Der vollständige Leitfaden für Nylon-Sorten: PA6, PA66, PA11, PA12 und mehr

Nylon grades comprehensive guide
Choosing the right nylon grade is critical for engineering success

Nylon isn’t one material—it’s a family of polyamides with distinctly different properties. From the workhorse PA6 to the premium PA12, understanding the full range of nylon grades helps you select the optimal material for your application.

The Nylon Family Overview

Klasse Typ Schmelzpunkt Moisture (50% RH) Key Characteristic
PA6 Aliphatic 220°C 2.7% Toughness, processability
PA66 Aliphatic 260°C 2.5% Festigkeit, Hitzebeständigkeit
PA11 Bio-based 185°C 0.8% Flexibility, low moisture
PA12 Aliphatic 178°C 0.7% Lowest moisture absorption
PA46 Aliphatic 295°C 3.5% Highest heat resistance
Nylon grade comparison chart
Each nylon grade fills a specific performance niche

PA6: The Versatile Workhorse

PA6 is the most widely used nylon grade, representing approximately 60% of nylon consumption. It offers an excellent balance of strength, toughness, and processability.

Wichtige Eigenschaften

  • Tensile strength: 70-85 MPa
  • Excellent impact resistance
  • Good surface finish and colorability
  • Wider processing window than PA66

PA66: The High-Performance Standard

PA66 applications in automotive
PA66 dominates under-hood automotive applications

PA66 offers approximately 10-15% higher strength and stiffness than PA6, with superior heat resistance. It’s the preferred choice for demanding applications.

PA11 and PA12: The Specialty Nylons

PA11 and PA12 are distinguished by their exceptionally low moisture absorption—less than 1% even at saturation. This gives them outstanding dimensional stability.

PA11 and PA12 applications
PA11 and PA12 excel in chemical resistance and dimensional stability

PA46: The High-Temperature Specialist

PA46 (Stanyl) offers the highest heat resistance of any aliphatic nylon, with a melting point of 295°C.

Selection Guide

Anforderung Recommended Grade
General purpose, cost-sensitive PA6
High temperature (>120°C) PA66, PA46
Wet/humid environment PA12, PA11
Maximum stiffness PA66-GF30/50

Unser Leistungsvermögen

Mit über 300 CNC-Maschinen, produzieren wir mehr als 10.000 Stück täglich mit so engen Toleranzen wie ±0,005 mm. Wir akzeptieren MOQ ab 1 Stück, mit Lieferzeiten von 24 Stunden bis 15 Tage. We supply all major nylon grades. Erhalten Sie innerhalb von 24 Stunden ein Angebot.

FAQ

How do you know whether The Complete Guide to Nylon Grades: PA6, PA66, PA11, PA12 and More fits a part?

The Complete Guide to Nylon Grades: PA6, PA66, PA11, PA12 and More fits a part when its load capacity, temperature range, moisture exposure, wear behavior, and processing method match the real service conditions.

What properties should be checked for The Complete Guide to Nylon Grades: PA6, PA66, PA11, PA12 and More?

Check strength, stiffness, impact resistance, heat resistance, moisture absorption, dimensional stability, friction, wear, and chemical compatibility.

What is the biggest selection risk for The Complete Guide to Nylon Grades: PA6, PA66, PA11, PA12 and More?

The biggest risk is choosing from a datasheet value without considering actual environment, processing method, part geometry, and long-term use.

When should The Complete Guide to Nylon Grades: PA6, PA66, PA11, PA12 and More be tested before production?

Testing is recommended when the part faces load, heat, chemicals, moisture, tight tolerances, regulatory requirements, or a new operating environment.

Entwerfen wir Ihre individuelle Lösung

Dieses Feld ist erforderlich.
Dieses Feld ist erforderlich.
Dieses Feld ist erforderlich.
Dieses Feld ist erforderlich.
Dieses Feld ist erforderlich.

Weiterführende Lektüre

Nach oben blättern