PA6 GF50 | 50% Glass Fiber Reinforced Nylon 6 – Nylon Plastic

What is PA6 GF50?

PA6 GF50 is a high-performance engineering thermoplastic where polyamide 6 (nylon 6) is reinforced with 50% by weight glass fibers. This maximum fiber loading pushes the material’s rigidity, strength, and heat resistance to the upper limits of the standard PA6 GF series, creating a composite capable of replacing metals in the most demanding structural applications.

Why Choose Nylon Plastic’s PA6 GF50?

✅ Premium High-Performance Grade: Our PA6 GF50 is formulated for maximum property consistency, delivering unparalleled strength and thermal stability critical for advanced engineering applications.

✅ Dedicated Processing Support: We provide expert guidance on handling high-fiber materials, including optimal drying, molding parameters, and equipment recommendations (e.g., wear-resistant screws and tooling) to ensure successful production.

✅ Custom-Tailored Solutions: We can tailor formulations with specific additives—such as enhanced heat stabilizers, lubricants, or coupling agents—to meet your unique requirements for extreme environments.

✅ Guaranteed Supply & Scalability: Our robust supply chain and production planning ensure reliable material availability, from your initial prototyping runs through to full-scale mass production.

Categories: , Brand:

万翰详情 01

 

PA6 G50 Technical Specifications (Estimated)

Property Value Test Standard
Glass Fiber Content 50% (±2%) ISO 1172
Tensile Strength 160 – 220 MPa ISO 527
Flexural Modulus 9,000 – 14,000 MPa ISO 178
Impact Strength (Notched Izod) 8 – 12 kJ/m² ISO 180
Heat Deflection Temperature (HDT) 200 – 220 °C @ 1.8 MPa ISO 75
Melting Point 215 – 230 °C ISO 3146
Moisture Absorption (Equilibrium, 23°C/50% RH) ~1.3% ISO 62

PA6 Series Material Performance Comparison Table:

Property PA6 GF15 PA6 GF30 PA6 GF40 PA6 GF50 PA6 GF60
Glass Fiber Content 15% 30% 40% 50% 60%
Density (g/cm³) 1.21 1.38 1.46 1.56 1.67
Tensile Strength (MPa) 118 165 185 200 220
Elongation at Break (%) 3.3 3.0 2.8 2.0 2.0
Notched Impact Strength (kJ/m²) 10 12 13 14 14
Heat Deflection Temperature (℃, 1.8MPa) 160 175 215 216 220

Key Advantages of PA6 G50:

✅ Metal-Replacement Strength and Stiffness

PA6 G50 delivers exceptional tensile strength and the highest flexural modulus among common GF grades, approaching the performance of metals like aluminum in specific applications. This enables the design of ultra-rigid, load-bearing components that contribute to significant weight reduction.

✅ Maximum Thermal Performance

Featuring the highest Heat Deflection Temperature (HDT) in the PA6 GF series, PA6 G50 maintains structural integrity and dimensional stability under intense and continuous heat exposure, making it suitable for the most demanding high-temperature environments.

✅ Ultimate Dimensional Stability

The extremely high glass fiber content minimizes the inherent moisture absorption of nylon and drastically reduces thermal expansion. This results in superior dimensional stability, ensuring critical parts maintain precise tolerances under varying humidity and temperature conditions.

✅ Enhanced Wear and Chemical Resistance

In addition to the good chemical resistance inherited from PA6, the high fiber load significantly improves wear resistance and reduces creep under sustained load, making it ideal for high-stress mechanical, automotive, and industrial applications.

Industry Applications:

the crucial role of injection molding in automotive industry

PA6GF50 is commonly used in automotive components, interior parts, and other applications that require a good surface finish and fundamental rigidity.

Powering Innovation Across Industries

Industry Key Applications
Automotive Engine covers, intake manifolds, structural brackets, sensor housings, connectors.
Explore Automotive Applications →
Electrical & Electronics Circuit breakers, switches, connector housings, insulating components.
Discover E&E Solutions →
Industrial Equipment Gears, bearings, machine housings, rollers, mechanical components.
See Industrial Uses →
Various application scenarios of PA plastics
Various application scenarios of PA plastics

How to Choose?

In simple terms:

  • For good toughness or cost-effectiveness, consider PA6 GF15.

  • For balanced overall performance, choose PA6 GF30.

  • For higher stiffness, strength, and heat resistance, and where cost is less sensitive, consider PA6 GF40/50/60. Generally, higher glass fiber content improves these properties.

Why Choose Us?

万翰详情 03

万翰详情 04

FAQ Section:

Q: Can I get a sample before placing an order?
A: Yes! We provide free samples for qualified projects.

Q: What’s the lead time for production?
A: Standard grades: 5-7 days; Custom formulations: 2-3 weeks.

Q: Do you provide material certifications?
A: Yes, we provide full material documentation and certifications.

Tell Us About Your Part

This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
Scroll to Top

Get in Touch

Fill out the form below, and we will be in touch shortly.

Contact Information