工程塑膠選擇指南:尼龍、POM、PC 和 PEEK 應用比較

Engineering plastics selection guide
Selecting the right engineering plastic requires understanding all the options

Choosing between nylon, POM, polycarbonate, and PEEK can be challenging. Each of these engineering plastics offers a unique combination of properties, costs, and processing characteristics.

The Four Major Engineering Plastics at a Glance

財產 Nylon (PA6) POM (乙縮醛) 個人電腦 PEEK
Strength (MPa) 70-85 60-70 55-75 90-100
Max Use Temp (°C) 100 100 120 250
耐化學性 良好 極佳 Poor Outstanding
吸濕性 非常低 非常低 非常低
相對成本 $$ $$$ $$$ $$$$$$$$$

Nylon: The All-Round Workhorse

Nylon applications
Nylon offers the best balance of properties and cost

Best For: General engineering applications, parts requiring toughness and fatigue resistance, oil/hydrocarbon exposure, cost-sensitive projects.

Watch Out For: Moisture absorption causing dimensional changes, property variation with humidity, acid exposure.

POM (Acetal): The Precision Specialist

Best For: Precision mechanical components (gears, bearings), dimensional stability in varying humidity, low-friction sliding components.

Watch Out For: Limited impact resistance, formaldehyde degradation if overheated, poor adhesion.

Polycarbonate: The Impact Champion

Polycarbonate applications
Polycarbonate is unmatched for impact resistance and optical clarity

Best For: Optical clarity applications, exceptional impact resistance, electrical enclosures, safety equipment.

Watch Out For: Very poor chemical resistance, environmental stress cracking, UV degradation without stabilizers.

PEEK: The High-Performance Specialist

Best For: Extreme temperatures (up to 250°C), aggressive chemical environments, aerospace and medical implants.

Watch Out For: Extremely high cost (10-20x nylon), high processing temperatures (350-400°C), requires specialized equipment.

Decision Matrix

If Your Priority Is… Best Choice Second Choice
Lowest Cost 尼龍 個人電腦
Highest Strength PEEK Nylon GF30
耐化學性 PEEK POM
Wear Resistance POM 尼龍
耐衝擊性 個人電腦 尼龍
尺寸穩定性 POM PEEK
Material selection flowchart
Use this decision framework to narrow down your material choices

Our Capabilities

With over 300 CNC machines, we produce more than 10,000 pieces daily with tolerances as tight as ±0.005mm. We accept MOQ from 1 piece, with delivery times ranging from 24 hours to 15 days. We work with all four engineering plastics. Get a quote within 24 hours.

常見問題

When is Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared a good option?

Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared is a good option when fast iteration, complex geometry, low tooling cost, or low-volume production is more important than molded-part unit cost.

What should be checked before choosing Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared?

檢查零件尺寸、材料特性、表面光潔度、尺寸公差、受熱情況、負載方向,以及是否需要後加工。.

How does Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared compare with CNC machining?

3D 列印可以快速製造複雜的形狀,而 CNC 加工通常在精密表面、更小的公差和生產級材料方面更強。.

What affects the cost of Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared?

成本取決於材料、建置量、列印時間、層高、支撐移除、精加工、檢查以及建置中的零件數量。.

讓我們為您量身打造解決方案

此欄位必須填寫。.
此欄位必須填寫。.
此欄位必須填寫。.
此欄位必須填寫。.
此欄位必須填寫。.

相關閱讀

滾動到頂端