Nylon isn’t one material—it’s a family of polyamides with distinctly different properties. From the workhorse PA6 to the premium PA12, understanding the full range of nylon grades helps you select the optimal material for your application.
The Nylon Family Overview
| Grau | Tipo | Ponto de fusão | Moisture (50% RH) | Key Characteristic |
|---|---|---|---|---|
| PA6 | Aliphatic | 220°C | 2.7% | Toughness, processability |
| PA66 | Aliphatic | 260°C | 2.5% | Strength, heat resistance |
| PA11 | Bio-based | 185°C | 0.8% | Flexibility, low moisture |
| PA12 | Aliphatic | 178°C | 0.7% | Lowest moisture absorption |
| PA46 | Aliphatic | 295°C | 3.5% | Highest heat resistance |

PA6: The Versatile Workhorse
PA6 is the most widely used nylon grade, representing approximately 60% of nylon consumption. It offers an excellent balance of strength, toughness, and processability.
Propriedades principais
- Tensile strength: 70-85 MPa
- Excellent impact resistance
- Good surface finish and colorability
- Wider processing window than PA66
PA66: The High-Performance Standard

PA66 offers approximately 10-15% higher strength and stiffness than PA6, with superior heat resistance. It’s the preferred choice for demanding applications.
PA11 and PA12: The Specialty Nylons
PA11 and PA12 are distinguished by their exceptionally low moisture absorption—less than 1% even at saturation. This gives them outstanding dimensional stability.

PA46: The High-Temperature Specialist
PA46 (Stanyl) offers the highest heat resistance of any aliphatic nylon, with a melting point of 295°C.
Selection Guide
| Requisito | Recommended Grade |
|---|---|
| General purpose, cost-sensitive | PA6 |
| High temperature (>120°C) | PA66, PA46 |
| Wet/humid environment | PA12, PA11 |
| Maximum stiffness | PA66-GF30/50 |
As nossas capacidades
Com mais de 300 máquinas CNC, produzimos mais de 10.000 peças por dia com tolerâncias tão apertadas como ±0,005mm. Aceitamos MOQ a partir de 1 peça, com prazos de entrega que variam entre 24 horas a 15 dias. We supply all major nylon grades. Obter um orçamento no prazo de 24 horas.
FAQ
How do you know whether The Complete Guide to Nylon Grades: PA6, PA66, PA11, PA12 and More fits a part?
The Complete Guide to Nylon Grades: PA6, PA66, PA11, PA12 and More fits a part when its load capacity, temperature range, moisture exposure, wear behavior, and processing method match the real service conditions.
What properties should be checked for The Complete Guide to Nylon Grades: PA6, PA66, PA11, PA12 and More?
Verificar a resistência, a rigidez, a resistência ao impacto, a resistência ao calor, a absorção de humidade, a estabilidade dimensional, a fricção, o desgaste e a compatibilidade química.
What is the biggest selection risk for The Complete Guide to Nylon Grades: PA6, PA66, PA11, PA12 and More?
O maior risco é escolher a partir de um valor da folha de dados sem considerar o ambiente real, o método de processamento, a geometria da peça e a utilização a longo prazo.
When should The Complete Guide to Nylon Grades: PA6, PA66, PA11, PA12 and More be tested before production?
Recomenda-se a realização de ensaios quando a peça é sujeita a carga, calor, produtos químicos, humidade, tolerâncias apertadas, requisitos regulamentares ou um novo ambiente de funcionamento.