PA66 CF10 is an engineering thermoplastic composite based on nylon 66 (PA66) reinforced with 10% carbon fibers. This grade bridges the gap between standard PA66 and advanced composites, delivering a crucial combination of enhanced heat resistance, superior stiffness, exceptional dimensional stability, and inherent static dissipation.

Why Partner With Us for PA66 CF10?
✅ Superior High-Temperature Performance: We deliver a material that excels where heat is a factor, providing greater rigidity and reliability at elevated temperatures compared to standard PA66.
✅ Precision & Stability Guaranteed: Our PA66 CF10 offers extremely low moisture absorption and thermal expansion, ensuring your parts maintain precise tolerances in challenging environments.
✅ Expert Processing Partnership: We provide dedicated technical support to navigate the processing of carbon fiber-reinforced PA66, helping you achieve optimal part quality and performance.
✅ Your Gateway to Advanced Materials: We are your strategic partner in innovation, helping you leverage PA66 CF10 to achieve weight reduction, thermal management, and functional integration in applications demanding more than standard plastics.

分類: , Brand:

萬翰詳情 01

PA66 CF10 Technical Data (Estimated Typical Values)

財產 價值 測試標準
碳纖維含量 10% ISO 1172
拉伸強度 160 - 180 MPa ISO 527
彎曲模量 11,000 - 13,000 MPa ISO 178
缺口衝擊強度 8 - 11 kJ/m² ISO 180
HDT @1.8 MPa 250 - 260 °C ISO 75
體積電阻率 10^3 - 10^5 Ω-cm IEC 60093

PA66 CF 系列技術資料表(估算典型值)

財產 測試標準 PA66 CF10 PA66 CF20 PA66 CF30 PA66 CF40 PA66 CF50
碳纖維含量 ISO 1172 10% 20% 30% 40% 50%
拉伸強度 ISO 527 160 - 180 MPa 200 - 230 MPa 240 - 270 MPa 260 - 290 MPa 280 - 320 MPa
彎曲模量 ISO 178 11,000 - 13,000 MPa 16,000 - 19,000 MPa 21,000 - 24,000 MPa 25,000 - 28,000 MPa 29,000 - 33,000 MPa
缺口衝擊強度 ISO 180 8 - 11 kJ/m² 9 - 12 kJ/m² 10 - 13 kJ/m² 11 - 14 kJ/m² 12 - 15 kJ/m²
HDT @1.8 MPa ISO 75 250 - 260 °C 255 - 265 °C 260 - 270 °C 265 - 275 °C 270 - 280 °C
體積電阻率 IEC 60093 10^3 - 10^5 Ω-cm 10^2 - 10^4 Ω-cm 10^1 - 10^3 Ω-cm 10^0 - 10^2 Ω-cm 10^-1 - 10^1 Ω-cm

PA66 CF10 Key Advantages

Cost-Effective Performance Leap: Provides a superior performance and thermal advantage over standard PA66 at an accessible price point, making it the ideal entry into high-temperature capable carbon fiber composites.
✅ High-Temperature Rigidity & Stability: Delivers exceptional stiffness and maintains dimensional precision under elevated temperatures, perfect for under-the-hood automotive and hot-running mechanical parts.
✅ Inherent Functional Conductivity: Offers built-in electrostatic dissipation (ESD) and improved thermal conductivity, critical for protecting sensitive electronics in demanding thermal environments.

產業應用:

注塑成型在汽車工業中的重要作用

詳細探索 PA66 碳纖維系列

按一下下列連結,即可檢視各特定等級的全面技術資料、主要優勢及應用細節。.

等級 最適合 概述 詳細資訊
PA66 CF10 在預算有限的情況下,需要高硬度和靜電防護的耐高溫零件。. 最容易取得的高溫 CF 等級,提供比標準 PA66 更強的耐熱性、剛性和 ESD 保護。. 檢視 PA66 CF10 完整規格表 → 筆記型電腦
PA66 CF20 在熱量、強度和重量都很重要的情況下,需要更換金屬。. 適用於高溫環境的均衡表現,在強度重量比和功能導電性方面表現優異。. 檢視 PA66 CF20 完整規格表 → 筆記型電腦
PA66 CF30 承受高熱和機械應力的結構組件。. 高溫結構完整性的基準,提供近乎金屬的剛性和出色的抗疲勞性。. 檢視 PA66 CF30 完整規格表 → 筆記型電腦
PA66 CF40 對撓度要求極高的超硬、高熱應用。. 在極端熱和機械負載下,可達到最大剛性和尺寸穩定性。. 檢視 PA66 CF40 完整規格表 → 筆記型電腦
PA66 CF50 關鍵任務應用在熱和機械性能的極限。. 頂尖等級,在最嚴峻的高溫環境中提供最高的比強度和剛度。. 檢視 PA66 CF50 完整規格表 → 筆記型電腦

推動跨產業創新

產業 主要應用
汽車 引擎蓋、進氣歧管、結構支架、感測器外殼、連接器。.
探索汽車應用 →
電子電機 斷路器、開關、連接器外殼、絕緣元件。.
發現 E&E 解決方案 →
工業設備 齒輪、軸承、機器外殼、滾筒、機械組件。.
請參閱工業用途 →
PA 塑膠的各種應用情境
PA 塑膠的各種應用情境

如何選擇合適的 PA66 CF 等級?

簡單來說

  • 以符合成本效益的方式升級為耐高溫的碳纖維複合材料 剛性、耐熱性和 ESD 都有顯著改善,請考慮 PA66 CF10.

  • 達到高強度、熱變形溫度和輕量化設計的最佳平衡 在高要求的金屬替換應用中,選擇 PA66 CF30. .它是大多數高溫結構用途的性能基準。.

  • 達到極致的高溫剛性、強度和尺寸穩定性 如果在極端條件下性能非常重要,請考慮 PA66 CF50.

為什麼選擇我們?

萬翰詳情 03

萬翰詳情 04

常見問題部分:

Q1: 與標準 PA66 相比,PA66 CF10 的主要優勢是什麼?
PA66 CF10 以 10% 碳纖維強化,提供多方面的升級。主要優點包括

  • 更高的耐熱性: 大幅提升熱變形溫度 (HDT),適用於較熱的環境。.

  • 增強剛性與尺寸穩定性: 更高的剛性和更低的熱膨脹,適用於精密零件。.

  • 靜電耗散: 內建導電性可保護電子元件。.
    對於需要比標準 PA66 更佳散熱和機械性能的應用而言,這是理想的起點。.

Q2: PA66 CF10 是否適用於汽車引擎蓋下零件?
是的,它是一個優秀的候選人。. 其固有的 高耐熱 (HDT >250°C) 結合改進的剛性和 ESD 保護,使其適用於溫度較高的感測器外殼、連接器、支架和引擎附近的其他元件。.

Q3: PA66 CF10 應該如何加工?
達到最佳效果:

  • 徹底乾燥 加工前在 80-90°C 下放置 4-6 小時,以防止水解。.

  • 使用 熔融溫度 在 280-310°C 的範圍內。.

  • 模溫 建議使用 80-110°C 的溫度,以獲得最佳的結晶度和表面光澤度。.

  • 由於碳纖維的磨損性,請使用耐磨的螺絲和料筒。.