PA6 GF15 FR(V0) 15% GF Reinforced V-0 Nylon 6

PA66 GF15 FR(V0)

What is PA66 GF15 FR(V0)?
PA66 GF15 FR(V0) is an engineered thermoplastic where nylon 66 is compounded with 15% glass fibers and flame-retardant additives to achieve UL94 V-0. It is designed for applications that demand a meaningful and reliable upgrade in mechanical strength, stiffness, and thermal capability from a flame-safe material. Serving as a robust and versatile entry-level reinforced FR solution, this grade effectively replaces non-reinforced FR grades where increased load-bearing capacity and better long-term dimensional stability are required.

Why Choose Nylon Plastic’s PA66 GF15 FR(V0)?
✅ Robust Foundation for Safety-Critical Parts: We provide a material that delivers certified flame retardancy alongside reliable structural performance, making it a trusted choice for a wide range of automotive and industrial components.
✅ Proven in High-Volume Manufacturing: Our grade is optimized for efficient, stable processing, making it an ideal and economical selection for mass-producing durable parts like power tool housings, automotive connectors, and appliance components.
✅ Focused on Durability & Long Service Life: Our formulation ensures good resistance to creep and environmental stress cracking, enhancing the durability and extending the operational life of your products in demanding conditions.
✅ Strategic Partnership for Mainstream Projects: We are committed to being a reliable, long-term supply partner for your projects that require this versatile and widely applicable FR workhorse material.

万翰详情 01

PA6 GF15 FR(V0) Technical Data (Estimated Typical Values)

Property Value Test Standard
Glass Fiber Content 15% ISO 1172
Flame Retardancy UL94 V-0 (at specified thickness) UL 94
Tensile Strength 100 – 130 MPa ISO 527
Flexural Modulus 4,500 – 6,000 MPa ISO 178
Notched Impact Strength 8 – 12 kJ/m² ISO 180
HDT @1.8 MPa 195 – 205 °C ISO 75
Melting Point 215 – 225 °C ISO 3146

PA6 FR Series Performance Comparison Table (Updated)

Property PA6 FR(V0) PA6 GF15 FR(V0) PA6 GF25 FR(V0) PA6 GF30 FR(V0) PA6 GF50 FR(V0)
Glass Fiber Content 0% 15% 25% 30% 50%
Flame Retardancy UL94 V-0 UL94 V-0 UL94 V-0 UL94 V-0 UL94 V-0
Tensile Strength ~65 MPa ~110 MPa ~140 MPa ~155 MPa ~195 MPa
Flexural Modulus ~2,800 MPa ~5,000 MPa ~7,500 MPa ~8,200 MPa ~12,500 MPa
Notched Impact ~5 kJ/m² ~9 kJ/m² ~10 kJ/m² ~11 kJ/m² ~9 kJ/m²
HDT @1.8MPa ~75 °C ~200 °C ~205 °C ~210 °C ~215 °C
Key Profile Basic FR, economical Balanced FR performer High-stiffness FR grade Premium all-round FR Ultra-rigid FR composite

Key Advantages of PA6 GF15 FR(V0)

✅Enhanced Mechanical Performance:

he 15% glass fiber reinforcement significantly boosts tensile strength and rigidity over non-reinforced FR grades, allowing for more durable part design.

✅Improved Heat Resistance & Stability:

 Offers a higher Heat Deflection Temperature (HDT) and reduced warpage, ensuring reliable performance in warmer operating environments.

✅Optimal for Demanding Electrical Housings:

Combines structural integrity with fire safety, making it a top choice for power tool housings, appliance components, and automotive electrical parts.

✅ Excellent Value for Performance:

Delivers a substantial upgrade in load-bearing capability and thermal performance, providing outstanding value for a wide array of applications.

Industry Applications:

the crucial role of injection molding in automotive industry

PA6 FR Series: Application Scenarios & Product Keywords

Grade Typical Application Scenarios
PA6 FR(V0) General Electrical & Consumer Parts: Sockets, switch housings, light diffusers, cable management clips, small appliance housings, electronic device enclosures, internal insulators.
PA6 GF15 FR(V0) Durable Consumer & Light Industrial Components: Power tool housings (body), household appliance structural parts, electrical junction boxes, ventilation fan blades, automotive interior trim clips, connector housings.
PA6 GF25 FR(V0) Enhanced-Structural Components: Industrial control enclosures, power supply housings, automotive fuse box housings, pump covers, medium-load gears and levers, functional brackets in appliances.
PA6 GF30 FR(V0) High-Performance Industrial & Automotive Parts: Gear wheels in machinery, bearing cages, high-strength connectors and bobbins, electric vehicle charging gun components, industrial fan impellers, automotive engine cooling fan shrouds.
PA6 GF50 FR(V0) Ultra-High Stiffness Specialized Parts: Lightweight structural frames and brackets (e.g., for drones or equipment), high-load bearing components, industrial automation guides and rails, robotic arm links, specialized tooling and jigs.

Powering Innovation Across Industries

Industry Key Applications
Automotive Engine covers, intake manifolds, structural brackets, sensor housings, connectors.
Explore Automotive Applications →
Electrical & Electronics Circuit breakers, switches, connector housings, insulating components.
Discover E&E Solutions →
Industrial Equipment Gears, bearings, machine housings, rollers, mechanical components.
See Industrial Uses →
Various application scenarios of PA plastics
Various application scenarios of PA plastics

How to Choose the Right PA6 Flame Retardant (FR) Grade?

