Plastic Materials Database | Comprehensive Material Selection

Engineering Plastics Database

Comprehensive material selection for manufacturing. Compare 200+ plastic materials with detailed properties and performance data.

200+ Materials
15 Material Types
6 Processes
50+ Applications

ABS

Standard
Tensile Strength 40 MPa
Heat Deflection 98°C
Impact Strength High
Chemical Resistance Medium

PP Homopolymer

Polypropylene
Tensile Strength 35 MPa
Heat Deflection 105°C
Impact Strength Medium
Chemical Resistance Excellent

Nylon 6/6

Polyamide
Tensile Strength 80 MPa
Heat Deflection 255°C
Impact Strength High
Wear Resistance Excellent

Polycarbonate

PC
Tensile Strength 65 MPa
Heat Deflection 138°C
Impact Strength Very High
Transparency Excellent

PEEK 450G

High Performance
Tensile Strength 100 MPa
Heat Deflection 315°C
Chemical Resistance Excellent
Wear Resistance Excellent

Acetal (POM)

Delrin
Tensile Strength 69 MPa
Heat Deflection 124°C
Friction Coefficient Very Low
Dimensional Stability Excellent

Material Comparison

Compare key properties of different plastic materials side by side.

PropertyABSPPNylon 6/6PCPEEKPOM
Tensile Strength (MPa)4035806510069
Flexural Modulus (GPa)2.31.52.82.43.82.8
HDT @ 1.82 MPa (°C)98105255138315124
Impact Strength (J/m)400501108508075
Density (g/cm³)1.050.911.141.201.321.41