Carbon fiber reinforced nylon (CF-Nylon) is a high-performance composite material where short carbon fibers (typically 10-30% by weight) are compounded into a nylon matrix. This reinforcement dramatically improves mechanical properties, making CF-Nylon one of the strongest engineering materials available for both 3D printing and CNC machining applications.




CF-Nylon Material Properties
With tensile strength up to 120 MPa for CF30 grades (vs 80 MPa for unfilled nylon 66) and flexural modulus of 15,000-18,000 MPa (approaching aluminum stiffness), CF-Nylon offers exceptional performance. The coefficient of thermal expansion is 70% lower than unfilled nylon, ensuring dimensional stability. Our PA6-CF 필라멘트 provides excellent strength-to-weight ratio.
3D Printing vs CNC Machining
For 3D printing, CF-Nylon offers rapid prototyping and complex geometries but requires hardened steel or ruby nozzle (brass wears rapidly). CNC machining provides consistent properties and tighter tolerances (±0.02mm). For CNC applications, our PA66-CF30 stock material is recommended.
애플리케이션
CF-Nylon is used in aerospace for UAV frames, satellite components, and interior brackets. Automotive applications include engine mounts, structural components, and lightweight replacements. Industrial uses include pump impellers, bearing surfaces, and wear components.
Source CF-Nylon Materials
As a specialized source manufacturer, we supply CF-Nylon in multiple grades with custom compounding capabilities. 문의하기 for samples and technical support.
Carbon Fiber Nylon — Frequently Asked Questions
Why does carbon fiber wear out brass nozzles quickly?
Carbon fiber has hardness of approximately 200 HB (Brinell), while standard brass has hardness of only 55-100 HB. A brass nozzle will wear out within 10-50 hours of printing with CF filament. Highly filled CF30 can destroy brass within 10 hours. Always use hardened steel or ruby nozzles.
Is CF-Nylon stronger than aluminum?
CF-Nylon PA66+CF30 has tensile strength up to 120 MPa with specific strength comparable to 6061-T6 aluminum at approximately 60% of the weight. Carbon fiber reinforcement reduces thermal expansion by 70% vs unfilled nylon.
Where can I source CF-Nylon materials?
Nylonplastic is a specialized manufacturer with ISO9001/14001/45001/IATF16949 certifications. We supply PA6+CF, PA66+CF30, and PA12+CF in filament, sheet, rod, and tube forms. Our 6000m2 facility has 300+ CNC machines. Contact us for free samples.
Get a Free Quote
Fill out the form below and our engineers will respond within 24 hours.
자주 묻는 질문
When is Carbon Fiber Reinforced Nylon — High-Strength FDM and CNC Material the right choice?
Carbon Fiber Reinforced Nylon — High-Strength FDM and CNC Material is the right choice when the part requires machined accuracy, controlled surfaces, repeatable features, and a material that can be cut reliably.
What should be confirmed before ordering Carbon Fiber Reinforced Nylon — High-Strength FDM and CNC Material?
생산을 시작하기 전에 도면 버전, 재료 등급, 공차, 수량, 임계 치수, 표면 마감 및 검사 요구 사항을 확인합니다.
What usually drives cost in Carbon Fiber Reinforced Nylon — High-Strength FDM and CNC Material?
비용은 일반적으로 재료, 설정 시간, 기계 시간, 공차 난이도, 고정, 공구 접근, 마감, 검사 및 주문 수량에 따라 결정됩니다.
How can quality risk be reduced in Carbon Fiber Reinforced Nylon — High-Strength FDM and CNC Material?
중요한 기능을 명확하게 표시하고, 불필요하게 엄격한 공차를 피하고, 제조 가능성을 조기에 확인하고, 중요한 치수에 대한 검사 데이터를 사용하면 품질 위험을 줄일 수 있습니다.