PA12 GF25 Reinforced Nylon 12 Pellets

PA12 GF25 is a 25% glass fiber reinforced nylon 12 compound supplied as pellets. The supplied reference sheet identifies the material as PA12 GF25. Equipment housings, mounting parts and fluid-system component concepts are candidates for review against the actual component requirements.

Reference grade: PA12 GF25

Supply: 25% glass fiber reinforced pellets. Confirm color, quantity and required documents with your inquiry.

Categories: ,

PA12 GF25 Material Overview

PA12 GF25 is a 25% glass fiber reinforced nylon 12 compound supplied as pellets. The supplied reference sheet identifies the material as PA12 GF25. Equipment housings, mounting parts and fluid-system component concepts are candidates for review against the actual component requirements.

Item Details
Reference grade PA12 GF25
Polymer PA12
Reinforcement 25% glass fiber
Form Pellets for material-supply inquiries
Color and processing Confirm the offered grade and current processing guidance

Reference Material Properties

Typical values for PA12 GF25 from the linked supplier PDF.

Property Typical value Test method
Tensile strength 98 MPa ISO 527
Tensile modulus 5250 MPa ISO 527
Elongation at break 9% ISO 527
Density 1.20 g/cm³ ISO 1183

Specimen conditioning is not stated in the reference sheet. These values are not guaranteed specification limits. Confirm the current datasheet, required test conditions and acceptance criteria for your component.

Download PA12 GF25 supplier reference datasheet (PDF)

Application Review

PA12 GF25 illustrative component applications
Illustrative component concepts. Confirm the selected formulation for the actual part.

Component candidates

Equipment housings, mounting parts and fluid-system component concepts. Define fluid exposure, pressure where relevant, mounting loads and dimensional acceptance. Validate the selected formulation on representative parts.

Assembly interfaces

Define mounting points, ribs, inserts, sealing faces and critical fits on the drawing. Agree which dimensions and functional features require sample approval.

Sample acceptance

Use representative parts made with the intended formulation and process. Specify the load, environment, appearance and inspection conditions that matter for the application.

Processing and Part Checks

Define fluid exposure, pressure where relevant, mounting loads and dimensional acceptance. Validate the selected formulation on representative parts. Follow the current processing instructions for PA12 GF25. Review gate location, weld lines, shrinkage and inspection timing with the molding team before fixing production conditions.

For component production, review our injection molding service. For other resin options, browse engineering plastic materials.

Material Supply and Manufacturing Support

Nylon Plastic connects engineering plastic supply with custom manufacturing. WANHAN is our cooperating compounding factory; the photographs below show its material-feeding equipment, extrusion process and laboratory.

Material feeding equipment at WANHAN, Nylon Plastic’s cooperating factory
Material feeding
Extruded plastic strands at the WANHAN cooperating factory
Extrusion process
Laboratory work area at the WANHAN cooperating factory
Laboratory

Grade and formulation selection

Share your current grade, application and operating conditions. We coordinate the material review and identify the matching datasheet for the formulation offered.

Quality documents for your order

Specify the TDS, batch records, inspection requirements or compliance files your purchasing team needs. The documents and acceptance criteria are agreed for the quoted material.

Support beyond resin pellets

For a finished component, connect material selection with part design, tooling and molding review. Start with the drawing, expected quantity and critical dimensions.

Cooperating Factory Management-System Certificates

The supplied ISO 9001, ISO 14001 and ISO 45001 certificates identify Guangdong Wanhan as the certified entity. Their scope concerns modified plastic granules and the related management activities; it does not certify every material grade or every finished-part manufacturing service.

Review manufacturing capabilities and quality documentation. For document approval, match the legal entity, certificate scope and quoted grade.

Frequently Asked Questions

What material does this page cover?

PA12 GF25 is a 25% glass fiber reinforced nylon 12 compound supplied as pellets. The supplied reference sheet identifies the material as PA12 GF25. Equipment housings, mounting parts and fluid-system component concepts are candidates for review against the actual component requirements.

Are these pellets ready-to-use filament or a qualified tubing material?

No. A pellet grade needs a processing-route review and component validation. Filament conversion, extrusion or tubing applications require separate approval and equipment compatibility checks.

Are these values a production specification?

No. They are typical reference values for PA12 GF25. Agree the current grade, test conditions, acceptance limits and required documents for the order.

Do the images show the exact supplied color and finished parts?

The images illustrate resin appearance and possible component concepts. Confirm color and finish on the offered material and samples; the pictured parts do not establish suitability for your design.

What is required for a material replacement?

Identify the current resin and reason for changing it. Compare exact-grade data, dimensions, loads, temperature and environmental exposure, then validate the intended part before production.

What should I send for a quote or sample request?

Send the reference grade, application, color, estimated material quantity and required documents. For a molded-part inquiry, add the drawing, critical dimensions and acceptance requirements. A CAD file is optional for a material-only inquiry.

Related Material Grades

PA12 GF30   |   PA12 CF30

Request Material Data and a Quote

Share the grade, application, service conditions, color, quantity and required documents so the offered material can be reviewed against your project.

Request PA12 GF25 TDS and Quote

Scroll to Top

Get in Touch

Fill out the form below, and we will be in touch shortly.

Contact Information