PA6 GF20 | 20% Glass Fiber Reinforced Nylon 6

What is PA6 GF20?

PA6 GF20 is a reinforced engineering plastic where nylon 6 is compounded with 20% glass fibers. It is strategically positioned to bridge the gap between standard and high-performance grades, delivering a significant and cost-effective boost in mechanical properties over PA6 GF15 without fully committing to the stiffness and processing demands of PA6 GF30. It’s the ideal choice when you need “more than GF15 but not quite GF30.”

Why Choose Nylon Plastic’s PA6 GF20?

✅Optimized Performance per Cost: Achieves an excellent balance, offering more strength for your investment compared to lower-filled grades.

✅  Versatile Application Range: Suitable for a wide array of components that require reliable performance under moderate stress and heat.

✅ Proven Processing Reliability: Our formulation ensures consistent flow and molding behavior for predictable production outcomes.

✅ Fast Delivery: Reliable supply chain from prototyping to mass production

Categories: , Brand:

万翰详情 01

Technical Specifications Table :

Property Value Test Standard
Glass Fiber Content 20% (±2%) ISO 1172
Tensile Strength 100 – 145 MPa ISO 527
Flexural Modulus 4,200 – 6,500 MPa ISO 178
Impact Strength (Notched Izod) 11 – 16 kJ/m² ISO 180
Heat Deflection Temperature (HDT) 165 – 195 °C @ 1.8 MPa ISO 75
Melting Point 215 – 230 °C ISO 3146
Moisture Absorption ~1.7% (23°C/50% RH) ISO 62

 

PA6 Series Material Performance Comparison Table:

Property PA6 GF15 PA6 GF20 PA6 GF30 PA6 GF33 PA6 GF40 PA6 GF50 PA6 GF60
Glass Fiber Content 15% 20% 30% 33% 40% 50% 60%
Tensile Strength (MPa) ~118 ~125 ~165 ~175 ~185 ~200 ~220
Flexural Modulus (MPa) ~3,800 ~4,500 ~5,218 ~7,000 ~7,500 ~9,000 ~12,000
Notched Impact (kJ/m²) ~10 ~12 ~12 ~12.5 ~13 ~14 ~14
HDT @1.8MPa (°C) ~160 ~180 ~190 ~195 ~215 ~216 ~220
Key Profile High toughness, cost-effective Balance of toughness & strength Best all-around, most widely used Performance upgrade of GF30 Start of high stiffness & heat resist. Metal-like stiffness & strength Ultimate stiffness for extreme cases

 

Key Advantages of PA6 GF20

✅ Enhanced Strength with Good Toughness:

Offers a noticeable improvement in rigidity and strength over GF15, while retaining better impact resistance than higher GF grades.

✅Improved Thermal Capability:

Higher heat deflection temperature provides a greater safety margin for applications in warm environments.

✅ Cost-Effective Performance Upgrade:

An economical step-up material when PA6 GF15 reaches its mechanical limit.

✅ Good Processability:

Maintains relatively good flow compared to GF30 and above, suitable for molding parts with moderate complexity.

 

Industry Applications:

the crucial role of injection molding in automotive industry

PA6GF20 is commonly used in automotive components, interior parts, and other applications that require a good surface finish and fundamental rigidity.

Powering Innovation Across Industries

Industry Key Applications
Automotive Engine covers, intake manifolds, structural brackets, sensor housings, connectors.
Explore Automotive Applications →
Electrical & Electronics Circuit breakers, switches, connector housings, insulating components.
Discover E&E Solutions →
Industrial Equipment Gears, bearings, machine housings, rollers, mechanical components.
See Industrial Uses →
Various application scenarios of PA plastics
Various application scenarios of PA plastics

How to Choose?

In simple terms:

  • For good toughness or cost-effectiveness, consider PA6 GF15.

  • For balanced overall performance, choose PA6 GF30.

  • For higher stiffness, strength, and heat resistance, and where cost is less sensitive, consider PA6 GF40/50/60. Generally, higher glass fiber content improves these properties.

Why Choose Us?

万翰详情 03

万翰详情 04

FAQ Section:

Q: Can I get a sample before placing an order?
A: Yes! We provide free samples for qualified projects.

Q: What’s the lead time for production?
A: Standard grades: 5-7 days; Custom formulations: 2-3 weeks.

Q: Do you provide material certifications?
A: Yes, we provide full material documentation and certifications.

Tell Us About Your Part

This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
Scroll to Top

Get in Touch

Fill out the form below, and we will be in touch shortly.

Contact Information