POM Acetal (Polyoxymethylene) — The Complete CNC Machining Plastics Guide

POM acetal Delrin CNC machined gears and precision parts - Nylonplastic CNC service

What Is POM Acetal Plastic?

POM (Polyoxymethylene), also known as acetal or Delrin, is a highly crystalline engineering thermoplastic. Its combination of high stiffness, low friction, and excellent dimensional stability makes it ideal for precision mechanical components.

Key Properties of POM

  • Tensile Strength: 60–70 MPa
  • Flexural Modulus: 2,500–2,800 MPa
  • Melting Point: 165–175°C
  • Coefficient of Friction: 0.2–0.35

CNC Machining Best Practices

Use sharp carbide tools, 150–250 m/min cutting speed for turning, and air blast or flood coolant.

Common Applications

Gears, sprockets, bearings, bushings, guide rails, food processing equipment, and medical device components.

Créons votre solution personnalisée

Ce champ est requis.
Ce champ est requis.
Ce champ est requis.
Ce champ est requis.

Laisser un commentaire

Votre adresse e-mail ne sera pas publiée. Les champs obligatoires sont indiqués avec *

Défiler vers le haut