엔지니어링 플라스틱 선택 가이드: 나일론, POM, PC 및 PEEK 애플리케이션 비교

Engineering plastics selection guide
Selecting the right engineering plastic requires understanding all the options

Choosing between nylon, POM, polycarbonate, and PEEK can be challenging. Each of these engineering plastics offers a unique combination of properties, costs, and processing characteristics.

The Four Major Engineering Plastics at a Glance

속성 Nylon (PA6) POM(아세탈) PC PEEK
Strength (MPa) 70-85 60-70 55-75 90-100
Max Use Temp (°C) 100 100 120 250
내화학성 Good 우수 Poor Outstanding
수분 흡수 높음 매우 낮음 매우 낮음 매우 낮음
상대적 비용 $$ $$$ $$$ $$$$$$$$$

Nylon: The All-Round Workhorse

Nylon applications
Nylon offers the best balance of properties and cost

Best For: General engineering applications, parts requiring toughness and fatigue resistance, oil/hydrocarbon exposure, cost-sensitive projects.

Watch Out For: Moisture absorption causing dimensional changes, property variation with humidity, acid exposure.

POM (Acetal): The Precision Specialist

Best For: Precision mechanical components (gears, bearings), dimensional stability in varying humidity, low-friction sliding components.

Watch Out For: Limited impact resistance, formaldehyde degradation if overheated, poor adhesion.

Polycarbonate: The Impact Champion

Polycarbonate applications
Polycarbonate is unmatched for impact resistance and optical clarity

Best For: Optical clarity applications, exceptional impact resistance, electrical enclosures, safety equipment.

Watch Out For: Very poor chemical resistance, environmental stress cracking, UV degradation without stabilizers.

PEEK: The High-Performance Specialist

Best For: Extreme temperatures (up to 250°C), aggressive chemical environments, aerospace and medical implants.

Watch Out For: Extremely high cost (10-20x nylon), high processing temperatures (350-400°C), requires specialized equipment.

Decision Matrix

If Your Priority Is… Best Choice Second Choice
Lowest Cost 나일론 PC
Highest Strength PEEK Nylon GF30
내화학성 PEEK POM
내마모성 POM 나일론
내충격성 PC 나일론
치수 안정성 POM PEEK
Material selection flowchart
Use this decision framework to narrow down your material choices

Our Capabilities

With over 300 CNC machines, we produce more than 10,000 pieces daily with tolerances as tight as ±0.005mm. We accept MOQ from 1 piece, with delivery times ranging from 24 hours to 15 days. We work with all four engineering plastics. Get a quote within 24 hours.

자주 묻는 질문

When is Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared a good option?

Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared is a good option when fast iteration, complex geometry, low tooling cost, or low-volume production is more important than molded-part unit cost.

What should be checked before choosing Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared?

부품 크기, 재료 특성, 표면 마감, 치수 공차, 열 노출, 하중 방향, 후처리가 필요한지 여부를 확인합니다.

How does Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared compare with CNC machining?

3D 프린팅은 복잡한 형상을 빠르게 제작할 수 있는 반면, CNC 가공은 정밀한 표면, 엄격한 공차 및 생산 등급 재료에 더 적합한 경우가 많습니다.

What affects the cost of Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared?

비용은 재료, 빌드 볼륨, 프린트 시간, 레이어 높이, 서포트 제거, 마감, 검사 및 빌드 내 부품 수에 따라 달라집니다.

맞춤형 솔루션 제작하기

이 필드는 필수 입력 사항입니다.
이 필드는 필수 입력 사항입니다.
이 필드는 필수 입력 사항입니다.
이 필드는 필수 입력 사항입니다.
이 필드는 필수 입력 사항입니다.

관련 읽기

맨 위로 스크롤