PA66 GF25 FR(V0) Flame Retardant Nylon 66 – Nylon Plastic

What is PA66 GF25 FR(V0)?
PA66 GF25 FR(V0) is a flame-retardant nylon 66 reinforced with 25% glass fibers. It occupies a strategic position between standard and high-performance FR grades, delivering significantly higher stiffness and strength than GF15 or GF20 grades. This material is engineered for components that require substantial structural integrity to withstand mechanical loads and thermal stress, all while complying with stringent V-0 fire safety standards in challenging environments.

Why Choose Nylon Plastic’s PA66 GF25 FR(V0)?
✅ Superior Structural Performance with Safety: We deliver a material that excels in load-bearing applications where flame retardancy cannot be compromised, such as electrical enclosures and automotive brackets.
✅ Engineered for Stability Under Stress: Our formulation prioritizes low warpage and high dimensional stability, ensuring part precision and reliability in demanding conditions.
✅ Solution for Complex Functional Parts: We provide the technical expertise to help you mold larger or more complex components that require this balanced performance profile.
✅ Commitment to Consistent High Quality: We maintain stringent control over our compounding process to ensure every batch meets the high mechanical and safety standards this grade demands.

万翰详情 01

PA66 GF25 FR(V0) Technical Data (Estimated Typical Values)

Property Value Test Standard
Glass Fiber Content 25% ISO 1172
Flame Retardancy UL94 V-0 (at specified thickness) UL 94
Tensile Strength 135 – 170 MPa ISO 527
Flexural Modulus 7,000 – 9,500 MPa ISO 178
Notched Impact Strength 9 – 12 kJ/m² ISO 180
HDT @1.8 MPa 247 – 257 °C ISO 75
Melting Point 255 – 265 °C ISO 3146

PA66 FR Series Performance Comparison Table (Updated)

Property PA66 FR(V0) PA66 GF15 FR(V0) PA66 GF20 FR(V0) PA66 GF25 FR(V0) PA66 GF30 FR(V0) PA66 GF50 FR(V0)
Glass Fiber Content 0% 15% 20% 25% 30% 50%
Flame Retardancy UL94 V-0 UL94 V-0 UL94 V-0 UL94 V-0 UL94 V-0 UL94 V-0
Tensile Strength ~75 MPa ~120 MPa ~140 MPa ~150 MPa ~160 MPa ~190 MPa
Flexural Modulus ~3,000 MPa ~5,500 MPa ~7,000 MPa ~7,800 MPa ~8,500 MPa ~13,500 MPa
Notched Impact ~6 kJ/m² ~9 kJ/m² ~9.5 kJ/m² ~9.8 kJ/m² ~10 kJ/m² ~8 kJ/m²
HDT @1.8MPa ~240 °C ~245 °C ~248 °C ~249 °C ~250 °C ~255 °C
Key Profile Basic FR, good toughness Entry-level balance Balanced for medium-duty Enhanced structural FR performance Best balance of strength, heat & FR Ultimate stiffness for high-load FR designs

Key Advantages of PA66 GF25 FR(V0)

✅ Superior Stiffness for Structural FR Applications:

Delivers a high level of rigidity and load-bearing capacity, making it a prime candidate for structural components that cannot compromise on fire safety.

✅Exceptional Stability Under Heat and Load:

Inherits PA66’s high melting point, with a Heat Deflection Temperature (HDT) typically above 245°C, ensuring stability in under-hood and high-heat electrical environments.

✅ Designed for High-Stress Safety-Critical Parts:

Provides the mechanical integrity needed for demanding applications such as circuit breaker housings, large electrical enclosures, and automotive structural brackets.

✅ Long-Term Durability in Harsh Conditions:

Offers excellent resistance to creep and fatigue under sustained stress, alongside inherent chemical resistance, for dependable long-term performance.

 

Industry Applications:

the crucial role of injection molding in automotive industry

PA66 FR Series: Application Scenarios & Product Keywords

Grade Typical Application Scenarios (with Product Keywords)
PA66 FR(V0) Electrical Insulation Parts: Sockets, switch housings, circuit breaker bases, fuse boxes, wiring harness clips, relay housings, small electrical enclosures.
PA66 GF10 FR(V0) Thin-Wall Electronic Components: LED lamp holders, miniature connectors, coil bobbins, power adapter housings, internal brackets for electronic devices, cable clamps.
PA66 GF15 FR(V0) Appliances & Automotive Electrical: Power tool housings, junction boxes for home appliances, automotive wiring harness connectors, sensor plugs, HVAC damper actuator housings.
PA66 GF20 FR(V0) Heat-Resistant Electrical & Under-Hood Parts: Engine bay electrical connectors, ignition coil housings, transmission sensor covers, small fan impellers, electric water pump housings.
PA66 GF25 FR(V0) Medium-Structural Strength Parts: Circuit breaker enclosures, power module housings, industrial control equipment panels, automotive headlamp adjustment brackets, mirror housings.
PA66 GF30 FR(V0) High-Demand Structural & Automotive Parts: Intake manifold components (resonators), throttle body brackets, engine cover caps, heavy-duty connectors, industrial gears, power tool gearboxes.
PA66 GF33 FR(V0) High-Performance Precision Structural Parts: Precision gears, bearing housings, high-load electrical terminals, automotive Electronic Control Unit (ECU) housings, high-performance cooling fan frames.
PA66 GF35 FR(V0) High-Rigidity Heat-Resistant Structural Parts: Large under-hood brackets, Battery Management System (BMS) enclosures, motor end covers, industrial valve bodies, pump housings.
PA66 GF40 FR(V0) Metal Replacement Structural Parts: Intake air ducts, turbocharger inlet pipe connectors, structural brackets, heavy-duty industrial equipment panels, drone airframe structural parts.
PA66 GF50 FR(V0) Ultra-High Rigidity Load-Bearing Parts: Structural reinforcement parts, high-performance automotive seat frame components, large industrial bearing cages, robotic arm structural parts, drone landing gear.

Powering Innovation Across Industries

Industry Key Applications
Automotive Engine covers, intake manifolds, structural brackets, sensor housings, connectors.
Explore Automotive Applications →
Electrical & Electronics Circuit breakers, switches, connector housings, insulating components.
Discover E&E Solutions →
Industrial Equipment Gears, bearings, machine housings, rollers, mechanical components.
See Industrial Uses →
Various application scenarios of PA plastics
Various application scenarios of PA plastics

How to Choose the Right Flame Retardant (FR) Grade?

In simple terms:

For basic flame retardancy with good toughness and lowest cost, consider PA6 FR(V0) or PA6 GF15 FR(V0).

For the best balance of flame safety, strength, and heat resistance, choose PA6 GF30 FR(V0) or PA66 GF30 FR(V0).

For applications requiring maximum stiffness and thermal performance alongside V-0 rating, consider PA6 GF40/50 FR(V0) or PA66 GF40/50 FR(V0).

Unsure which is perfect for your part? Describe your application to our engineers for a tailored recommendation: https://nylonplastic.com/contact/

Why Choose Us?

万翰详情 03

万翰详情 04

FAQ Section:

Q: Can I get a sample before placing an order?
A: Yes! We provide free samples for qualified projects.

Q: What’s the lead time for production?
A: Standard grades: 5-7 days; Custom formulations: 2-3 weeks.

Q: Do you provide material certifications?
A: Yes, we provide full material documentation and certifications.

Tell Us About Your Part

This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
Scroll to Top

Get in Touch

Fill out the form below, and we will be in touch shortly.

Contact Information