{"id":64,"count":10,"description":"A uniquely flexible and impact-resistant polyamide, PA11 stands out for its bio-based origin and exceptional durability. It maintains its properties over a wide temperature range and exhibits superior resistance to stress cracking when exposed to fuels, salts, and various chemicals.\r\nKey Applications: Automotive fuel lines, fluid transfer hoses, pneumatic airbrake tubing, sports footwear components, and protective coatings for cables.","link":"https:\/\/nylonplastic.com\/ru\/%d0%bf%d1%80%d0%be%d0%b4%d1%83%d0%ba%d1%82-%d0%ba%d0%b0%d1%82%d0%b5%d0%b3%d0%be%d1%80%d0%b8%d1%8f-2\/polyamide-11\/","name":"PA11","slug":"polyamide-11","taxonomy":"product_cat","parent":0,"meta":[],"menu_order":12,"_links":{"self":[{"href":"https:\/\/nylonplastic.com\/ru\/wp-json\/wp\/v2\/product_cat\/64","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/nylonplastic.com\/ru\/wp-json\/wp\/v2\/product_cat"}],"about":[{"href":"https:\/\/nylonplastic.com\/ru\/wp-json\/wp\/v2\/taxonomies\/product_cat"}],"wp:post_type":[{"href":"https:\/\/nylonplastic.com\/ru\/wp-json\/wp\/v2\/product?product_cat=64"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}