PA66+Fibra de carbono

Featuring carbon fiber reinforcement, this advanced composite delivers exceptional stiffness, tensile strength, and reduced weight. It offers superior creep resistance and enhanced thermal conductivity compared to glass-fiber grades, ideal for high-performance applications.
Key Applications: Drone frames, automotive lightweight structural parts, high-end sports equipment, and industrial components requiring low inertia.