Engineering Plastics Knowledge Base
Technical Data, Material Comparisons & Processing Guidelines for Optimal Performance
停止妥協。升級為高性能塑膠
Engineering Plastics Database
Comprehensive material selection for manufacturing. Compare 200+ plastic materials with detailed properties and performance data.
200+
材料
15
Material Types
6
Processes
50+
應用
ABS
Standard
拉伸強度
40 MPa
Heat Deflection
98°C
衝擊強度
高
耐化學性
Medium
CNC
Injection
PP Homopolymer
Polypropylene
拉伸強度
35 MPa
Heat Deflection
105°C
衝擊強度
Medium
耐化學性
極佳
Injection
Nylon 6/6
Polyamide
拉伸強度
80 MPa
Heat Deflection
255°C
衝擊強度
高
Wear Resistance
極佳
CNC
Injection
Polycarbonate
個人電腦
拉伸強度
65 MPa
Heat Deflection
138°C
衝擊強度
Very High
Transparency
極佳
CNC
Injection
PEEK 450G
High Performance
拉伸強度
100 MPa
Heat Deflection
315°C
耐化學性
極佳
Wear Resistance
極佳
CNC
Injection
乙縮醛 (POM)
Delrin
拉伸強度
69 MPa
Heat Deflection
124°C
Friction Coefficient
Very Low
尺寸穩定性
極佳
CNC
Injection
Material Comparison
Compare key properties of different plastic materials side by side.
| 財產 | ABS | PP | Nylon 6/6 | 個人電腦 | PEEK | POM |
|---|---|---|---|---|---|---|
| 拉伸強度 (MPa) | 40 | 35 | 80 | 65 | 100 | 69 |
| Flexural Modulus (GPa) | 2.3 | 1.5 | 2.8 | 2.4 | 3.8 | 2.8 |
| HDT @ 1.82 MPa (°C) | 98 | 105 | 255 | 138 | 315 | 124 |
| Impact Strength (J/m) | 400 | 50 | 110 | 850 | 80 | 75 |
| Density (g/cm³) | 1.05 | 0.91 | 1.14 | 1.20 | 1.32 | 1.41 |
We do not sell, trade, or rent your personal data. You can contact us at any time to request, update, or delete your information.