PA66 GF60 Technical Specifications (Estimated)
| Property | Value | Test Standard |
|---|---|---|
| Glass Fiber Content | 60% (±2%) | ISO 1172 |
| Tensile Strength | 190 – 250 MPa | ISO 527 |
| Flexural Modulus | 14,000 – 18,000 MPa | ISO 178 |
| Impact Strength (Notched Izod) | 6 – 9 kJ/m² | ISO 180 |
| Heat Deflection Temperature (HDT) | 257 – 262 °C @ 1.8 MPa | ISO 75 |
| Melting Point | 255 – 265 °C | ISO 3146 |
| Moisture Absorption (Equilibrium, 23°C/50% RH) | ~0.6% | ISO 62 |
PA66 Series Material Performance Comparison Table:
| Property | PA66 GF15 | PA66 GF30 | PA66 GF40 | PA66 GF50 | PA66 GF60 |
|---|---|---|---|---|---|
| Glass Fiber Content | 15% | 30% | 40% | 50% | 60% |
| Tensile Strength (MPa) | ~120 | ~175 | ~190 | ~210 | ~220 |
| Flexural Modulus (MPa) | ~5,500 | ~8,750 | ~10,500 | ~14,000 | ~16,000 |
| Notched Impact (kJ/m²) | ~13 | ~11.5 | ~10 | ~9 | ~7.5 |
| HDT @1.8MPa (°C) | ~240 | ~252 | ~255 | ~257 | ~260 |
Key Advantages of PA66 GF60
Ultimate Stiffness & Dimensional Stability:
Represents the pinnacle of achievable rigidity and minimal thermal expansion in PA66 composites.
Maximum Thermal Endurance:
Designed to operate at the upper limit of continuous use temperatures for thermoplastic composites.
Specialized for Extreme Static Loads:
Where deformation under load is unacceptable, even at high temperatures.
Good Chemical & Wear Resistance:
Inherits good resistance to oils, fuels, and chemicals from PA66, with enhanced wear resistance due to high fiber content.
Industry Applications:

PA66GF60 is commonly used in automotive components, interior parts, and other applications that require a good surface finish and fundamental rigidity.
Powering Innovation Across Industries
| Industry | Key Applications |
|---|---|
| Automotive | Engine covers, intake manifolds, structural brackets, sensor housings, connectors. |
| Electrical & Electronics | Circuit breakers, switches, connector housings, insulating components. |
| Industrial Equipment | Gears, bearings, machine housings, rollers, mechanical components. |

How to Choose the Right PA66 Grade?
For optimal toughness and cost-effectiveness, start with PA66 GF15. It provides a solid upgrade from unreinforced PA66, offering solid strength and good impact resistance for general industrial and automotive components.
For the best all-around, industry-proven performance, choose PA66 GF30. It delivers an excellent balance of high strength, stiffness, and exceptional heat resistance (HDT >250°C), making it the default choice for demanding structural and under-hood applications.
For a measurable performance upgrade where standard grades reach their limit, consider PA66 GF33. This grade offers higher stiffness and thermal margin than GF30, ideal for precision parts requiring guaranteed performance.
For maximum stiffness, strength, and thermal resistance where metal replacement is the goal, look to PA66 GF50 or PA66 GF60. These high-fiber grades deliver near-metallic properties for extreme loads and temperatures, but require careful evaluation of their reduced impact toughness and significant processing challenges.
Why Choose Us?


FAQ Section:
Q: Can I get a sample before placing an order?
A: Yes! We provide free samples for qualified projects.
Q: What’s the lead time for production?
A: Standard grades: 5-7 days; Custom formulations: 2-3 weeks.
Q: Do you provide material certifications?
A: Yes, we provide full material documentation and certifications.
PA66 GF60 Grade and Project Review
Use the PA66 properties and grades guide for base-resin context and the PA66 GF30 vs GF50 comparison for lower reinforcement options. The verified download library currently lists standard PA66 GF10 through GF50 and separate FR variants; it does not list a standard PA66 GF60 PDF, so GF50 data must not be used as GF60 release data.