Common Injection Molding Defects

Short Shots

Insufficient material fills the cavity. Solutions: Increase injection pressure, raise melt temperature, check for leaks.

Sink Marks

Visible depressions on thick sections. Solutions: Increase packing pressure, adjust cooling time, reduce wall thickness variation.

Flash

Excess material escapes the cavity. Solutions: Reduce injection pressure, repair worn molds, check clamp force.

Warpage

Uneven cooling causes distortion. Solutions: Uniform cooling, symmetric wall design, post-mold annealing.

Surface Streaks

Flow lines visible on surface. Solutions: Increase melt temperature, modify gate location, improve venting.

Vamos criar a sua solução personalizada

Este campo é obrigatório.
Este campo é obrigatório.
Este campo é obrigatório.
Este campo é obrigatório.

Deixar um comentário

O seu endereço de email não será publicado. Campos obrigatórios marcados com *

Deslocar para o topo