ガラス繊維入りナイロンとガラス繊維なしナイロンの比較:完全な性能比較

Glass-filled vs unfilled nylon
Glass fiber reinforcement transforms nylon’s mechanical properties

Adding glass fibers to nylon dramatically changes its performance characteristics. While unfilled nylon offers excellent toughness and processability, glass-filled grades deliver substantially higher strength, stiffness, and thermal stability.

What Is Glass-Filled Nylon?

Glass-filled nylon is a composite material consisting of nylon resin reinforced with short glass fibers. The most common grades contain 15%, 25%, 30%, or 50% glass fiber by weight.

機械的特性の比較

プロパティ PA6 Unfilled PA6 GF15 PA6 GF30 PA6 GF50
引張強さ (MPa) 75 120 170 210
曲げ弾性率 (GPa) 2.7 5.5 8.5 14.0
HDT at 1.8 MPa (°C) 65 180 195 210
Mechanical properties chart
Glass fiber content directly correlates with strength and stiffness improvements

寸法安定性

Glass fibers reduce the material’s coefficient of linear thermal expansion (CLTE) by 50-70%, bringing it closer to metals like aluminum.

Shrinkage comparison
Glass-filled nylon shows significantly lower and more uniform shrinkage

加工に関する考慮事項

Glass-filled nylon requires: higher melt temperatures, higher injection pressures, hardened molds due to abrasive wear, and careful gate design for fiber orientation.

Surface finish comparison
Glass-filled parts typically show a matte surface with visible fiber orientation

Cost Considerations

GF30 provides the best balance of cost and performance for most applications. It’s the most widely used glass-filled grade.

Application Guide

Choose Unfilled Nylon When:

  • Impact resistance and toughness are critical
  • Parts need good surface finish
  • Snap-fits or living hinges are required
  • Cost is the primary concern

Choose Glass-Filled Nylon When:

  • High strength and stiffness are needed
  • Dimensional stability under heat is critical
  • Metal replacement is the goal
  • Precision tolerances must be maintained

当社の能力

を超える。 300台のCNCマシン, を生産している。 毎日10,000個 という厳しい公差で ±0.005mm. .我々は受け入れる 1個からのMOQ, 納期は以下の通り。 24時間~15日間. We supply nylon in all grades—unfilled, GF15, GF30, and GF50. 24時間以内にお見積もりいたします。.

よくあるご質問

How do you know whether Glass-Filled vs Unfilled Nylon: Complete Performance Comparison fits a part?

Glass-Filled vs Unfilled Nylon: Complete Performance Comparison fits a part when its load capacity, temperature range, moisture exposure, wear behavior, and processing method match the real service conditions.

What properties should be checked for Glass-Filled vs Unfilled Nylon: Complete Performance Comparison?

Check strength, stiffness, impact resistance, heat resistance, moisture absorption, dimensional stability, friction, wear, and chemical compatibility.

What is the biggest selection risk for Glass-Filled vs Unfilled Nylon: Complete Performance Comparison?

The biggest risk is choosing from a datasheet value without considering actual environment, processing method, part geometry, and long-term use.

When should Glass-Filled vs Unfilled Nylon: Complete Performance Comparison be tested before production?

Testing is recommended when the part faces load, heat, chemicals, moisture, tight tolerances, regulatory requirements, or a new operating environment.