What Is POM Acetal Plastic?

POM (Polyoxymethylene), also known as acetal or Delrin, is a highly crystalline engineering thermoplastic. Its combination of high stiffness, low friction, and excellent dimensional stability makes it ideal for precision mechanical components.

Key Properties of POM

  • Tensile Strength: 60–70 MPa
  • Flexural Modulus: 2,500–2,800 MPa
  • Melting Point: 165–175°C
  • Coefficient of Friction: 0.2–0.35

CNC Machining Best Practices

Use sharp carbide tools, 150–250 m/min cutting speed for turning, and air blast or flood coolant.

Common Applications

Gears, sprockets, bearings, bushings, guide rails, food processing equipment, and medical device components.

Vamos criar a sua solução personalizada

Este campo é obrigatório.
Este campo é obrigatório.
Este campo é obrigatório.
Este campo é obrigatório.

Deixar um comentário

O seu endereço de email não será publicado. Campos obrigatórios marcados com *

Deslocar para o topo