Food Grade Plastics — FDA-Compliant Materials Guide

Food Grade Plastics - image 1

FDA Food Contact Regulations

Plastic components contacting food must meet FDA 21 CFR requirements.

Common Food-Grade Materials

  • PA6-FDA / PA66-FDA: Food processing machinery
  • POM-FDA: Pump components, valves
  • PP-FDA: Containers, equipment
  • HDPE-FDA: Cutting boards, surfaces

Frequently Asked Questions

Can I use regular nylon for food contact?

No. Always specify FDA-compliant grades for food applications.

Where can I source FDA-compliant plastics?

Nylonplastic supplies food-grade materials with full FDA documentation.

Food Grade Plastics — Frequently Asked Questions

Can I use regular nylon for food contact?

No. Always specify FDA-compliant grades for food applications.

Where can I source FDA-compliant plastics?

Nylonplastic supplies food-grade materials with full FDA documentation.