PA66 CF30 Nylon 66 with 30% Carbon Fiber | Nylon Plastic

PA66 CF30 is an engineering thermoplastic composite based on nylon 66 (PA66) reinforced with 30% carbon fibers. As the performance benchmark of the series, it is designed for critical structural components that must withstand high continuous stress, elevated temperatures, and dynamic loads with unwavering reliability.

Why Choose Nylon Plastic’s PA66 CF30?
✅ Unmatched Structural Integrity: We supply the definitive grade for mission-critical structures, providing an unmatched combination of tensile strength, flexural modulus, and creep resistance.
✅ Precision Engineered for Extreme Conditions: Our PA66 CF30 is formulated to maintain its superior properties at high temperatures, ensuring your designs perform reliably at the edge of their operational limits.
✅ Technical Partnership for Critical Applications: We offer deep material science expertise to support the design and processing of PA66 CF30, ensuring optimal performance in your most challenging applications.
✅ Driving Innovation in Core Sectors: We enable you to push the boundaries in automotive, aerospace, and industrial automation by providing a material that meets the highest standards of performance and durability.

Categories: , Brand:

万翰详情 01

PA66 CF30 Technical Data (Estimated Typical Values)

Property Value Test Standard
Carbon Fiber Content 30% ISO 1172
Tensile Strength 240 – 270 MPa ISO 527
Flexural Modulus 21,000 – 24,000 MPa ISO 178
Notched Impact Strength 10 – 13 kJ/m² ISO 180
HDT @1.8 MPa 260 – 270 °C ISO 75
Volume Resistivity 10^1 – 10^3 Ω·cm IEC 60093

 

PA66 CF Series Technical Data Table (Estimated Typical Values)

Property Test Standard PA66 CF10 PA66 CF20 PA66 CF30 PA66 CF40 PA66 CF50
Carbon Fiber Content ISO 1172 10% 20% 30% 40% 50%
Tensile Strength ISO 527 160 – 180 MPa 200 – 230 MPa 240 – 270 MPa 260 – 290 MPa 280 – 320 MPa
Flexural Modulus ISO 178 11,000 – 13,000 MPa 16,000 – 19,000 MPa 21,000 – 24,000 MPa 25,000 – 28,000 MPa 29,000 – 33,000 MPa
Notched Impact Strength ISO 180 8 – 11 kJ/m² 9 – 12 kJ/m² 10 – 13 kJ/m² 11 – 14 kJ/m² 12 – 15 kJ/m²
HDT @1.8 MPa ISO 75 250 – 260 °C 255 – 265 °C 260 – 270 °C 265 – 275 °C 270 – 280 °C
Volume Resistivity IEC 60093 10^3 – 10^5 Ω·cm 10^2 – 10^4 Ω·cm 10^1 – 10^3 Ω·cm 10^0 – 10^2 Ω·cm 10^-1 – 10^1 Ω·cm

PA66 CF30 Key Advantages

✅ Benchmark Structural Performance: Represents the industry standard for high-load applications, delivering near-metallic stiffness, exceptional strength, and outstanding fatigue resistance.
✅ Maximum Thermal & Dimensional Stability: Provides the highest heat deflection temperature and lowest thermal expansion in the mid-range series, ensuring precision in volatile environments.
✅ Advanced Conductivity for Demanding Uses: Offers tailored electrical properties suitable for grounding components and applications requiring consistent static dissipation and thermal management.

Industry Applications:

the crucial role of injection molding in automotive industry

Explore the PA66 Carbon Fiber Series in Detail

Click on the links below to view comprehensive technical data, key advantages, and application details for each specific grade.

Grade Best For Overview Full Details
PA66 CF10 High-temp capable parts needing stiffness & ESD on a budget. The most accessible high-temperature CF grade, offering enhanced heat resistance, rigidity, and ESD protection over standard PA66. View PA66 CF10 Full Data Sheet →
PA66 CF20 Demanding metal replacement where heat, strength & weight matter. A balanced performer for high-temperature environments, excelling in strength-to-weight ratio and functional conductivity. View PA66 CF20 Full Data Sheet →
PA66 CF30 Structural components under high thermal and mechanical stress. The benchmark for high-temperature structural integrity, providing near-metallic stiffness and outstanding fatigue resistance. View PA66 CF30 Full Data Sheet →
PA66 CF40 Ultra-stiff, high-heat applications where deflection is critical. Engineered for maximum rigidity and dimensional stability under extreme thermal and mechanical loads. View PA66 CF40 Full Data Sheet →
PA66 CF50 Mission-critical applications at the limits of thermal & mechanical performance. The pinnacle grade, delivering peak specific strength and stiffness in the most severe high-temperature environments. View PA66 CF50 Full Data Sheet →

Powering Innovation Across Industries

Industry Key Applications
Automotive Engine covers, intake manifolds, structural brackets, sensor housings, connectors.
Explore Automotive Applications →
Electrical & Electronics Circuit breakers, switches, connector housings, insulating components.
Discover E&E Solutions →
Industrial Equipment Gears, bearings, machine housings, rollers, mechanical components.
See Industrial Uses →
Various application scenarios of PA plastics
Various application scenarios of PA plastics

How to Choose the Right PA66 CF Grade?

In simple terms:

  • For a cost-effective upgrade into high-temperature capable carbon fiber composites with significantly improved stiffness, heat resistance, and ESD, consider PA66 CF10.

  • For the optimal balance of high strength, heat deflection temperature, and lightweight design in demanding metal replacement applications, choose PA66 CF30. It is the performance benchmark for most high-temperature structural uses.

  • For the ultimate high-temperature stiffness, strength, and dimensional stability where performance is critical under extreme conditions, consider PA66 CF50.

Why Choose Us?

万翰详情 03

万翰详情 04

FAQ Section:

Q1: When should I choose PA66 CF30 over CF20?
Choose PA66 CF30 when your application demands benchmark structural performance. It offers significantly higher stiffness, strength, and thermal stability than CF20, making it the preferred grade for high-stress components, critical structural brackets, and parts under continuous dynamic load.

Q2: Can PA66 CF30 be used in under-the-hood automotive applications?
Absolutely. Its high Heat Deflection Temperature (260-270°C) and excellent creep resistance make PA66 CF30 suitable for under-the-hood components like sensor housings, connectors, and structural parts that must endure long-term heat and vibration.

Q3: Does the higher carbon fiber content in CF30 affect processing?
Yes. While offering superior properties, PA66 CF30 has lower melt viscosity and is more abrasive.

  • Tooling: Hardened steel tooling is strongly recommended.

  • Injection Speed: Use moderate to high injection speeds to ensure good fiber orientation and surface finish.

  • Drying: Thorough drying (4-6 hours at 80-90°C) remains critical.

Tell Us About Your Part

This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
This field is required.
Scroll to Top

Get in Touch

Fill out the form below, and we will be in touch shortly.

Contact Information