尼龍與 POM (乙縮醛):工程塑料比較指南

Nylon vs POM acetal engineering plastics
Nylon vs POM comparison — Nylon Plastic

Head-to-head comparison of nylon and POM (acetal/delrin) for engineering applications — mechanical, thermal, chemical, wear, and processing differences.

Nylon vs. POM: Two Giants of Engineering Plastics

Nylon (polyamide) and POM (polyoxymethylene, also called acetal or Delrin) are the two most-used engineering thermoplastics for mechanical components. Both offer excellent wear resistance, low friction, and good dimensional stability — but their different molecular structures create distinct performance trade-offs that matter enormously in precision applications.

Choosing between nylon and POM is not trivial. A bearing that lasts 50,000 cycles in POM may fail in 8,000 cycles in nylon under the same load. Conversely, a gear housing exposed to automotive fluids will crack with POM but survive with PA66. This guide provides the data-driven comparison engineers need to make the right choice.

Mechanical Properties Comparison

Tensile and Flexural Properties:

財產 PA6 PA66 POM (Homopolymer) POM (Copolymer)
拉伸強度 (MPa) 80 82 70 62
Tensile Modulus (GPa) 2.8 3.0 2.8 2.5
Flexural Strength (MPa) 100 110 98 90
彎曲模量 (GPa) 2.6 2.8 2.6 2.3
斷裂伸長率 (%) 150 60 40 35
缺口 Izod (J/m) 55 45 75 65
Creep Modulus (1000h, 20 MPa) 1.2 GPa 1.4 GPa 2.3 GPa 2.0 GPa

Key Insight: Creep Resistance — POM has significantly better creep resistance than nylon. Under sustained loading, POM retains more of its stiffness over time. For components under constant load (spring clips, retaining rings, fastener bushings), POM’s superior creep resistance often makes it the better choice despite similar initial strength.

耐衝擊性 — Nylon has higher unnotched impact resistance. But POM often outperforms nylon in notched impact tests because POM’s ductile failure mode absorbs more energy at the crack tip. For parts with stress concentrations (keyways, holes, threads), POM’s toughness at sharp notches is an advantage.

Fatigue Resistance — Nylon has superior fatigue resistance for repeated loading. In cyclic loading tests, nylon components survive 3-5× more cycles before failure than equivalent POM parts. Critical for components like conveyor belt guides, pump impellers, and hinge mechanisms.

Thermal and Environmental Performance

Thermal Properties:

財產 PA6 PA66 POM
Melting Point (°C) 225 265 175
Continuous Service Temp (°C) 100-115 130-150 90-100
HDT @ 1.82 MPa (°C) 65 90 95
HDT @ 0.45 MPa (°C) 170 250 160
熱膨脹 (×10-⁵/°C) 8-9 8-9 11-12

POM’s thermal weakness — The 175°C melting point of POM is its thermal limitation. At temperatures above 100°C, POM loses mechanical strength rapidly. PA66-GF30 (HDT 250°C) operates at temperatures where POM would melt.

Moisture Absorption Comparison:

財產 PA6 PA66 POM
Saturation Moisture (%) 9.5% 8.5% 0.8%
Dimensional Change (saturation) 1.5-2.0% 1.3-1.8% 0.2%

POM wins decisively on moisture — At 0.8% maximum moisture absorption, POM is essentially dimensionally stable in humid environments. Nylon’s 8-9% absorption causes measurable swelling and property changes. For underwater or outdoor exposed applications without encapsulation, POM is often the only viable choice.

