Carbon fiber reinforced nylon (CF-Nylon) is a high-performance composite material where short carbon fibers (typically 10-30% by weight) are compounded into a nylon matrix. This reinforcement dramatically improves mechanical properties, making CF-Nylon one of the strongest engineering materials available for both 3D printing and CNC machining applications.

Carbon Fiber Reinforced Nylon — High-Strength FDM and CNC Material
Carbon Fiber Reinforced Nylon — High-Strength FDM and CNC Material
Carbon Fiber Reinforced Nylon — High-Strength FDM and CNC Material
Carbon Fiber Reinforced Nylon — High-Strength FDM and CNC Material
Carbon Fiber Reinforced Nylon — High-Strength FDM and CNC Material
Carbon Fiber Reinforced Nylon — High-Strength FDM and CNC Material
Carbon Fiber Reinforced Nylon — High-Strength FDM and CNC Material
Carbon Fiber Reinforced Nylon — High-Strength FDM and CNC Material

CF-Nylon Material Properties

With tensile strength up to 120 MPa for CF30 grades (vs 80 MPa for unfilled nylon 66) and flexural modulus of 15,000-18,000 MPa (approaching aluminum stiffness), CF-Nylon offers exceptional performance. The coefficient of thermal expansion is 70% lower than unfilled nylon, ensuring dimensional stability. Our PA6-CFフィラメント provides excellent strength-to-weight ratio.

3D Printing vs CNC Machining

For 3D printing, CF-Nylon offers rapid prototyping and complex geometries but requires hardened steel or ruby nozzle (brass wears rapidly). CNC machining provides consistent properties and tighter tolerances (±0.02mm). For CNC applications, our PA66-CF30 stock material is recommended.

アプリケーション

CF-Nylon is used in aerospace for UAV frames, satellite components, and interior brackets. Automotive applications include engine mounts, structural components, and lightweight replacements. Industrial uses include pump impellers, bearing surfaces, and wear components.

Source CF-Nylon Materials

As a specialized source manufacturer, we supply CF-Nylon in multiple grades with custom compounding capabilities. お問い合わせ for samples and technical support.

Carbon Fiber Nylon — Frequently Asked Questions

Why does carbon fiber wear out brass nozzles quickly?

Carbon fiber has hardness of approximately 200 HB (Brinell), while standard brass has hardness of only 55-100 HB. A brass nozzle will wear out within 10-50 hours of printing with CF filament. Highly filled CF30 can destroy brass within 10 hours. Always use hardened steel or ruby nozzles.

Is CF-Nylon stronger than aluminum?

CF-Nylon PA66+CF30 has tensile strength up to 120 MPa with specific strength comparable to 6061-T6 aluminum at approximately 60% of the weight. Carbon fiber reinforcement reduces thermal expansion by 70% vs unfilled nylon.

Where can I source CF-Nylon materials?

Nylonplastic is a specialized manufacturer with ISO9001/14001/45001/IATF16949 certifications. We supply PA6+CF, PA66+CF30, and PA12+CF in filament, sheet, rod, and tube forms. Our 6000m2 facility has 300+ CNC machines. Contact us for free samples.

無料見積もり

下記のフォームにご記入いただければ、エンジニアが24時間以内に対応いたします。.

よくあるご質問

When is Carbon Fiber Reinforced Nylon — High-Strength FDM and CNC Material the right choice?

Carbon Fiber Reinforced Nylon — High-Strength FDM and CNC Material is the right choice when the part requires machined accuracy, controlled surfaces, repeatable features, and a material that can be cut reliably.

What should be confirmed before ordering Carbon Fiber Reinforced Nylon — High-Strength FDM and CNC Material?

製造開始前に、図面のバージョン、材料等級、公差、数量、重要寸法、表面仕上げ、検査要件を確認する。.

What usually drives cost in Carbon Fiber Reinforced Nylon — High-Strength FDM and CNC Material?

コストは通常、材料、段取り時間、機械時間、公差の難易度、治具、工具アクセス、仕上げ、検査、注文数量によって左右される。.

How can quality risk be reduced in Carbon Fiber Reinforced Nylon — High-Strength FDM and CNC Material?

重要なフィーチャーを明確にマーキングし、不必要な厳しい公差を避け、製造可能性を早期に確認し、重要な寸法の検査データを使用することで、品質リスクを低減します。.

カスタムソリューションを作りましょう

このフィールドは必須です。.
このフィールドは必須です。.
このフィールドは必須です。.
このフィールドは必須です。.

コメントを残す

メールアドレスが公開されることはありません。 が付いている欄は必須項目です

トップに戻る