In simple terms:

For basic flame retardancy with good toughness and the lowest cost, consider PA6 FR(V0) or PA6 GF15 FR(V0). These are ideal for general electrical housings, consumer appliance parts, and applications where ease of processing is key.

For the best all-around balance of flame safety, mechanical strength, and thermal performance, choose PA6 GF30 FR(V0). It is the industry-preferred grade for demanding components like gears, industrial enclosures, and automotive under-hood fans that require reliable durability.

For applications demanding maximum stiffness and dimensional stability alongside the V-0 rating, consider PA6 GF50 FR(V0). This ultra-high modulus grade enables metal replacement in structural designs where weight reduction is critical.

Unsure which is perfect for your part? Describe your application to our engineers for a tailored recommendation: https://nylonplastic.com/contact/

Why Choose Us?

万翰详情 03

万翰详情 04

PA6 FR Series: Frequently Asked Questions (FAQ)

Q1: What is PA6 FR(V0) material and what are its key features?
A1: PA6 FR(V0) is a flame-retardant grade of Nylon 6 (Polyamide 6) that meets the stringent UL94 V-0 standard, meaning it can stop burning within seconds in a vertical flame test. Its key features include good balance of toughness, excellent electrical insulation properties, and relatively low cost compared to higher-performance engineering plastics. It is widely used in electrical and electronic components.

Q2: What’s the difference between PA6 FR(V0), PA6 GF30 FR(V0), and PA6 GF50 FR(V0)?
A2: The core difference lies in glass fiber (GF) content and the resulting mechanical properties:

  • PA6 FR(V0): Contains 0% glass fiber. Best for applications where flame retardancy and good processability are the main requirements, without the need for high structural strength.

  • PA6 GF30 FR(V0): Reinforced with 30% glass fibers. It offers a superior balance of high strength, stiffness, heat resistance (HDT >200°C), and V-0 rating, making it the most versatile grade for demanding structural parts.

  • PA6 GF50 FR(V0): Contains 50% glass fibers, providing the highest stiffness and dimensional stability in the series. It’s designed for metal replacement in applications requiring extreme rigidity alongside fire safety.

Q3: How do I choose the right PA6 FR grade for my application?
A3: Follow this simple guideline based on your primary need:

  • For basic flame safety and lowest cost in non-structural parts (e.g., housings, covers), choose PA6 FR(V0).

  • For the best all-around performance of strength, heat resistance, and flame retardancy (e.g., gears, connectors, enclosures), choose PA6 GF30 FR(V0).

  • For maximum stiffness and load-bearing capacity where part deflection must be minimized, choose PA6 GF50 FR(V0).
    For a precise recommendation, please contact our engineering team with your specific part design and requirements.

Q4: Can PA6 FR grades replace metal parts?
A4: Yes, especially the glass-reinforced grades. PA6 GF50 FR(V0), with its ultra-high modulus, is specifically engineered for lightweight metal replacement. It can replace metals like aluminum in certain structural applications, offering significant weight reduction, corrosion resistance, and design freedom while maintaining V-0 flame retardancy. The choice depends on the specific load, temperature, and environmental conditions.

Q5: Are PA6 FR materials resistant to chemicals and high temperatures?
A5: PA6 FR grades inherit good resistance to many oils, greases, and hydrocarbons from the base Nylon 6. Regarding temperature:

  • Continuous Use Temperature: They are suitable for long-term use in elevated temperature environments common in electrical and automotive applications.

  • Heat Deflection Temperature (HDT): This increases with glass fiber content. For example, PA6 GF30 FR(V0) has a significantly higher HDT than the unreinforced FR(V0) grade, making it stable under higher thermal load.
    Always consult the specific material datasheet for exact chemical compatibility and thermal performance data.

Q6: What should I consider when processing (injection molding) PA6 FR materials?
A6: Key processing considerations include:

  1. Drying: PA6 is hygroscopic. Proper drying (e.g., 80-90°C for 4+ hours) is essential before processing to prevent hydrolysis and ensure optimal properties and surface finish.

  2. Mold Temperature: A higher mold temperature (e.g., 80-100°C) is recommended to reduce internal stresses, improve crystallinity, and enhance surface appearance.

  3. Screw and Barrel: Use general-purpose screws. Due to the fillers, some wear can occur over time, so hardened steel is advised for long production runs.
    Our technical datasheets provide detailed processing guidelines.

Q7: Where can I get technical data sheets (TDS) or request a sample for PA6 FR materials?
A7: You can download preliminary technical data sheets from our product pages. For official, lot-specific datasheets or to request material samples for testing and validation, please visit our contact page to get in touch with our sales or technical support team: https://nylonplastic.com/contact/

Start Your Project Review

This field is required.
This field is required.
What do you need?
Choose the option that best matches your current project stage.
This field is required.
This field is required.
This field is required.
This field is required.
Accepted: JPG, JPEG, GIF, PNG or PDF, up to 10 MB. CAD files can be sent by email after submission.
This field is required.
This field is required.
Scroll to Top

Get in Touch

Fill out the form below, and we will be in touch shortly.

Contact Information