吸濕性

ConditionPA6PA66
50% RH2.7%2.5%
Saturation8-10%6-8%

Effects

  • Reduces strength and stiffness
  • Increases impact resistance
  • Changes dimensions

Drying Guidelines

  • PA6: 80°C for 4-6 hours
  • PA66: 100°C for 4-6 hours

常見問題

How do you know whether Moisture Effects on Nylon — Storage & Drying Guide fits a part?

Moisture Effects on Nylon — Storage & Drying Guide fits a part when its load capacity, temperature range, moisture exposure, wear behavior, and processing method match the real service conditions.

What properties should be checked for Moisture Effects on Nylon — Storage & Drying Guide?

Check strength, stiffness, impact resistance, heat resistance, moisture absorption, dimensional stability, friction, wear, and chemical compatibility.

What is the biggest selection risk for Moisture Effects on Nylon — Storage & Drying Guide?

The biggest risk is choosing from a datasheet value without considering actual environment, processing method, part geometry, and long-term use.

When should Moisture Effects on Nylon — Storage & Drying Guide be tested before production?

Testing is recommended when the part faces load, heat, chemicals, moisture, tight tolerances, regulatory requirements, or a new operating environment.

讓我們為您量身打造解決方案

此欄位必須填寫。.
此欄位必須填寫。.
此欄位必須填寫。.
此欄位必須填寫。.

Moisture Effects on Nylon — Frequently Asked Questions

Why does nylon absorb moisture?

Nylon contains amide groups that form hydrogen bonds with water.

Where can I get properly dried nylon?

Nylonplastic supplies nylon vacuum-sealed with desiccant.