Mechanical Properties Compared

プロパティNylon (PA6)ポリカーボネート(PC)
引張強さ (MPa)70-8555-75
曲げ弾性率 (GPa)2.5-3.02.2-2.4
Notched Izod Impact (kJ/m²)5-1560-80
密度 (g/cm³)1.141.20
Impact resistance comparison
Polycarbonate offers dramatically higher impact resistance than nylon

Impact Resistance: Polycarbonate’s Signature Strength

Polycarbonate is legendary for its impact resistance—it’s used in bulletproof glass and safety goggles. With notched Izod impact values of 60-80 kJ/m², PC is virtually unbreakable under normal use.

Thermal and Optical Properties

Optical clarity comparison
Polycarbonate’s optical clarity is a key differentiator

Polycarbonate is naturally transparent with light transmission of 88-90%. Nylon is naturally translucent to opaque.

耐薬品性

Nylon holds a distinct advantage here. Polycarbonate has poor chemical resistance—it’s attacked by hydrocarbons, ketones, and many cleaners. Nylon offers excellent resistance to oils, greases, fuels, and many organic solvents.

Moisture and Environmental Resistance

Moisture and weathering comparison
Polycarbonate resists moisture but is susceptible to UV degradation

Polycarbonate absorbs negligible moisture (0.15-0.35%). Nylon’s moisture absorption (2.5-3.0%) can cause dimensional changes. However, PC is susceptible to UV degradation.

Application Guide

いつナイロンを選ぶか:

  • Chemical resistance to oils and fuels is needed
  • Wear resistance matters
  • Parts must survive dynamic loading

Choose Polycarbonate When:

  • Optical clarity is required
  • Exceptional impact resistance is critical
  • Dimensional stability under varying humidity is needed

当社の能力

を超える。 300台のCNCマシン, を生産している。 毎日10,000個 という厳しい公差で ±0.005mm. .我々は受け入れる 1個からのMOQ, 納期は以下の通り。 24時間~15日間. We machine both nylon and polycarbonate. 24時間以内にお見積もりいたします。.

よくあるご質問

How do you know whether Nylon vs Polycarbonate: Strength, Heat Resistance, and Cost Compared fits a part?

Nylon vs Polycarbonate: Strength, Heat Resistance, and Cost Compared fits a part when its load capacity, temperature range, moisture exposure, wear behavior, and processing method match the real service conditions.

What properties should be checked for Nylon vs Polycarbonate: Strength, Heat Resistance, and Cost Compared?

Check strength, stiffness, impact resistance, heat resistance, moisture absorption, dimensional stability, friction, wear, and chemical compatibility.

What is the biggest selection risk for Nylon vs Polycarbonate: Strength, Heat Resistance, and Cost Compared?

The biggest risk is choosing from a datasheet value without considering actual environment, processing method, part geometry, and long-term use.

When should Nylon vs Polycarbonate: Strength, Heat Resistance, and Cost Compared be tested before production?

Testing is recommended when the part faces load, heat, chemicals, moisture, tight tolerances, regulatory requirements, or a new operating environment.

カスタムソリューションを作りましょう

このフィールドは必須です。.
このフィールドは必須です。.
このフィールドは必須です。.
このフィールドは必須です。.

コメントを残す

メールアドレスが公開されることはありません。 が付いている欄は必須項目です

トップに戻る