ABS vs PC vs PP vs PA — How to Choose the Right Injection Molding Plastic

ABS PC PP PA injection molding plastic materials comparison - Nylonplastic

The Four Pillars of Injection Molding

ABS, PC, PP, and PA account for over 70% of all injection molded parts globally.

ABS — The Versatile All-Rounder

  • Strengths: Excellent surface finish, good impact resistance, easy to mold
  • Limitations: Poor UV resistance, limited chemical resistance
  • Best for: Consumer electronics, automotive interiors, toys

ポリカーボネート(PC)

  • Strengths: Highest impact strength, optically clear, heat resistant
  • Limitations: Poor chemical resistance, requires careful drying
  • Best for: Safety products, lenses, medical devices

ポリプロピレン(PP)

  • Strengths: Best chemical resistance, flexible, low cost
  • Limitations: Poor UV resistance, lower strength
  • Best for: Packaging, containers, living hinges

Polyamide (PA/Nylon)

  • Strengths: Excellent mechanical properties, chemical resistant
  • Limitations: Absorbs moisture, requires drying
  • Best for: Gears, bearings, automotive parts