Chemical Resistance: Where Each Material Excels

Chemical Resistance Comparison:

Chemical Nylon (PA66) POM
Gasoline/Fuels 極佳 極佳
Motor Oil 極佳 極佳
Brake Fluid 良好 Poor (swells)
Alcohol 極佳 良好
Ketones (Acetone) 良好 Poor (dissolves)
Weak Acids Fair 良好
Strong Acids Poor Poor
Esters/Plasticizers 極佳 Poor
Hot Water (>60°C) Poor 良好
Steam Poor Poor

Critical Decision Points: – Brake fluid or glycol coolants: POM swells and cracks — use PA66 or PA12 – Hot water (>60°C): Nylon hydrolyzes — use POM or PVDF – Plasticizer migration (flexible cables, wire insulation): POM absorbs plasticizers — use PA12 – Automotive under-hood: PA66-GF30 for its heat resistance (180°C+) and fluid resistance – Consumer appliances: POM for its dimensional stability and surface finish

Wear and Friction Performance

Both materials offer low friction and good wear resistance — but with important differences:

財產 PA6 PA66 POM
Coefficient of Friction (vs. steel, dry) 0.25-0.40 0.20-0.35 0.15-0.35
PV Limit (MPa·m/min) 80-120 90-130 80-100
Wear Factor (vs. steel, dry) 15-40 10-30 1-3
Machinability 良好 極佳 極佳

The critical difference: wear factor — POM’s wear factor (1-3) is 10-20× lower than nylon’s (10-40). This means POM parts generate less heat and wear more slowly in sliding contact. For high-PV applications (bearings, wear strips, sliding inserts), POM is the superior choice.

Self-lubricating versions: – POM + PTFE: Wear factor drops to 0.5-1.0 — excellent for boundary lubrication – PA6/66 + PTFE or silicone: Significantly reduces friction, but PTFE can migrate to surface and affect bonding – Carbon fiber reinforced: Improves wear resistance in both materials, especially at elevated temperatures

Surface Speed Consideration: At surface speeds above 1 m/s in dry sliding, both materials generate enough heat to cause thermal softening. For high-speed applications, consider internally lubricated grades or oil-impregnated sintered bronze backings.

Injection molding nylon processing parameters
Nylon injection molding guide — Nylon Plastic

How to Choose: Decision Framework

Choose Nylon (PA66-GF30) when: – Operating temperature exceeds 100°C – Repeated impact or cyclic loading is expected – Exposure to brake fluid, coolants, or plasticizers – You need higher fatigue life in dynamic loading – Cost is the primary driver (PA66 is generally less expensive than POM)

Choose POM when: – Dimensional stability in humid environments is critical – Low friction and low wear factor are priorities (sliding/rotating contact) – Parts will be exposed to hot water or steam – Acetone, esters, or plasticizers are present – You need excellent surface finish and tight tolerances

Hybrid Solution — Metal Replacement: For many metal-replacement applications, the choice is not between nylon and POM, but between them and aluminum. Nylon-GF and POM are both excellent metal substitutes for housings, brackets, and structural components, offering 70-85% weight reduction vs. aluminum with adequate strength. For these applications, PA66-GF30 is the default choice due to its superior thermal and fluid resistance.

Related Products

Nylon Rods & Sheets

Semi-finished shapes for CNC machining

Nylon Granules (PA6/PA66/PA12)

Engineering-grade nylon raw materials for injection molding

常見問題

尼龍與 POM (乙縮醛):工程塑料比較指南
尼龍與 POM (乙縮醛):工程塑料比較指南
When is Nylon vs. POM (Acetal): Engineering Plastics Comparison Guide a good option?

Nylon vs. POM (Acetal): Engineering Plastics Comparison Guide is a good option when fast iteration, complex geometry, low tooling cost, or low-volume production is more important than molded-part unit cost.

What should be checked before choosing Nylon vs. POM (Acetal): Engineering Plastics Comparison Guide?

檢查零件尺寸、材料特性、表面光潔度、尺寸公差、受熱情況、負載方向,以及是否需要後加工。.

How does Nylon vs. POM (Acetal): Engineering Plastics Comparison Guide compare with CNC machining?

3D 列印可以快速製造複雜的形狀,而 CNC 加工通常在精密表面、更小的公差和生產級材料方面更強。.

What affects the cost of Nylon vs. POM (Acetal): Engineering Plastics Comparison Guide?

成本取決於材料、建置量、列印時間、層高、支撐移除、精加工、檢查以及建置中的零件數量。.

讓我們為您量身打造解決方案

此欄位必須填寫。.
此欄位必須填寫。.
此欄位必須填寫。.
此欄位必須填寫。.
此欄位必須填寫。.
滾動到頂端