Nylon vs Policarbonato: Força, resistência ao calor e custo comparados

Nylon vs Polycarbonate comparison
Nylon and polycarbonate are both engineering plastics but excel in different areas

Nylon and polycarbonate are two of the most specified engineering thermoplastics. Both offer excellent mechanical properties, but their unique characteristics—impact resistance for polycarbonate, wear resistance for nylon—make each better suited for specific applications.

Mechanical Properties Compared

Imóveis Nylon (PA6) Policarbonato (PC)
Resistência à tração (MPa) 70-85 55-75
Módulo de flexão (GPa) 2.5-3.0 2.2-2.4
Notched Izod Impact (kJ/m²) 5-15 60-80
Densidade (g/cm³) 1.14 1.20
Impact resistance comparison
Polycarbonate offers dramatically higher impact resistance than nylon

Impact Resistance: Polycarbonate’s Signature Strength

Polycarbonate is legendary for its impact resistance—it’s used in bulletproof glass and safety goggles. With notched Izod impact values of 60-80 kJ/m², PC is virtually unbreakable under normal use.

Thermal and Optical Properties

Optical clarity comparison
Polycarbonate’s optical clarity is a key differentiator

Polycarbonate is naturally transparent with light transmission of 88-90%. Nylon is naturally translucent to opaque.

Resistência química

Nylon holds a distinct advantage here. Polycarbonate has poor chemical resistance—it’s attacked by hydrocarbons, ketones, and many cleaners. Nylon offers excellent resistance to oils, greases, fuels, and many organic solvents.

Moisture and Environmental Resistance

Moisture and weathering comparison
Polycarbonate resists moisture but is susceptible to UV degradation

Polycarbonate absorbs negligible moisture (0.15-0.35%). Nylon’s moisture absorption (2.5-3.0%) can cause dimensional changes. However, PC is susceptible to UV degradation.

Application Guide

Choose Nylon When:

  • Chemical resistance to oils and fuels is needed
  • Wear resistance matters
  • Parts must survive dynamic loading

Choose Polycarbonate When:

  • Optical clarity is required
  • Exceptional impact resistance is critical
  • Dimensional stability under varying humidity is needed

As nossas capacidades

Com mais de 300 máquinas CNC, produzimos mais de 10.000 peças por dia com tolerâncias tão apertadas como ±0,005mm. Aceitamos MOQ a partir de 1 peça, com prazos de entrega que variam entre 24 horas a 15 dias. We machine both nylon and polycarbonate. Obter um orçamento no prazo de 24 horas.

FAQ

How do you know whether Nylon vs Polycarbonate: Strength, Heat Resistance, and Cost Compared fits a part?

Nylon vs Polycarbonate: Strength, Heat Resistance, and Cost Compared fits a part when its load capacity, temperature range, moisture exposure, wear behavior, and processing method match the real service conditions.

What properties should be checked for Nylon vs Polycarbonate: Strength, Heat Resistance, and Cost Compared?

Verificar a resistência, a rigidez, a resistência ao impacto, a resistência ao calor, a absorção de humidade, a estabilidade dimensional, a fricção, o desgaste e a compatibilidade química.

What is the biggest selection risk for Nylon vs Polycarbonate: Strength, Heat Resistance, and Cost Compared?

O maior risco é escolher a partir de um valor da folha de dados sem considerar o ambiente real, o método de processamento, a geometria da peça e a utilização a longo prazo.

When should Nylon vs Polycarbonate: Strength, Heat Resistance, and Cost Compared be tested before production?

Recomenda-se a realização de ensaios quando a peça é sujeita a carga, calor, produtos químicos, humidade, tolerâncias apertadas, requisitos regulamentares ou um novo ambiente de funcionamento.

Vamos criar a sua solução personalizada

Este campo é obrigatório.
Este campo é obrigatório.
Este campo é obrigatório.
Este campo é obrigatório.
Este campo é obrigatório.

Related Reading

Deslocar para o topo