Nylon 6 vs Nylon 66 — Engineering Plastic Selection Guide

nylon 6 plastic pellets granules industrial packaging

Chemical Structure Differences

The fundamental difference between PA6 (Nylon 6) und PA66 (Nylon 66) lies in their molecular structure:

  • Nylon 6: Made from caprolactam, has 6 carbon atoms in each repeating unit. Less crystalline structure.
  • Nylon 66: Made from hexamethylenediamine and adipic acid, has two 6-carbon chains. More crystalline structure.

Mechanical Properties Comparison

Eigentum PA6 PA66
Zugfestigkeit 70-85 MPa 80-100 MPa
Biegemodus 2.5-3.0 GPa 2.8-3.5 GPa
Dehnung beim Bruch 30-100% 15-60%
Notched Izod Impact 50-100 J/m 40-80 J/m
Schmelzpunkt 220°C 260°C
HDT at 1.8 MPa 70°C 90°C

Feuchtigkeitsabsorption

Moisture absorption is critical for nylon applications:

Condition PA6 PA66
At 50% RH 2.5-3.0% 2.0-2.5%
Saturation 8-10% 6-8%

Processing Characteristics

Nylon 6 Processing

  • Melting Point: 220°C
  • Processing Range: 240-280°C
  • Mold Temperature: 40-80°C

Nylon 66 Processing

  • Melting Point: 260°C
  • Processing Range: 280-320°C
  • Mold Temperature: 60-90°C

Applications by Material

Nylon 6 Applications

  • Gears and sprockets
  • Industrial monofilament
  • Film and packaging
  • Consumer products

Nylon 66 Applications

  • Automotive under-hood components
  • Electrical connectors
  • High-temperature bearings
  • Precision mechanical components

Reinforced Grades

Both materials are commonly reinforced with glass fiber:

Klasse PA6 + GF30 PA66 + GF30
Zugfestigkeit 140-160 MPa 170-200 MPa
HDT (1.8 MPa) 205°C+ 250°C+
Feuchtigkeitsabsorption 1.0-1.5% 0.8-1.2%

Selection Summary

Choose Nylon 6 when:

  • Impact resistance is critical
  • Cost sensitivity is high
  • Operating temperatures are moderate

Choose Nylon 66 when:

  • Higher mechanical strength is required
  • Elevated temperatures are expected
  • Dimensional stability is critical

Frequently Asked Questions

Is Nylon 66 stronger than Nylon 6?

Yes. Nylon 66 typically offers 15-25% higher tensile strength due to more crystalline structure.

Which nylon is better for gears?

Both work well. PA6 is preferred for impact-loaded gears due to higher toughness. PA66 is better for high-load, high-temperature gear applications.

Where can I source quality PA6 and PA66?

Nylonplastic supplies both grades in natural, colored, and reinforced versions. Contact us for samples.

Nylon 6 vs Nylon 66 — Frequently Asked Questions

Is Nylon 66 stronger than Nylon 6?

Yes. Nylon 66 typically offers 15-25% higher tensile strength (80-100 MPa vs 70-85 MPa) due to more crystalline structure.

Which nylon is better for gears?

Both work well. PA6 is preferred for impact-loaded gears due to higher toughness. PA66 is better for high-load, high-temperature applications.

Where can I source quality PA6 and PA66 granules?

Nylonplastic supplies both grades in natural, colored, and reinforced versions. Contact us for samples.



Entwerfen wir Ihre individuelle Lösung

This field is required.

This field is required.

This field is required.

This field is required.

Entwerfen wir Ihre individuelle Lösung

Dieses Feld ist erforderlich.
Dieses Feld ist erforderlich.
Dieses Feld ist erforderlich.
Dieses Feld ist erforderlich.
Nach oben blättern