Nylon vs. POM (Acetal/Delrin): Die Wahl zwischen zwei technischen Kunststoffen

Nylon vs POM Acetal comparison
Nylon and POM are both engineering plastics but serve different purposes

Nylon and POM (polyoxymethylene, also known as acetal or Delrin) are two of the most important engineering plastics. Both are widely used for precision mechanical components, but their distinctly different properties make each better suited for specific applications.

Mechanical Properties Head-to-Head

Eigentum PA6 (Nylon) POM (Acetal)
Zugfestigkeit (MPa) 70-85 60-70
Biegemodul (GPa) 2.5-3.0 2.6-2.9
Bruchdehnung (%) 50-150 25-75
Dichte (g/cm³) 1.14 1.41
Mechanical properties radar chart
Nylon leads in strength and toughness; POM excels in dimensional stability

Wear and Friction: A Critical Difference

POM’s key advantage over nylon is its excellent wear resistance and low coefficient of friction (0.2-0.35 against steel), making it preferred for gears, bearings, and sliding components.

Feuchtigkeitsabsorption

Moisture absorption comparison
POM absorbs virtually no water, while nylon shows significant moisture uptake

POM absorbs less than 0.3% water even at saturation, while nylon absorbs 2.5-9.5% depending on conditions. This means POM parts maintain consistent dimensions regardless of humidity.

Chemische Beständigkeit

Nylon is resistant to oils, greases, fuels, and alkalis. POM offers excellent resistance to organic solvents, oils, and neutral chemicals but is attacked by strong acids.

Thermal Properties

Eigentum PA6 POM
Melting Point (°C) 220 165-175
HDT at 1.8 MPa (°C) 65 95-110
Continuous Use Temp (°C) 80-100 90-100
Thermal properties comparison
POM maintains stiffness better at elevated temperatures

Application Guide

Choose Nylon When:

  • Impact resistance and toughness are critical
  • Parts experience dynamic loading
  • Higher temperature resistance is needed (PA66)

Choose POM When:

  • Dimensional stability in varying humidity is critical
  • Low friction and wear resistance are priorities
  • Parts operate in wet environments
  • Precision mechanical components are needed

Unser Leistungsvermögen

Mit über 300 CNC-Maschinen, produzieren wir mehr als 10.000 Stück täglich mit so engen Toleranzen wie ±0,005 mm. Wir akzeptieren MOQ ab 1 Stück, mit Lieferzeiten von 24 Stunden bis 15 Tage. We machine both nylon and POM for precision applications. Erhalten Sie innerhalb von 24 Stunden ein Angebot.

FAQ

When is Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics a good option?

Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics is a good option when fast iteration, complex geometry, low tooling cost, or low-volume production is more important than molded-part unit cost.

What should be checked before choosing Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics?

Prüfen Sie die Größe des Teils, die Materialeigenschaften, die Oberflächenbeschaffenheit, die Maßtoleranz, die Wärmeeinwirkung, die Belastungsrichtung und ob eine Nachbearbeitung erforderlich ist.

How does Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics compare with CNC machining?

Mit dem 3D-Druck lassen sich komplexe Formen schnell erstellen, während die CNC-Bearbeitung für präzise Oberflächen, engere Toleranzen und serienreife Materialien oft besser geeignet ist.

What affects the cost of Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics?

Die Kosten hängen vom Material, dem Bauvolumen, der Druckzeit, der Schichthöhe, der Entfernung von Stützen, der Endbearbeitung, der Prüfung und der Anzahl der Teile im Bau ab.

Entwerfen wir Ihre individuelle Lösung

Dieses Feld ist erforderlich.
Dieses Feld ist erforderlich.
Dieses Feld ist erforderlich.
Dieses Feld ist erforderlich.
Dieses Feld ist erforderlich.

Weiterführende Lektüre

Nach oben blättern