PC/ABS Flame Retardant (V-0) Technical Data (Estimated Typical Values)
| Imóveis | Valor | Norma de ensaio |
|---|---|---|
| Resistência à tração | 45 – 55 MPa | ISO 527 |
| Módulo de flexão | 2,300 – 2,600 MPa | ISO 178 |
| Resistência ao impacto entalhado | 25 – 35 kJ/m² | ISO 180 |
| HDT @1,8 MPa | 95 - 105 °C | ISO 75 |
| Melt Flow Rate (240°C/5kg) | 10 – 20 g/10min | ISO 1133 |
| Flame Rating | UL94 V-0 (na espessura especificada) | UL 94 |
PC/ABS Series Performance Comparison Table (Estimated Typical Values)
| Imóveis | PC/ABS GP | PC/ABS HF | PC/ABS FR (V-0) | PC/ABS GF20 |
|---|---|---|---|---|
| Resistência à tração | 50 – 60 MPa | 48 – 55 MPa | 45 – 55 MPa | 70 - 85 MPa |
| Módulo de flexão | 2,200 – 2,500 MPa | 2,000 – 2,300 MPa | 2,300 – 2,600 MPa | 4.500 - 5.500 MPa |
| Resistência ao impacto entalhado | 45 – 55 kJ/m² | 40 – 50 kJ/m² | 25 – 35 kJ/m² | 15 – 25 kJ/m² |
| HDT @1,8 MPa | 105 - 115 °C | 100 - 110 °C | 95 - 105 °C | 115 - 125 °C |
| Melt Flow Rate (240°C/5kg) | 15 – 25 g/10min | 30 – 50 g/10min | 10 – 20 g/10min | 10 – 18 g/10min |
| Flame Rating (UL94) | HB | HB | V-0 | HB |
| Perfil-chave | Balanced all-rounder | Easy flow for complex parts | Safety compliance | High stiffness |
PC/ABS Flame Retardant (V-0) Key Advantages
✅ Reliable Fire Safety Rating: UL94 V-0 certification provides critical fire safety protection for electrical/electronic products, meeting international safety regulations.
✅ Good Mechanical Property Balance: Maintains good impact strength and rigidity while achieving flame retardancy, ensuring enclosures resist physical damage.
✅ Stable Processing & Electrical Properties: Offers a predictable processing window and good electrical insulation, making it ideal for E&E applications.
Aplicações do sector:

Explore the PC/ABS Alloy Series in Detail
Clique nas hiperligações abaixo para ver os dados técnicos completos, as principais vantagens e os detalhes de aplicação para cada tipo específico.
| Grau | Melhor para | Visão geral | Detalhes completos |
|---|---|---|---|
| PC/ABS General Purpose | Applications demanding an optimal balance of impact strength, heat resistance, and processability. | The benchmark alloy grade, offering the classic combination of PC’s toughness and ABS’s ease of processing for a wide range of structural parts. | View PC/ABS GP Full Data Sheet → |
| PC/ABS High Flow | Thin-walled, complex geometry parts requiring excellent filling and surface finish. | Engineered with enhanced melt flow, facilitating the molding of intricate designs and reducing cycle times without sacrificing key mechanical properties. | View PC/ABS HF Full Data Sheet → |
| PC/ABS Flame Retardant (V-0) | Electronic enclosures and components with mandatory fire safety requirements. | A UL94 V-0 rated grade that combines inherent flame retardancy with good impact strength and thermal stability for safe electronic applications. | View PC/ABS FR Full Data Sheet → |
| PC/ABS Reinforced (GF20) | Structural components requiring higher stiffness, dimensional stability, and heat deflection temperature. | Glass fiber reinforced grade that significantly boosts rigidity and creep resistance while maintaining good overall toughness. | View PC/ABS GF20 Full Data Sheet → |
Powering Innovation Across Industries (PC/ABS Series)
| Indústria | Principais aplicações |
|---|---|
| Automóvel | Interior trim (instrument panels, pillar covers, glove box doors), exterior components (wheel covers, mirror housings), and connectors requiring heat resistance & aesthetics. Explorar soluções para o sector automóvel → |
| Eletricidade e eletrónica | Durable housings for laptops, monitors, printers, power tools, and consumer electronics that demand a balance of impact strength, heat resistance, and good surface finish. Descubra as soluções E&E → |
| Consumer Appliances & Tools | Vacuum cleaner bodies, blender and coffee maker housings, power tool grips, and other appliance components needing structural integrity and a premium feel. Explorar aplicações de consumo → |
| Industrial & Business Equipment | Robust casings for printers, copiers, industrial control panels, and handheld scanners where durability and dimensional stability are critical. Ver Usos industriais → |
| Medical & Specialty Devices | Housings for non-implantable medical devices, diagnostic equipment, and specialty enclosures requiring a combination of cleanliness, durability, and compliance. Informe-se sobre utilizações especiais → ou Contact for Special Uses → |
How to Choose the Right PC/ABS Grade?
Em termos simples:
For most structural applications requiring the best all-around balance of toughness, heat resistance, and cost-effectiveness, choose PC/ABS General Purpose.
For complex, thin-walled designs such as intricate housings or large panels, select PC/ABS High Flow to ensure complete filling and a superior surface.
For safety-critical electrical/electronic parts that must meet flame retardancy standards, specify PC/ABS Flame Retardant (V-0).
For applications where maximum stiffness, minimal deflection, and higher thermal performance are critical, opt for PC/ABS Reinforced (GF20).
Não tem a certeza de qual é o ideal para a sua peça? Descreva a sua aplicação aos nossos engenheiros para obter uma recomendação personalizada.
Porquê escolher-nos?


PC/ABS Flame Retardant (V-0) FAQ
Q1: Do flame retardants affect other material properties?
Yes, adding flame retardants involves a typical performance trade-off. It usually reduces impact toughness and may slightly lower HDT. It can also affect weatherability (e.g., UV stability) and colorability. Selecting optimized, dedicated FR grades minimizes these effects.
Q2: What are the main applications for Flame Retardant PC/ABS?
Applications are concentrated in fields with mandatory or high fire safety standards, including: TV/display/printer housings, power adapter/charger casings, laptop internal frames, smart home device housings, e automotive electronics.
Q3: What are special processing considerations for FR grades?
Beyond standard drying, strict melt temperature control is crucial. Some FR agents may degrade at excessively high temperatures, harming properties or corroding screws/molds. Strictly adhere to the recommended processing temperature range and avoid long residence time in the barrel. Ensure good workshop ventilation.