Nylon vs POM (Acetal/Delrin): Kiezen tussen twee technische kunststoffen

Nylon vs POM Acetal comparison
Nylon and POM are both engineering plastics but serve different purposes

Nylon and POM (polyoxymethylene, also known as acetal or Delrin) are two of the most important engineering plastics. Both are widely used for precision mechanical components, but their distinctly different properties make each better suited for specific applications.

Mechanical Properties Head-to-Head

Eigendom PA6 (Nylon) POM (acetaal)
Treksterkte (MPa) 70-85 60-70
Flexural Modulus (GPa) 2.5-3.0 2.6-2.9
Rek bij breuk (%) 50-150 25-75
Dichtheid (g/cm³) 1.14 1.41
Mechanical properties radar chart
Nylon leads in strength and toughness; POM excels in dimensional stability

Wear and Friction: A Critical Difference

POM’s key advantage over nylon is its excellent wear resistance and low coefficient of friction (0.2-0.35 against steel), making it preferred for gears, bearings, and sliding components.

Vochtabsorptie

Moisture absorption comparison
POM absorbs virtually no water, while nylon shows significant moisture uptake

POM absorbs less than 0.3% water even at saturation, while nylon absorbs 2.5-9.5% depending on conditions. This means POM parts maintain consistent dimensions regardless of humidity.

Chemische weerstand

Nylon is resistant to oils, greases, fuels, and alkalis. POM offers excellent resistance to organic solvents, oils, and neutral chemicals but is attacked by strong acids.

Thermal Properties

Eigendom PA6 POM
Melting Point (°C) 220 165-175
HDT at 1.8 MPa (°C) 65 95-110
Continuous Use Temp (°C) 80-100 90-100
Thermal properties comparison
POM maintains stiffness better at elevated temperatures

Application Guide

Choose Nylon When:

  • Impact resistance and toughness are critical
  • Parts experience dynamic loading
  • Higher temperature resistance is needed (PA66)

Choose POM When:

  • Dimensional stability in varying humidity is critical
  • Low friction and wear resistance are priorities
  • Parts operate in wet environments
  • Precision mechanical components are needed

Onze mogelijkheden

Met meer dan 300 CNC machines, produceren we meer dan 10.000 stuks per dag met toleranties zo nauw als ±0,005mm. Wij accepteren MOQ vanaf 1 stuk, met levertijden variërend van 24 uur tot 15 dagen. We machine both nylon and POM for precision applications. Ontvang binnen 24 uur een offerte.

FAQ

When is Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics a good option?

Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics is a good option when fast iteration, complex geometry, low tooling cost, or low-volume production is more important than molded-part unit cost.

What should be checked before choosing Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics?

Controleer de onderdeelgrootte, materiaaleigenschappen, oppervlakteafwerking, maattolerantie, blootstelling aan hitte, belastingsrichting en of nabewerking nodig is.

How does Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics compare with CNC machining?

Met 3D-printen kunnen complexe vormen snel worden gemaakt, terwijl CNC-bewerking vaak sterker is voor precieze oppervlakken, nauwere toleranties en productiematerialen.

What affects the cost of Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics?

De kosten zijn afhankelijk van het materiaal, het bouwvolume, de printtijd, de laaghoogte, het verwijderen van de ondersteuning, de afwerking, de inspectie en het aantal onderdelen in de bouw.

Laten we een oplossing op maat maken

Dit veld is verplicht.
Dit veld is verplicht.
Dit veld is verplicht.
Dit veld is verplicht.
Dit veld is verplicht.

Gerelateerde lezen

Scroll naar boven