Choosing between nylon, POM, polycarbonate, and PEEK can be challenging. Each of these engineering plastics offers a unique combination of properties, costs, and processing characteristics.
The Four Major Engineering Plastics at a Glance
| الممتلكات | Nylon (PA6) | بوم (أسيتال) | كمبيوتر شخصي | بيك |
|---|---|---|---|---|
| Strength (MPa) | 70-85 | 60-70 | 55-75 | 90-100 |
| Max Use Temp (°C) | 100 | 100 | 120 | 250 |
| مقاومة المواد الكيميائية | جيد | ممتاز | Poor | Outstanding |
| امتصاص الرطوبة | عالية | منخفضة جداً | منخفضة جداً | منخفضة جداً |
| Relative Cost | $$ | $$$ | $$$ | $$$$$$$$$ |
Nylon: The All-Round Workhorse

Best For: General engineering applications, parts requiring toughness and fatigue resistance, oil/hydrocarbon exposure, cost-sensitive projects.
Watch Out For: Moisture absorption causing dimensional changes, property variation with humidity, acid exposure.
POM (Acetal): The Precision Specialist
Best For: Precision mechanical components (gears, bearings), dimensional stability in varying humidity, low-friction sliding components.
Watch Out For: Limited impact resistance, formaldehyde degradation if overheated, poor adhesion.
Polycarbonate: The Impact Champion

Best For: Optical clarity applications, exceptional impact resistance, electrical enclosures, safety equipment.
Watch Out For: Very poor chemical resistance, environmental stress cracking, UV degradation without stabilizers.
PEEK: The High-Performance Specialist
Best For: Extreme temperatures (up to 250°C), aggressive chemical environments, aerospace and medical implants.
Watch Out For: Extremely high cost (10-20x nylon), high processing temperatures (350-400°C), requires specialized equipment.
Decision Matrix
| If Your Priority Is… | Best Choice | Second Choice |
|---|---|---|
| Lowest Cost | نايلون | كمبيوتر شخصي |
| Highest Strength | بيك | Nylon GF30 |
| مقاومة المواد الكيميائية | بيك | POM |
| Wear Resistance | POM | نايلون |
| مقاومة الصدمات | كمبيوتر شخصي | نايلون |
| ثبات الأبعاد | POM | بيك |

Our Capabilities
With over 300 CNC machines, we produce more than 10,000 pieces daily with tolerances as tight as ±0.005mm. We accept MOQ from 1 piece, with delivery times ranging from 24 hours to 15 days. We work with all four engineering plastics. Get a quote within 24 hours.
الأسئلة الشائعة
When is Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared a good option?
Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared is a good option when fast iteration, complex geometry, low tooling cost, or low-volume production is more important than molded-part unit cost.
What should be checked before choosing Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared?
تحقق من حجم الجزء، وخصائص المواد، وتشطيب السطح، وتفاوت الأبعاد، والتعرض للحرارة، واتجاه التحميل، وما إذا كانت المعالجة اللاحقة مطلوبة.
How does Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared compare with CNC machining?
يمكن للطباعة ثلاثية الأبعاد إنشاء أشكال معقدة بسرعة، في حين أن التصنيع باستخدام الحاسب الآلي غالبًا ما يكون أقوى للأسطح الدقيقة والتفاوتات الأكثر دقة والمواد ذات درجة الإنتاج.
What affects the cost of Engineering Plastics Selection Guide: Nylon, POM, PC, and PEEK Applications Compared?
تعتمد التكلفة على المواد، وحجم البناء، ووقت الطباعة، وارتفاع الطبقة، وإزالة الدعم، والتشطيب، والفحص، وعدد الأجزاء في البناء.