Nylon and POM (polyoxymethylene, also known as acetal or Delrin) are two of the most important engineering plastics. Both are widely used for precision mechanical components, but their distinctly different properties make each better suited for specific applications.
Mechanical Properties Head-to-Head
| Недвижимость | PA6 (Nylon) | POM (ацеталь) |
|---|---|---|
| Прочность на разрыв (МПа) | 70-85 | 60-70 |
| Модуль упругости (ГПа) | 2.5-3.0 | 2.6-2.9 |
| Удлинение при разрыве (%) | 50-150 | 25-75 |
| Плотность (г/см³) | 1.14 | 1.41 |

Wear and Friction: A Critical Difference
POM’s key advantage over nylon is its excellent wear resistance and low coefficient of friction (0.2-0.35 against steel), making it preferred for gears, bearings, and sliding components.
Поглощение влаги

POM absorbs less than 0.3% water even at saturation, while nylon absorbs 2.5-9.5% depending on conditions. This means POM parts maintain consistent dimensions regardless of humidity.
Химическая стойкость
Nylon is resistant to oils, greases, fuels, and alkalis. POM offers excellent resistance to organic solvents, oils, and neutral chemicals but is attacked by strong acids.
Thermal Properties
| Недвижимость | PA6 | POM |
|---|---|---|
| Melting Point (°C) | 220 | 165-175 |
| HDT at 1.8 MPa (°C) | 65 | 95-110 |
| Continuous Use Temp (°C) | 80-100 | 90-100 |

Application Guide
Choose Nylon When:
- Impact resistance and toughness are critical
- Parts experience dynamic loading
- Higher temperature resistance is needed (PA66)
Choose POM When:
- Dimensional stability in varying humidity is critical
- Low friction and wear resistance are priorities
- Parts operate in wet environments
- Precision mechanical components are needed
Наши возможности
С более чем 300 станков с ЧПУ, Мы производим более 10 000 штук в день с такими жесткими допусками, как ±0,005 мм. Мы принимаем MOQ от 1 шт., Сроки доставки варьируются от От 24 часов до 15 дней. We machine both nylon and POM for precision applications. Получите предложение в течение 24 часов.
ЧАСТО ЗАДАВАЕМЫЕ ВОПРОСЫ
When is Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics a good option?
Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics is a good option when fast iteration, complex geometry, low tooling cost, or low-volume production is more important than molded-part unit cost.
What should be checked before choosing Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics?
Проверьте размер детали, свойства материала, качество обработки поверхности, допуск на размеры, тепловое воздействие, направление нагрузки и необходимость последующей обработки.
How does Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics compare with CNC machining?
3D-печать позволяет быстро создавать сложные формы, в то время как обработка на станках с ЧПУ часто более эффективна для получения точных поверхностей, более жестких допусков и материалов производственного класса.
What affects the cost of Nylon vs POM (Acetal/Delrin): Choosing Between Two Engineering Plastics?
Стоимость зависит от материала, объема сборки, времени печати, высоты слоя, удаления поддержки, финишной обработки, контроля и количества деталей в сборке.