Polycarbonate PC — Complete Guide to Engineering Properties and Industrial Applications

Clear polycarbonate PC sheet with optical clarity for engineering applications - Nylonplastic

What Is Polycarbonate?

PC is an amorphous engineering plastic known for exceptional impact strength (250x stronger than glass) and optical clarity.

Propriétés principales

  • Impact Strength: 600–900 J/m
  • Heat Deflection: 130°C
  • Transparency: Up to 90% light transmission
  • UL94 Rating: V-2

Applications

Safety glasses, helmets, automotive lenses, medical device housings, transparent structural components, smartphone screens.

CNC Machining PC

Requires careful drying (120°C for 4+ hours), moderate cutting speeds, and sharp tooling for clean edges.