ABS
Standard
Tensile Strength
40 MPa
Heat Deflection
98°C
Impact Strength
High
Chemical Resistance
Medium
CNC
Injection
PP Homopolymer
Polypropylene
Tensile Strength
35 MPa
Heat Deflection
105°C
Impact Strength
Medium
Chemical Resistance
Excellent
Injection
Nylon 6/6
Polyamide
Tensile Strength
80 MPa
Heat Deflection
255°C
Impact Strength
High
Wear Resistance
Excellent
CNC
Injection
Polycarbonate
PC
Tensile Strength
65 MPa
Heat Deflection
138°C
Impact Strength
Very High
Transparency
Excellent
CNC
Injection
PEEK 450G
High Performance
Tensile Strength
100 MPa
Heat Deflection
315°C
Chemical Resistance
Excellent
Wear Resistance
Excellent
CNC
Injection
Acetal (POM)
Delrin
Tensile Strength
69 MPa
Heat Deflection
124°C
Friction Coefficient
Very Low
Dimensional Stability
Excellent
CNC
Injection
Material Comparison
Compare key properties of different plastic materials side by side.
| Property | ABS | PP | Nylon 6/6 | PC | PEEK | POM |
|---|---|---|---|---|---|---|
| Tensile Strength (MPa) | 40 | 35 | 80 | 65 | 100 | 69 |
| Flexural Modulus (GPa) | 2.3 | 1.5 | 2.8 | 2.4 | 3.8 | 2.8 |
| HDT @ 1.82 MPa (°C) | 98 | 105 | 255 | 138 | 315 | 124 |
| Impact Strength (J/m) | 400 | 50 | 110 | 850 | 80 | 75 |
| Density (g/cm³) | 1.05 | 0.91 | 1.14 | 1.20 | 1.32 | 1.41 |