プロパティ Nylon (PA6) POM(アセタール) PC 覗き見
Strength (MPa) 70-85 60-70 55-75 90-100
Max Use Temp (°C) 100 100 120 250
耐薬品性 グッド 素晴らしい 貧しい Outstanding
水分吸収 高い 非常に低い 非常に低い 非常に低い
相対コスト $$ $$$ $$$ $$$$$$$$$

Nylon: The All-Round Workhorse

Nylon applications
Nylon offers the best balance of properties and cost

Best For: General engineering applications, parts requiring toughness and fatigue resistance, oil/hydrocarbon exposure, cost-sensitive projects.

Watch Out For: Moisture absorption causing dimensional changes, property variation with humidity, acid exposure.

POM (Acetal): The Precision Specialist

Best For: Precision mechanical components (gears, bearings), dimensional stability in varying humidity, low-friction sliding components.

Watch Out For: Limited impact resistance, formaldehyde degradation if overheated, poor adhesion.

Polycarbonate: The Impact Champion

Polycarbonate applications
Polycarbonate is unmatched for impact resistance and optical clarity

Best For: Optical clarity applications, exceptional impact resistance, electrical enclosures, safety equipment.

Watch Out For: Very poor chemical resistance, environmental stress cracking, UV degradation without stabilizers.

PEEK: The High-Performance Specialist

Best For: Extreme temperatures (up to 250°C), aggressive chemical environments, aerospace and medical implants.

Watch Out For: Extremely high cost (10-20x nylon), high processing temperatures (350-400°C), requires specialized equipment.

Decision Matrix

If Your Priority Is… Best Choice Second Choice
Lowest Cost ナイロン PC
Highest Strength 覗き見 Nylon GF30
耐薬品性 覗き見 POM
Wear Resistance POM ナイロン
耐衝撃性 PC ナイロン
寸法安定性 POM 覗き見
Material selection flowchart
Use this decision framework to narrow down your material choices

当社の能力

を超える。 300台のCNCマシン, を生産している。 毎日10,000個 という厳しい公差で ±0.005mm. .我々は受け入れる 1個からのMOQ, 納期は以下の通り。 24時間~15日間. We work with all four engineering plastics. 24時間以内にお見積もりいたします。.

よくあるご質問

When is Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared a good option?

Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared is a good option when fast iteration, complex geometry, low tooling cost, or low-volume production is more important than molded-part unit cost.

What should be checked before choosing Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared?

部品サイズ、材料特性、表面仕上げ、寸法公差、熱暴露、荷重方向、後処理が必要かどうかを確認する。.

How does Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared compare with CNC machining?

3Dプリンティングは複雑な形状を素早く作ることができるが、CNC機械加工は精密な表面、より厳しい公差、生産グレードの材料に強いことが多い。.

What affects the cost of Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared?

コストは、材料、造形量、印刷時間、レイヤーの高さ、サポート除去、仕上げ、検査、造形物の部品数によって異なる。.

カスタムソリューションを作りましょう

このフィールドは必須です。.
このフィールドは必須です。.
このフィールドは必須です。.
このフィールドは必須です。.
このフィールドは必須です。.

関連記事

トップに戻る