ガラス繊維入りナイロンとガラス繊維なしナイロンの比較:完全な性能比較

Glass-filled vs unfilled nylon
Glass fiber reinforcement transforms nylon’s mechanical properties

Adding glass fibers to nylon dramatically changes its performance characteristics. While unfilled nylon offers excellent toughness and processability, glass-filled grades deliver substantially higher strength, stiffness, and thermal stability.

What Is Glass-Filled Nylon?

Glass-filled nylon is a composite material consisting of nylon resin reinforced with short glass fibers. The most common grades contain 15%, 25%, 30%, or 50% glass fiber by weight.

機械的特性の比較

プロパティ PA6 Unfilled PA6 GF15 PA6 GF30 PA6 GF50
引張強さ (MPa) 75 120 170 210
曲げ弾性率 (GPa) 2.7 5.5 8.5 14.0
HDT at 1.8 MPa (°C) 65 180 195 210
Mechanical properties chart
Glass fiber content directly correlates with strength and stiffness improvements

寸法安定性

Glass fibers reduce the material’s coefficient of linear thermal expansion (CLTE) by 50-70%, bringing it closer to metals like aluminum.

Shrinkage comparison
Glass-filled nylon shows significantly lower and more uniform shrinkage

加工に関する考慮事項

Glass-filled nylon requires: higher melt temperatures, higher injection pressures, hardened molds due to abrasive wear, and careful gate design for fiber orientation.

Surface finish comparison
Glass-filled parts typically show a matte surface with visible fiber orientation

Cost Considerations

GF30 provides the best balance of cost and performance for most applications. It’s the most widely used glass-filled grade.

Application Guide

Choose Unfilled Nylon When:

  • Impact resistance and toughness are critical
  • Parts need good surface finish
  • Snap-fits or living hinges are required
  • Cost is the primary concern

Choose Glass-Filled Nylon When:

  • High strength and stiffness are needed
  • Dimensional stability under heat is critical
  • Metal replacement is the goal
  • Precision tolerances must be maintained

Our Capabilities

With over 300 CNC machines, we produce more than 10,000 pieces daily with tolerances as tight as ±0.005mm. We accept MOQ from 1 piece, with delivery times ranging from 24 hours to 15 days. We supply nylon in all grades—unfilled, GF15, GF30, and GF50. Get a quote within 24 hours.

よくある質問

Does glass-filled nylon absorb less moisture?

Yes. Glass fibers do not absorb moisture, so GF30 typically absorbs about 30% less moisture than unfilled nylon by weight.

Can glass-filled nylon parts be painted or plated?

Painting is possible but requires proper surface preparation. The glass fibers create a textured surface that can be challenging for high-gloss finishes.

Is glass-filled nylon more brittle?

Glass-filled nylon has lower elongation at break (3-5% vs 50-150%), making it less ductile, but GF30 maintains reasonable toughness.

Can I regrind glass-filled nylon?

Yes, but regrind reduces fiber length and degrades mechanical properties. Typically, no more than 20-25% regrind is recommended.