Moisture Effects on Nylon — Storage & Drying Guide

Moisture Effects on Nylon illustration 1
Moisture Effects on Nylon — Storage & Drying Guide
Moisture Effects on Nylon — Storage & Drying Guide

Moisture Absorption

Condition PA6 PA66
50% RH 2.7% 2.5%
Saturation 8-10% 6-8%

Effects

  • Reduces strength and stiffness
  • Increases impact resistance
  • Changes dimensions

Drying Guidelines

  • PA6: 80°C for 4-6 hours
  • PA66: 100°C for 4-6 hours

FAQ

How do you know whether Moisture Effects on Nylon — Storage & Drying Guide fits a part?

Moisture Effects on Nylon — Storage & Drying Guide fits a part when its load capacity, temperature range, moisture exposure, wear behavior, and processing method match the real service conditions.

What properties should be checked for Moisture Effects on Nylon — Storage & Drying Guide?

Check strength, stiffness, impact resistance, heat resistance, moisture absorption, dimensional stability, friction, wear, and chemical compatibility.

What is the biggest selection risk for Moisture Effects on Nylon — Storage & Drying Guide?

The biggest risk is choosing from a datasheet value without considering actual environment, processing method, part geometry, and long-term use.

When should Moisture Effects on Nylon — Storage & Drying Guide be tested before production?

Testing is recommended when the part faces load, heat, chemicals, moisture, tight tolerances, regulatory requirements, or a new operating environment.

Tell Us About Your Part

This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.

Related Reading

Scroll to Top