PA6 GF33 Technical Specifications (Estimated)
| 財產 | 價值 | 測試標準 |
|---|---|---|
| 玻璃纖維含量 | 33% (±2%) | ISO 1172 |
| 拉伸強度 | 135 – 185 MPa | ISO 527 |
| 彎曲模量 | 6,500 – 9,500 MPa | ISO 178 |
| 衝擊強度 (缺口伊佐德) | 11 – 15 kJ/m² | ISO 180 |
| 熱變形溫度 (HDT) | 180 – 200 °C @ 1.8 MPa | ISO 75 |
| 熔點 | 215 - 230 °C | ISO 3146 |
| 吸濕性(平衡,23°C/501TPT3T RH) | ~1.7% | ISO 62 |
PA6 Series Material Performance Comparison Table
| 財產 | PA6 GF15 | PA6 GF30 | PA6 GF33 | PA6 GF40 | PA6 GF50 | PA6 GF60 |
|---|---|---|---|---|---|---|
| 玻璃纖維含量 | 15% | 30% | 33% | 40% | 50% | 60% |
| 密度 (g/cm³) | 1.21 | 1.38 | ~1.42 | 1.46 | 1.56 | 1.67 |
| 拉伸強度 (MPa) | 118 | 165 | ~175 | 185 | 200 | 220 |
| 斷裂伸長率 (%) | 3.3 | 3.0 | ~2.9 | 2.8 | 2.0 | 2.0 |
| 缺口衝擊強度 (kJ/m²) | 10 | 12 | ~12.5 | 13 | 14 | 14 |
| 熱變形溫度 (℃,1.8MPa) | 160 | 175 | ~195 | 215 | 216 | 220 |
主要優勢:
Optimized Balance of Strength and Toughness
PA6 GF33 is engineered to offer a superior mechanical profile, delivering higher strength and rigidity than standard PA6 GF30, while maintaining better impact resistance and ductility compared to PA6 GF40. This makes it an ideal “upgraded” choice when GF30 is marginally insufficient.
增強的高溫能力
With a Heat Deflection Temperature (HDT) typically elevated beyond that of GF30, PA6 GF33 provides improved performance and dimensional stability in demanding thermal environments, offering a safety margin for applications near the upper limit of GF30.
Superior Dimensional Stability and Precision
The increased fiber content further reduces moisture absorption and thermal expansion compared to GF30, resulting in enhanced dimensional stability for parts that require tight tolerances under varying environmental conditions.
Retained Processability
While requiring more robust processing parameters than GF30, PA6 GF33 generally maintains better melt flow and is less demanding on equipment than higher-load grades like GF40 or GF50, facilitating more reliable production.
產業應用:

PA6GF33 is commonly used in automotive components, interior parts, and other applications that require a good surface finish and fundamental rigidity.
推動跨產業創新
| 產業 | 主要應用 |
|---|---|
| 汽車 | 引擎蓋、進氣歧管、結構支架、感測器外殼、連接器。. 探索汽車應用 → |
| 電子電機 | 斷路器、開關、連接器外殼、絕緣元件。. 發現 E&E 解決方案 → |
| 工業設備 | 齒輪、軸承、機器外殼、滾筒、機械組件。. 請參閱工業用途 → |

如何選擇?
簡單來說
適用於 良好的韌性 或 成本效益, 請考慮 PA6 GF15.
適用於 整體表現均衡, 選擇 PA6 GF30.
適用於 更高的硬度、強度和耐熱性, 而對成本不太敏感時,可考慮 PA6 GF40/50/60. .一般而言,較高的玻璃纖維含量可改善這些特性。.