Why Glass Fiber Reinforcement?
Adding glass fiber to nylon dramatically improves mechanical properties, making it suitable for demanding applications that unreinforced nylon cannot handle.
Property Improvements
| Propiedad | PA6 | PA6 + 30% GF |
|---|---|---|
| Resistencia a la tracción | 75 MPa | 150 MPa |
| Módulo de flexión | 2.8 GPa | 7.5 GPa |
| HDT (1.8 MPa) | 70°C | 205°C |
| Absorción de humedad | 8% | 1.5% |
Aplicaciones
- Automotive: radiator end tanks, intake manifolds
- Electrical: high-temperature connectors
- Industrial: pump housings, valve bodies
Processing Guidelines
- Dry at 80-100°C for 4-6 hours
- Use wear-resistant screw
- Higher mold temperatures (60-90°C)
Frequently Asked Questions
How much stronger is glass fiber nylon?
PA6 with 30% glass fiber offers approximately 2x tensile strength and 3x stiffness.
Where can I source glass fiber reinforced nylon?
Nylonplastic supplies PA6-GF and PA66-GF in various fiber contents. Contact us for samples.
Glass Fiber Reinforced Nylon — Frequently Asked Questions
How much stronger is glass fiber nylon?
PA6 with 30% glass fiber offers approximately 2x tensile strength and 3x stiffness.
Where can I source glass fiber reinforced nylon?
Nylonplastic supplies PA6-GF and PA66-GF in various fiber contents. Contact us for samples.