Propriétés des matériaux en nylon : Une référence technique complète

Comprehensive technical data on nylon/PA material properties — thermal, mechanical, chemical resistance, electrical, and comparison tables across grades.

Propriétés des matériaux

Overview of Nylon Material Properties

Propriétés des matériaux

Nylon (polyamide) materials occupy a unique position in engineering thermoplastics: they offer the highest combination of strength, toughness, and wear resistance among non-reinforced plastics, while remaining processable on standard injection molding and extrusion equipment. This technical reference compiles the key properties that engineers, designers, and procurement specialists need when evaluating nylon for specific applications.

All data in this reference applies to conditioned material (23°C, 50% RH) unless otherwise noted. Moisture content significantly affects mechanical properties — dry-as-molded values can be 20-40% higher than conditioned values for unfilled nylon.

Mechanical Properties by Nylon Grade

Résistance à la traction (MPa)80829055170185
Allongement à la rupture (%)150604520033
Tensile Modulus (GPa)2.83.03.21.79.010.0
Flexural Strength (MPa)10011013075240270
Module de flexion (GPa)2.62.82.91.68.59.2
Unnotched Izod (J/m)No breakNo break450No break600700

**Key Observations**:
– PA6 has higher elongation (more ductile) but PA66 has higher strength
– Glass fiber reinforcement (GF30 = 30% glass fiber) increases strength 2-2.5× but dramatically reduces ductility
– PA46 outperforms all standard nylons in both strength and thermal resistance, at higher cost
– PA12 is the softest and most flexible — lowest strength but best impact resistance at low temperatures

Thermal Properties

Thermal performance is often the deciding factor in grade selection:

Melting Point (°C)225265295180225
Glass Transition Temp (°C)50-6065-707540-4550-60
HDT @ 0.45 MPa (°C)170250285145215
HDT @ 1.82 MPa (°C)659016055195
Continuous Service Temp (°C)100-115130-150170-18080-95140-160
Specific Heat (J/g·K)1.71.71.41.61.3

**HDT Notes**:
– Heat Deflection Temperature (HDT) measures temperature at which a specimen deflects 0.25mm under specified load
– Glass fiber reinforcement dramatically improves HDT — GF30 grades achieve 2-3× the HDT of unfilled grades at 1.82 MPa
– PA66-GF30 at 1.82 MPa: 250°C — suitable for under-hood automotive applications
– PA12’s low HDT limits use to room-temperature applications

Moisture Absorption and Environmental Effects

Nylon’s moisture absorption is a critical consideration — more so than almost any other engineering plastic:

PA61.6%9.5%2.5-3.0%
PA661.2%8.5%2.5%
PA461.2%6.5%2.0%
PA110.4%2.0%0.8%

**Impact of Moisture on Properties**:
– Tensile strength decreases 15-25% at saturated condition vs. dry-as-molded
– Impact resistance INCREASES with moisture absorption (nylon becomes tougher when conditioned)
– Dimensional change: PA6 swells approximately 0.4% per 1% moisture absorbed — must be accounted for in precision parts
– Electrical insulation properties degrade significantly with moisture (dielectric constant increases 2×)

**Design Recommendations**:
– PA12 for parts exposed to humid environments or water immersion
– Dry-as-molded properties for designing dimensional tolerances in molds
– Condition parts to equilibrium before measuring critical dimensions

Chemical Resistance of Nylon

Nylon’s chemical resistance profile determines suitability for industrial environments:

**Good Resistance (no significant attack at 23°C)**:
– Aliphatic hydrocarbons (gasoline, mineral oils, diesel)
– Alcohols (methanol, ethanol, isopropanol)
– Esters and ketones (acetone, MEK — limited exposure)
– Weak acids (acetic acid, citric acid — verify case-by-case)
– Dilute alkalis and salts

**Poor Resistance (attack or degradation)**:
– Concentrated mineral acids (HCl, H2SO4, HNO3) — rapid hydrolysis
– Strong oxidizing agents (hydrogen peroxide >10%)
– Phenol and formic acid — dissolves nylon
– Calcium chloride (desiccant) — causes stress cracking
– Strong alkalis at elevated temperature

**Specialty Grades for Chemical Service**:
– PA12 for automotive fuel lines — resistant to aromatic fuels and alcohol blends
– PA6I/6T (transparent nylon) for chemical contact applications requiring clarity
– Glass-filled grades for chemical pump housings and valve components

Electrical and Flammability Properties

**Electrical Properties** (at 50% RH conditioning):

Dielectric Strength (kV/mm)202018
Volume Resistivity (Ω·cm)10^1510^1510^14
Surface Resistivity (Ω)10^1310^1310^12
Dissipation Factor (1 MHz)0.020.020.03

**Flammability Ratings**:

GradeUL94 RatingOxygen Index (%)
PA6HB24
PA66HB24
PA12HB22
FR gradesV-032+

Nylon burns with a self-sustaining flame and drips. For electrical enclosures or components requiring flame retardancy, specify FR (flame retardant) grades — typically PA66 with halogen or phosphorus-based flame retardants.

FAQ

Propriétés des matériaux en nylon : Une référence technique complète
Propriétés des matériaux en nylon : Une référence technique complète
How do you know whether Nylon Material Properties: A Complete Technical Reference fits a part?

Nylon Material Properties: A Complete Technical Reference fits a part when its load capacity, temperature range, moisture exposure, wear behavior, and processing method match the real service conditions.

What properties should be checked for Nylon Material Properties: A Complete Technical Reference?

Vérifier la résistance, la rigidité, la résistance aux chocs, la résistance à la chaleur, l'absorption d'humidité, la stabilité dimensionnelle, le frottement, l'usure et la compatibilité chimique.

What is the biggest selection risk for Nylon Material Properties: A Complete Technical Reference?

Le plus grand risque est de choisir à partir d'une fiche technique sans tenir compte de l'environnement réel, de la méthode de traitement, de la géométrie de la pièce et de l'utilisation à long terme.

When should Nylon Material Properties: A Complete Technical Reference be tested before production?

Les essais sont recommandés lorsque la pièce est soumise à une charge, à la chaleur, à des produits chimiques, à l'humidité, à des tolérances serrées, à des exigences réglementaires ou à un nouvel environnement de travail.

Créons votre solution personnalisée

Ce champ est requis.
Ce champ est requis.
Ce champ est requis.
Ce champ est requis.
Défiler vers le haut