PA66 GF30 Material Grade and Technical Documentation
PA66 GF30 identifies polyamide 66 reinforced with 30% glass fiber. Select the exact compound, color and processing route before purchasing; the material name alone does not define heat aging, impact behavior, flame rating or a finished-part specification.
The named grade reference below is WanHan PA66 WHG30A. Use the current PA66 WHG30A technical data sheet for initial screening, then confirm the production formulation and approval requirements. Request a PA66 GF30 TDS and Material Recommendation. An initial material inquiry does not require CAD or a confirmed quantity.
Data scope: the PDF gives typical values, not design allowables or guaranteed specification limits. It does not state the conditioning state or specimen details. HDT is reported under ISO 75-2/B; do not treat it as an ISO 75 result at 1.8 MPa or as a continuous-use temperature.
PA66 GF30 Named-Grade Technical Data
| Property | Test method | Unit | Typical value |
|---|---|---|---|
| Tensile strength | ISO 527-2 | MPa | 175 |
| Flexural strength | ISO 178 | MPa | 255 |
| Flexural modulus | ISO 178 | MPa | 7,000 |
| HDT, method B | ISO 75-2/B | °C | 220 |
| Density | ISO 1183 | g/cm³ | 1.38 |
| Molding shrinkage | ISO 2577 | % | 0.5 |
| Flammability rating | UL 94 | — | Not specified in this TDS |
PA66 Series Material Performance Comparison Table:
| Grade family | Initial selection consideration | Required validation |
|---|---|---|
| PA66 GF15 / GF20 | Compare when moderate reinforcement and retained toughness matter. | Exact-grade stiffness, impact, heat and conditioning data. |
| PA66 GF30 | Compare for a balance of reinforcement and processing requirements. | Selected formulation, gate/fiber orientation, moisture and molded-part performance. |
| PA66 GF33 | Review an intermediate glass loading against the actual grade data. | Do not assume a thermal or mechanical improvement from the percentage alone. |
| PA66 GF50 / GF60 | Compare where additional reinforcement is relevant to the design. | Flow, warpage, weld-line strength, impact and surface requirements. |
Key Advantages of PA66 GF30:
High Strength & Stiffness:
Offers an excellent strength-to-weight ratio, often used as a direct replacement for metals in structural parts.
Exceptional Heat Resistance:
Check the exact-grade HDT method, heat-aging data and service conditions; HDT does not establish continuous-use performance.
Good Dimensional Stability:
Review moisture conditioning, creep, fiber orientation and molded-part dimensions for the actual service environment.
Excellent Wear & Abrasion Resistance:
Superior performance in moving parts and gears compared to many other plastics.
Industry Applications:

PA66GF30 is commonly used in automotive components, interior parts, and other applications that require a good surface finish and fundamental rigidity.
Powering Innovation Across Industries
| Industry | Key Applications |
|---|---|
| Automotive | Engine covers, intake manifolds, structural brackets, sensor housings, connectors. Explore Automotive Applications → |
| Electrical & Electronics | Circuit breakers, switches, connector housings, insulating components. Discover E&E Solutions → |
| Industrial Equipment | Gears, bearings, machine housings, rollers, mechanical components. See Industrial Uses → |

How to Choose the Right PA66 Grade?
For optimal toughness and cost-effectiveness, start with PA66 GF15. It provides a solid upgrade from unreinforced PA66, offering solid strength and good impact resistance for general industrial and automotive components.
For the best all-around, industry-proven performance, choose PA66 GF30. It delivers an excellent balance of high strength, stiffness, and exceptional heat resistance (HDT >250°C), making it the default choice for demanding structural and under-hood applications.
For a measurable performance upgrade where standard grades reach their limit, consider PA66 GF33. This grade offers higher stiffness and thermal margin than GF30, subject to exact-grade data and molded-part validation.
For maximum stiffness, strength, and thermal resistance where metal replacement is the goal, look to PA66 GF50 or PA66 GF60. These high-fiber grades deliver near-metallic properties for extreme loads and temperatures, but require careful evaluation of their reduced impact toughness and significant processing challenges.
Why Choose Us?


Processing, Modifications and Material Inquiry
Follow the approved grade drying and processing instructions. Review moisture, fiber orientation, shrinkage, weld lines and conditioning before judging critical dimensions. Ask about reinforcement, color matching, heat stabilization, impact modification, flame-retardant or hydrolysis-resistant options only where the application requires them; availability and final properties are confirmed for the selected formulation.
For a grade review, send the application, temperature and load, chemical or moisture exposure, color, required documents and material usage if known. For finished parts, use a separate Manufacturing Quote with dimensions and process requirements. See the PA66 GF30 technical guide for selection context.
PA66 GF30 Questions
Can I request a PA66 GF30 TDS and sample?
Request the current datasheet and discuss sample material for the selected grade. Include the application, color, trial quantity and validation requirements. Sample availability, charges and delivery are confirmed for the request.
How is the delivery schedule confirmed?
The quotation confirms the selected grade, quantity, color or formulation changes, required documents, packaging and destination. Ask for the agreed dispatch and delivery milestones before ordering.
Which material and compliance documents should I request?
Ask for the exact-grade TDS and SDS, and specify whether batch COA or COC and application compliance records are required. UL 94, RoHS and REACH suitability must be confirmed for the selected formulation and document scope; PA66 GF30 alone is not a compliance approval.