6017 5.39698 18.3327 9.99935 18.3327Z\" stroke=\"currentColor\" stroke-width=\"1.5\" stroke-linecap=\"round\" stroke-linejoin=\"round\" \/><path d=\"M10 6.66602V9.99935\" stroke=\"currentColor\" stroke-width=\"1.5\" stroke-linecap=\"round\" stroke-linejoin=\"round\" \/><path d=\"M10 13.334H10.0083\" stroke=\"currentColor\" stroke-width=\"1.5\" stroke-linecap=\"round\" stroke-linejoin=\"round\" \/><\/svg>\t\t<\/span>\n\t\t<span class=\"srfm-error-content\">Er is een fout opgetreden bij het verzenden van je formulier. Probeer het opnieuw.<\/span><\/p>\n\t\t\t\t\t<input type=\"hidden\" name=\"trp-form-language\" value=\"nl\"\/><\/form>\n\t\t\t<div class=\"srfm-single-form srfm-success-box in-page\">\n\t\t\t\t<div aria-live=\"polite\" aria-atomic=\"true\" role=\"alert\" id=\"srfm-success-message-page-305\" class=\"srfm-success-box-description\"><\/div>\n\t\t\t<\/div>\n\t\t\t\t\t\t<\/div>","protected":false},"excerpt":{"rendered":"<h5><\/h5>\n<p class=\"ds-markdown-paragraph\">PA6 CF10 is een thermoplastisch composietmateriaal. Het is gebaseerd op nylon 6 (PA6) versterkt met 10% koolstofvezels. Deze koolstofvezelkwaliteit op instapniveau biedt een duidelijke verbetering ten opzichte van standaard en glasgevulde nylon en biedt een verbeterde stijfheid, superieure maatvastheid en inherente statische dissipatie, waardoor het geschikt is voor technische onderdelen die betere prestaties en betrouwbaarheid vereisen.<\/p>\n<p class=\"ds-markdown-paragraph\"><strong>Waarom PA6 CF10 van Nylon Plastic kiezen?<\/strong><br \/>\n\u2705\u00a0<strong>Verbeterde stijfheid en geleidbaarheid:<\/strong>\u00a0We leveren een materiaal dat een merkbare toename in stijfheid en betrouwbare statische dissipatie biedt in vergelijking met ongevuld of glasgevuld PA6, waardoor het ideaal is voor gevoelige elektronische behuizingen, tandwielen en mechanisch belaste onderdelen die baat hebben bij deze eigenschappen.<br \/>\n\u2705\u00a0<strong>Superieure dimensionale stabiliteit en precisie:<\/strong>\u00a0Onze PA6 CF10 biedt een uitzonderlijk lage thermische uitzetting en vochtabsorptie, waardoor nauwkeurige maattoleranties en consistente prestaties in verschillende omgevingsomstandigheden gegarandeerd zijn.<br \/>\n\u2705\u00a0<strong>Deskundige begeleiding voor kwaliteitsresultaten:<\/strong>\u00a0We bieden verwerkingsondersteuning voor deze koolstofvezelverbinding om een optimale oppervlakteafwerking en mechanische eigenschappen te bereiken, zodat de kloof tussen standaardmaterialen en geavanceerde composieten wordt overbrugd.<br \/>\n\u2705\u00a0<strong>Kosteneffectieve instap in koolstofvezeltechnologie:<\/strong>\u00a0Wij zijn uw partner in prestatieverbetering. Ons team helpt u PA6 CF10 te implementeren om gewichtsvermindering, slijtvastheid en functionele integratie te bereiken waar geavanceerde composieten voorheen niet werden overwogen.<\/p>\n<div data-elementor-type=\"page\" data-elementor-id=\"3469\" class=\"elementor elementor-3469\" data-elementor-post-type=\"elementor_library\">\n<div class=\"elementor-element elementor-element-753a2e7 e-grid e-con-boxed e-con e-parent\" data-id=\"753a2e7\" data-element_type=\"container\" data-e-type=\"container\">\n<div class=\"e-con-inner\">\n<div class=\"elementor-element elementor-element-aaa8317 elementor-button-warning elementor-widget elementor-widget-button\" data-id=\"aaa8317\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"button.default\">\n<div class=\"elementor-widget-container\">\n<div class=\"elementor-button-wrapper\">\n\t\t\t\t\t<a class=\"elementor-button elementor-button-link elementor-size-sm\" href=\"#elementor-action%3Aaction%3Dpopup%3Aopen%26settings%3DeyJpZCI6IjI0MDQiLCJ0b2dnbGUiOmZhbHNlfQ%3D%3D\"><br \/>\n\t\t\t\t\t\t<span class=\"elementor-button-content-wrapper\"><br \/>\n\t\t\t\t\t\t\t\t\t<span class=\"elementor-button-text\">Stuur uw bestand<\/span><br \/>\n\t\t\t\t\t<\/span><br \/>\n\t\t\t\t\t<\/a>\n\t\t\t\t<\/div>\n<\/p><\/div>\n<\/p><\/div>\n<div class=\"elementor-element elementor-element-69ce54b elementor-button-success elementor-widget elementor-widget-button\" data-id=\"69ce54b\" data-element_type=\"widget\" data-e-type=\"widget\" data-widget_type=\"button.default\">\n<div class=\"elementor-widget-container\">\n<div class=\"elementor-button-wrapper\">\n\t\t\t\t\t<a class=\"elementor-button elementor-button-link elementor-size-sm\" href=\"https:\/\/nylonplastic.com\/nl\/neem-contact-op-met\/\"><br \/>\n\t\t\t\t\t\t<span class=\"elementor-button-content-wrapper\"><br \/>\n\t\t\t\t\t\t\t\t\t<span class=\"elementor-button-text\">Neem contact met ons op<\/span><br \/>\n\t\t\t\t\t<\/span><br \/>\n\t\t\t\t\t<\/a>\n\t\t\t\t<\/div>\n<\/p><\/div>\n<\/p><\/div>\n<\/p><\/div>\n<\/p><\/div>\n<\/p><\/div>","protected":false},"featured_media":2810,"comment_status":"closed","ping_status":"closed","template":"","meta":{"rop_custom_images_group":[],"rop_custom_messages_group":[],"rop_publish_now":"initial","rop_publish_now_accounts":{"facebook_846085238273622_899381133262461":""},"rop_publish_now_history":[],"rop_publish_now_status":"pending","site-sidebar-layout":"default","site-content-layout":"","ast-site-content-layout":"default","site-content-style":"default","site-sidebar-style":"default","ast-global-header-display":"","ast-banner-title-visibility":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","ast-disable-related-posts":"","theme-transparent-header-meta":"default","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","astra-migrate-meta-layouts":"set","ast-page-background-enabled":"default","ast-page-background-meta":{"desktop":{"background-color":"var(--ast-global-color-5)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}},"ast-content-background-meta":{"desktop":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"tablet":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""},"mobile":{"background-color":"var(--ast-global-color-4)","background-image":"","background-repeat":"repeat","background-position":"center center","background-size":"auto","background-attachment":"scroll","background-type":"","background-media":"","overlay-type":"","overlay-color":"","overlay-opacity":"","overlay-gradient":""}}},"product_brand":[43],"product_cat":[42,57],"product_tag":[],"class_list":["post-2808","product","type-product","status-publish","has-post-thumbnail","product_brand-nylon-plastic","product_cat-nylon-6","product_cat-pa6-carbon-fiber","desktop-align-left","tablet-align-left","mobile-align-left","first","instock","shipping-taxable","product-type-simple"],"_links":{"self":[{"href":"https:\/\/nylonplastic.com\/nl\/wp-json\/wp\/v2\/product\/2808","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nylonplastic.com\/nl\/wp-json\/wp\/v2\/product"}],"about":[{"href":"https:\/\/nylonplastic.com\/nl\/wp-json\/wp\/v2\/types\/product"}],"replies":[{"embeddable":true,"href":"https:\/\/nylonplastic.com\/nl\/wp-json\/wp\/v2\/comments?post=2808"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/nylonplastic.com\/nl\/wp-json\/wp\/v2\/media\/2810"}],"wp:attachment":[{"href":"https:\/\/nylonplastic.com\/nl\/wp-json\/wp\/v2\/media?parent=2808"}],"wp:term":[{"taxonomy":"product_brand","embeddable":true,"href":"https:\/\/nylonplastic.com\/nl\/wp-json\/wp\/v2\/product_brand?post=2808"},{"taxonomy":"product_cat","embeddable":true,"href":"https:\/\/nylonplastic.com\/nl\/wp-json\/wp\/v2\/product_cat?post=2808"},{"taxonomy":"product_tag","embeddable":true,"href":"https:\/\/nylonplastic.com\/nl\/wp-json\/wp\/v2\/product_tag?post=2808"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}