PC-ABS is a practical engineering topic when you need to compare options, check limits, and choose a process with less risk.

PC-ABS (Polycarbonate-ABS blend) is a high-performance engineering filament combining polycarbonate’s exceptional strength and heat resistance with ABS’s ease of printing and toughness. This synergistic blend produces a material with superior mechanical properties suitable for demanding functional applications in automotive, aerospace, and industrial environments.



PC-ABS Material Properties
With tensile strength of 55-65 MPa (higher than ABS and PLA) and impact strength of 40-50 kJ/m² (3-4x higher than standard ABS), PC-ABS is exceptionally durable. The heat deflection temperature reaches 110-120°C at 1.82 MPa, making it suitable for elevated temperature applications. Our PC-ABS HF High Flow grade offers improved processability.
Printing Guidelines
Print at 270-290°C nozzle temperature (hardened steel recommended) with 100-110°C bed temperature using PEI or similar high-adhesion surface. An enclosed printer is essential—target 40-50°C chamber temperature for optimal results.
Applications
PC-ABS is used for automotive instrument clusters, functional prototypes, and under-hood components. In aerospace, it’s suitable for interior brackets, ducting, and structural prototypes. Electronics applications include durable housings, connectors, and insulators.
Source PC-ABS Materials
As a specialized source manufacturer, we offer PC-ABS in both filament form for 3D printing and as engineering stock for CNC machining. Our PC-ABS GF20 with 20% glass fiber provides enhanced stiffness. Contact us for technical support and pricing.
Get a Free Quote
Fill out the form below and our engineers will respond within 24 hours.
PC-ABS Blend Printing Checks
| Control | Why it matters |
|---|---|
| Drying | Moisture can reduce layer bonding, strength and surface quality |
| Chamber and bed | Stable heat reduces warping and residual stress |
| Orientation | Layer direction changes impact and tensile performance |
| Validation | Test the actual wall, hole, snap-fit and heat exposure on the finished part |
Record the resin grade, nozzle, bed, chamber, drying cycle, layer height and cooling settings with the part revision. Compare PC-ABS with pure PC when the heat ceiling or chemical exposure is the primary constraint.
FAQ
When is PC-ABS Blend — The Best of Both Worlds for Durable 3D Printed Parts a good option?
PC-ABS Blend — The Best of Both Worlds for Durable 3D Printed Parts is a good option when fast iteration, complex geometry, low tooling cost, or low-volume production is more important than molded-part unit cost.
What should be checked before choosing PC-ABS Blend — The Best of Both Worlds for Durable 3D Printed Parts?
Check part size, material properties, surface finish, dimensional tolerance, heat exposure, load direction, and whether post-processing is required.
How does PC-ABS Blend — The Best of Both Worlds for Durable 3D Printed Parts compare with CNC machining?
3D printing can create complex shapes quickly, while CNC machining is often stronger for precise surfaces, tighter tolerances, and production-grade materials.
What affects the cost of PC-ABS Blend — The Best of Both Worlds for Durable 3D Printed Parts?
Cost depends on material, build volume, print time, layer height, support removal, finishing, inspection, and the number of parts in the build.